ES8305608A1 - "procedimiento de colada vertical en continuo del aluminio y de sus aleaciones en forma de lingotes y de placas". - Google Patents
"procedimiento de colada vertical en continuo del aluminio y de sus aleaciones en forma de lingotes y de placas".Info
- Publication number
- ES8305608A1 ES8305608A1 ES513801A ES513801A ES8305608A1 ES 8305608 A1 ES8305608 A1 ES 8305608A1 ES 513801 A ES513801 A ES 513801A ES 513801 A ES513801 A ES 513801A ES 8305608 A1 ES8305608 A1 ES 8305608A1
- Authority
- ES
- Spain
- Prior art keywords
- casting process
- alloys
- aluminium
- vat
- high speed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
PROCEDIMIENTO DE COLADA VERTICAL CONTINUA DEL ALUMINIO Y SUS ALEACIONES. CARACTERIZADO PARA COMBINAR LA UTILIZACION DE UN REALCE (1) MOVIL Y UN CAMPO MAGNETICO, GENERADO POR UN INDUCTOR (3), QUE ACTUA SOBRE LA ZONA DE METAL LIQUIDO (4) SITUADA BAJO EL REALCE (1). SE COMPLEMENTA CON UN DISPOSITIVO DE REFRIGERACION (5) MOVIL QUE ENVIA UNA LAMINA DE AGUA (6) PERIFERICA POR DEBAJO DEL FRENTE DE SOLIDIFICACION (7), Y OTRO PASO COMPLEMENTARIO DE REFRIGERACION (8) COLOCADO POR DEBAJO DEL INDUCTOR (3) QUE SUMINISTRA EL CHORRO DE LIQUIDO (9). EL SISTEMA BOQUILLA-FLOTADOR (2) MANTIENE EL NIVEL DE METAL LIQUIDO (10), MIENTRAS QUE LA ACTUACION COMBINADA DEL REALCE (1), INDUCTOR (3) Y SISTEMAS DE REFRIGERACION (5, 8) MANTIENEN CONSTANTE LA DISTANCIA ENTRE FRENTE DE SOLIDIFICACION (7) Y EL PLANO DE LA BASE DEL REALCE, CON INDEPENDENCIA DE LA VELOCIDAD DE COLADA.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR8114037A FR2509207A1 (fr) | 1981-07-09 | 1981-07-09 | Procede de coulee continue verticale a grande vitesse de l'aluminium et de ses alliages |
Publications (2)
Publication Number | Publication Date |
---|---|
ES8305608A1 true ES8305608A1 (es) | 1983-04-16 |
ES513801A0 ES513801A0 (es) | 1983-04-16 |
Family
ID=9260641
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES513801A Granted ES513801A0 (es) | 1981-07-09 | 1982-07-08 | "procedimiento de colada vertical en continuo del aluminio y de sus aleaciones en forma de lingotes y de placas". |
Country Status (18)
Country | Link |
---|---|
US (1) | US4523627A (es) |
EP (1) | EP0083611B1 (es) |
JP (1) | JPS58500939A (es) |
AU (1) | AU547447B2 (es) |
BR (1) | BR8207785A (es) |
CA (1) | CA1178780A (es) |
DE (1) | DE3262654D1 (es) |
ES (1) | ES513801A0 (es) |
FR (1) | FR2509207A1 (es) |
GB (1) | GB2103972B (es) |
GR (1) | GR69780B (es) |
IN (1) | IN156297B (es) |
IT (1) | IT1151818B (es) |
NO (1) | NO830653L (es) |
RO (1) | RO87316B (es) |
SU (1) | SU1178315A3 (es) |
WO (1) | WO1983000107A1 (es) |
YU (1) | YU145382A (es) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2570304B1 (fr) * | 1984-09-19 | 1986-11-14 | Cegedur | Procede de reglage du niveau de la ligne de contact de la surface libre du metal avec la lingotiere dans une coulee verticale |
US5085265A (en) * | 1990-03-23 | 1992-02-04 | Nkk Corporation | Method for continuous casting of molten steel and apparatus therefor |
US5469911A (en) * | 1994-04-12 | 1995-11-28 | Reynolds Metals Company | Method for improving surface quality of electromagnetically cast aluminum alloys and products therefrom |
JP3696844B2 (ja) * | 2002-07-08 | 2005-09-21 | 九州三井アルミニウム工業株式会社 | 半溶融成型性に優れたアルミニウム合金 |
EP1486347A1 (en) * | 2003-06-12 | 2004-12-15 | Fuji Photo Film B.V. | Aluminium alloy substrate for lithographic printing plate and method for producing the same |
Family Cites Families (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB1491864A (en) * | 1973-11-06 | 1977-11-16 | Alcan Res & Dev | Continuous casting |
IT1113478B (it) * | 1978-02-13 | 1986-01-20 | Olin Corp | Procedimento ed apparecchio per la fusine di rame e leghe di rame |
CA1123897A (en) * | 1978-07-03 | 1982-05-18 | John C. Yarwood | Electromagnetic casting method and apparatus |
US4161978A (en) * | 1978-07-19 | 1979-07-24 | Reynolds Metals Company | Ingot casting |
US4236570A (en) * | 1979-01-08 | 1980-12-02 | Olin Corporation | Ingot shape control by dynamic head in electromagnetic casting |
-
1981
- 1981-07-09 FR FR8114037A patent/FR2509207A1/fr active Granted
