Zheng et al., 2022 - Google Patents
Action mechanism of liquid bridge between electroplated diamond wires for ultrathin wafer slicingZheng et al., 2022
- Document ID
- 13665312144406287576
- Author
- Zheng J
- Ge P
- Bi W
- Zhao Y
- Wang C
- Publication year
- Publication venue
- Solar Energy
External Links
Snippet
Ultrathin wafer slicing with low kerf loss for electroplated diamond wire sawing is the primary means to improve the productivity in wafering and reduce the manufacturing costs in the photovoltaic industry. Nevertheless, the reduction of the diameter and spacing of the …
- 229910003460 diamond 0 title abstract description 205
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GASES [GHG] EMISSION, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E10/00—Energy generation through renewable energy sources
- Y02E10/50—Photovoltaic [PV] energy
- Y02E10/52—PV systems with concentrators
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GASES [GHG] EMISSION, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E10/00—Energy generation through renewable energy sources
- Y02E10/40—Solar thermal energy
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GASES [GHG] EMISSION, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies or technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Zheng et al. | Action mechanism of liquid bridge between electroplated diamond wires for ultrathin wafer slicing | |
Li et al. | Nucleation location and propagation direction of radial and median cracks for brittle material in scratching | |
Xiao et al. | Evaluation of fixed abrasive diamond wire sawing induced subsurface damage of solar silicon wafers | |
Li et al. | The effect of cut depth and distribution for abrasives on wafer surface morphology in diamond wire sawing of PV polycrystalline silicon | |
Wang et al. | Analytical prediction of subsurface microcrack damage depth in diamond wire sawing silicon crystal | |
Yin et al. | Experimental study on slicing photovoltaic polycrystalline silicon with diamond wire saw | |
Bin et al. | Theoretical and experimental investigation on surface generation and subsurface damage in fixed abrasive lapping of optical glass | |
Li et al. | Experiment and theoretical prediction for subsurface microcracks and damage depth of multi-crystalline silicon wafer in diamond wire sawing | |
Zheng et al. | Effect of capillary adhesion on fracture of photovoltaic silicon wafers during diamond wire slicing | |
CN105058223A (en) | Single-side grinding method for germanium single crystal wafer | |
Wu et al. | The orientation and optical properties of inverted-pyramid-like structures on multi-crystalline silicon textured by Cu-assisted chemical etching | |
Lai et al. | Dynamic model and machining mechanism of wire sawing | |
Ge et al. | Crack damage control for diamond wire sawing of silicon: The selection of processing parameters | |
Ryningen et al. | Capillary forces as a limiting factor for sawing of ultrathin silicon wafers by diamond multi-wire saw | |
Wallburg et al. | A material removal coefficient for diamond wire sawing of silicon | |
Wang et al. | Fracture strength of photovoltaic silicon wafers cut by diamond wire saw based on half-penny crack system | |
Cheng et al. | Fracture probability of PV mono-Si wafers in diamond wire slicing due to coupling of capillary adhesion bending stress and sawing stress | |
Cheng et al. | A critical review on the fracture of ultra-thin photovoltaics silicon wafers | |
Zheng et al. | Transverse forced vibration of a diamond wire under support excitations | |
CN102277574B (en) | Monocrystalline silicon solar cell, etching liquid thereof, texturing method, preparation method and photovoltaic component | |
Omer et al. | Ultra-thin silicon wafers fabrication and inverted pyramid texturing based on cu-catalyzed chemical etching | |
CN108044819A (en) | A kind of silicon rod cutting method | |
Zheng et al. | Study on the abrasive retention capacity on the surface of electroplated diamond wire saw | |
Sullivan et al. | A thin rivulet of perfectly wetting fluid subject to a longitudinal surface shear stress | |
Yin et al. | Study on cutting PV polysilicon with a new type of diamond abrasives-helix-distribution saw wire based on controlling the subsurface microcrack damage depth |