[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

PL422895A1 - Method for improving the soil subbase - Google Patents

Method for improving the soil subbase

Info

Publication number
PL422895A1
PL422895A1 PL422895A PL42289517A PL422895A1 PL 422895 A1 PL422895 A1 PL 422895A1 PL 422895 A PL422895 A PL 422895A PL 42289517 A PL42289517 A PL 42289517A PL 422895 A1 PL422895 A1 PL 422895A1
Authority
PL
Poland
Prior art keywords
soil
improving
binder
weight
amount
Prior art date
Application number
PL422895A
Other languages
Polish (pl)
Other versions
PL240184B1 (en
Inventor
Rafał Sochacki
Original Assignee
Sochacki Rafał Technologie Drogowe Sochacki
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sochacki Rafał Technologie Drogowe Sochacki filed Critical Sochacki Rafał Technologie Drogowe Sochacki
Priority to PL422895A priority Critical patent/PL240184B1/en
Publication of PL422895A1 publication Critical patent/PL422895A1/en
Publication of PL240184B1 publication Critical patent/PL240184B1/en

Abstract

Przedmiotem wynalazku jest sposób ulepszenia podłoża gruntowego na drodze powierzchniowej lub wgłębnej stabilizacji. Sposób ulepszenia podłoża gruntowego poprzez zmieszanie gruntu z odpowiednią ilością spoiwa i wody, wałowanie oraz zagęszczenie i profilowanie charakteryzuje się tym, że po wymieszaniu gruntu z mineralnym spoiwem z aktywnych wypełniaczy hydraulicznych opartego na bazie popiołów lotnych z węgla brunatnego dozowanym wagowo w przeliczeniu na 1 m2 powierzchni z dokładnością do ± 5% oraz zagęszczeniu rozprowadza się na podłożu gruntowym spoiwo w postaci cementu w ilości 2 -3% i miesza mieszankę gruntową na mniejszą głębokość. Mineralne spoiwo w postaci popiołów lotnych aplikuje się do gruntu w ilości od 2,5 - 6% w stosunku do masy gruntu, wodę dozuje się objętościowo lub wagowo, aż do uzyskania wilgotności optymalnej, z tolerancją +10%, -20% jej wartości.The subject of the invention is a method for improving a soil substrate by surface or downhole stabilization. The method of improving the subsoil by mixing the soil with the right amount of binder and water, rolling, compaction and profiling is characterized by the fact that after mixing the soil with a mineral binder made of active hydraulic fillers based on fly ash from brown coal, dosed by weight calculated per 1 m2 of surface with an accuracy of ± 5% and compaction, the binder in the form of cement is spread in the amount of 2 -3% on the ground, and the soil mix is mixed to a smaller depth. Mineral binder in the form of fly ash is applied to the soil in an amount of 2.5 - 6% in relation to the weight of the soil, water is dosed by volume or weight, until optimal humidity is obtained, with a tolerance of + 10%, -20% of its value.

PL422895A 2017-09-16 2017-09-16 Method for improving the soil subbase PL240184B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL422895A PL240184B1 (en) 2017-09-16 2017-09-16 Method for improving the soil subbase

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL422895A PL240184B1 (en) 2017-09-16 2017-09-16 Method for improving the soil subbase

Publications (2)

Publication Number Publication Date
PL422895A1 true PL422895A1 (en) 2019-03-25
PL240184B1 PL240184B1 (en) 2022-02-28

Family

ID=65799880

Family Applications (1)

Application Number Title Priority Date Filing Date
PL422895A PL240184B1 (en) 2017-09-16 2017-09-16 Method for improving the soil subbase

Country Status (1)

Country Link
PL (1) PL240184B1 (en)

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CA1199484A (en) * 1981-03-19 1986-01-21 Yuichiro Takahashi Composition for improving strength of soft ground containing organic matter, and method of improving strength of soft ground by utilizing said composition
JPH09125362A (en) * 1995-10-30 1997-05-13 Mitsubishi Heavy Ind Ltd Dry improved coal ash backfilling technique
JP2006056909A (en) * 2004-07-20 2006-03-02 Kyokado Eng Co Ltd Plastic grout and grouting technique
JP2008223475A (en) * 2004-07-20 2008-09-25 Kyokado Eng Co Ltd Grouting method
US20150376499A1 (en) * 2013-02-06 2015-12-31 Etablissements Hublet Binder for self-compacting and re-excavatable backfill

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CA1199484A (en) * 1981-03-19 1986-01-21 Yuichiro Takahashi Composition for improving strength of soft ground containing organic matter, and method of improving strength of soft ground by utilizing said composition
JPH09125362A (en) * 1995-10-30 1997-05-13 Mitsubishi Heavy Ind Ltd Dry improved coal ash backfilling technique
JP2006056909A (en) * 2004-07-20 2006-03-02 Kyokado Eng Co Ltd Plastic grout and grouting technique
JP2008223475A (en) * 2004-07-20 2008-09-25 Kyokado Eng Co Ltd Grouting method
US20150376499A1 (en) * 2013-02-06 2015-12-31 Etablissements Hublet Binder for self-compacting and re-excavatable backfill

Also Published As

Publication number Publication date
PL240184B1 (en) 2022-02-28

Similar Documents

Publication Publication Date Title
CN103290750A (en) Road subgrade, base layer and subbase layer made of cementing ultra-strong chloride saline soil and construction method thereof
MX2020002599A (en) Stable asphalt emulsions, methods of forming the same, and composite structures formed from the same.
PL423255A1 (en) Method for asphalt foaming
PL422895A1 (en) Method for improving the soil subbase
PL410528A1 (en) Method for preventing relocation of impurities from the excavations after exploitation of mineral material to ground waters
NZ759197A (en) Additive formulation for reduction or prevention of microbially induced corrosion in concrete or cementitious material
PL436174A1 (en) Method for improving natural land and a mix for improving natural land
Farooq et al. Effect of lime and curing period on unconfined compressive strength of Gazipur soil, Bangladesh
Lee et al. Application and Characteristics of Dune Sand Concrete in the Middle East and North Africa
PL433017A1 (en) Rubber-asphalt-cement mortar for mineral mixtures
Kinahan Equilibrial Dynamics as an Alternative to Seasonality Models in the Late Holocene Human Ecology of the Namib Desert
PL416054A1 (en) Mix for producing aggregate concrete
PL431928A1 (en) Composition of the low-cement grout
PL423668A1 (en) Concrete mixer for forming foundation walls
PL423018A1 (en) Fluorescent concrete road surface
RU2011107394A (en) METHOD FOR CONSTRUCTION OF ROAD CLOTHES OF MILITARY-ROAD ROADS FROM SOIL STRENGTHENED WITH CEMENT
PL418053A1 (en) Mineral binder for repairing and sealing flood banks and method for repairing and sealing flood banks using the mineral binder
GEP20197002B (en) Method for bases of roads and ground structures building
JP2008013963A (en) Underwater filler, method of producing the same, and method of filling underground cavity
PL429522A1 (en) Method for foaming bituminous binder using zeolite
PL424711A1 (en) Method for consolidation, strengthening and drying of surface of building materials, preferably produced on the basis of lime and cement
Helanová et al. Utilization of liquefying additives in clay fly ash grouting mixtures
GB734106A (en) Improvements in and relating to surfaces particularly for use on sports grounds
PL414193A1 (en) Ground stabilizer and method for stabilization of grounds
PL423586A1 (en) Method for hydrophobic impregnation of concretes