-
1982
- 1982-06-09 GB GB08216749A patent/GB2103972B/en not_active Expired
- 1982-06-11 IN IN679/CAL/82A patent/IN156297B/en unknown
- 1982-07-02 IT IT22215/82A patent/IT1151818B/it active
- 1982-07-05 YU YU01453/82A patent/YU145382A/xx unknown
- 1982-07-06 GR GR68668A patent/GR69780B/el unknown
- 1982-07-07 AU AU86812/82A patent/AU547447B2/en not_active Ceased
- 1982-07-07 EP EP82902070A patent/EP0083611B1/fr not_active Expired
- 1982-07-07 JP JP57502068A patent/JPS58500939A/ja active Pending
- 1982-07-07 US US06/474,669 patent/US4523627A/en not_active Expired - Fee Related
- 1982-07-07 DE DE8282902070T patent/DE3262654D1/de not_active Expired
- 1982-07-07 WO PCT/FR1982/000115 patent/WO1983000107A1/en active IP Right Grant
- 1982-07-07 BR BR8207785A patent/BR8207785A/pt unknown
- 1982-07-08 ES ES513801A patent/ES513801A0/es active Granted
- 1982-07-08 CA CA000406906A patent/CA1178780A/fr not_active Expired
-
1983
- 1983-02-24 NO NO830653A patent/NO830653L/no unknown
- 1983-03-03 RO RO110207A patent/RO87316B/ro unknown
- 1983-03-04 SU SU833560644A patent/SU1178315A3/ru active
Also Published As
Publication number | Publication date |
---|---|
BR8207785A (pt) | 1983-06-21 |
ES513801A0 (es) | 1983-04-16 |
IN156297B (es) | 1985-06-15 |
DE3262654D1 (en) | 1985-04-25 |
EP0083611B1 (fr) | 1985-03-20 |
SU1178315A3 (ru) | 1985-09-07 |
GR69780B (es) | 1982-07-07 |
IT8222215A0 (it) | 1982-07-02 |
IT1151818B (it) | 1986-12-24 |
YU145382A (en) | 1986-04-30 |
AU547447B2 (en) | 1985-10-17 |
RO87316A (ro) | 1985-08-31 |
CA1178780A (fr) | 1984-12-04 |
JPS58500939A (ja) | 1983-06-09 |
US4523627A (en) | 1985-06-18 |
AU8681282A (en) | 1983-02-02 |
GB2103972B (en) | 1985-01-09 |
IT8222215A1 (it) | 1984-01-02 |
FR2509207B1 (es) | 1983-11-10 |
NO830653L (no) | 1983-02-24 |
RO87316B (ro) | 1985-08-31 |
EP0083611A1 (fr) | 1983-07-20 |
FR2509207A1 (fr) | 1983-01-14 |
GB2103972A (en) | 1983-03-02 |
WO1983000107A1 (en) | 1983-01-20 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB993086A (en) | Process for the horizontal continuous casting of molten metal | |
GB1269833A (en) | A method and apparatus for producing a metal article | |
ES477107A1 (es) | Un metodo para controlar la velocidad de vertido de metal fundido. | |
ES8305608A1 (es) | "procedimiento de colada vertical en continuo del aluminio y de sus aleaciones en forma de lingotes y de placas". | |
GB1133426A (en) | Casting aluminium based alloys containing lead | |
GB944141A (en) | Continuous casting method and apparatus | |
DE3062505D1 (en) | Method and apparatus for the continuous casting of several strands | |
ES8500104A1 (es) | Procedimiento de reglaje de la refrigeracion secundaria de una maquina de colada continua. | |
GB1290758A (es) | ||
FI862091A0 (fi) | Foerfarande foer reglering av nivaon pao kontaktlinjen mellan metallens fria yta och gjutformen vid kontinuerlig vertikalgjutning. | |
JPS5659568A (en) | Method and device for improving quality of metal continuously casted | |
JPS57130741A (en) | Continuous casting method for faultless ingot | |
ES420075A1 (es) | Un metodo mejorado de colar continuamente acero. | |
GB1267466A (en) | Shaping an ingot during continuous and semi-continuous casting | |
GB1148803A (en) | Improvements in or relating to a continuous metal casting machine for the production of ingots of square or substantially square cross-section | |
JPS5536088A (en) | Separated cooling box of horizontal continuous casting machine | |
GB1221960A (en) | Method of cooling molds | |
JPS5356113A (en) | Grain refining method for aluminum or its alloy | |
Heard | The Influence of Withdrawal Parameters on Surface Quality of Horizontally Cast Bars | |
JPS5794450A (en) | Method for administration of size of ingot width in continuous casting | |
JPS5675512A (en) | Method of adding aluminum for deoxidation to molten steel | |
GB1259286A (es) | ||
JPS56144853A (en) | Preventing method for pickup of carbon in continuous casting | |
Larrecq et al. | Results Obtained With a 900 mm High Continuous Casting Mould at Sollac | |
Mulcahy | Method of and Apparatus for Continuous Casting of Molten Metals Such as Steel |