PL429522A1 - Method for foaming bituminous binder using zeolite - Google Patents

Method for foaming bituminous binder using zeolite

Info

Publication number
PL429522A1
PL429522A1 PL429522A PL42952219A PL429522A1 PL 429522 A1 PL429522 A1 PL 429522A1 PL 429522 A PL429522 A PL 429522A PL 42952219 A PL42952219 A PL 42952219A PL 429522 A1 PL429522 A1 PL 429522A1
Authority
PL
Poland
Prior art keywords
foaming
asphalt binder
zeolite
asphalt
weight
Prior art date
Application number
PL429522A
Other languages
Polish (pl)
Other versions
PL235885B1 (en
Inventor
Agnieszka Woszuk
Wojciech Franus
Original Assignee
Politechnika Lubelska
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Politechnika Lubelska filed Critical Politechnika Lubelska
Priority to PL429522A priority Critical patent/PL235885B1/en
Publication of PL429522A1 publication Critical patent/PL429522A1/en
Publication of PL235885B1 publication Critical patent/PL235885B1/en

Abstract

Przedmiotem wynalazku jest sposób spieniania lepiszcza asfaltowego z użyciem zeolitu nasączonego wodą pozwalający na obniżenie lepkości asfaltu. Pozwoli to na obniżenie temperatury produkcji i zagęszczania mieszanek mineralno-asfaltowych oraz poprawę ich zagęszczalności. Sposób spieniania lepiszcza asfaltowego, polega na tym, że do zeolitu naturalnego dodaje się olej silnikowy w ilości od 15 do 40% w stosunku do masy zeolitu naturalnego i miesza się do momentu uzyskania mieszaniny o jednolitej strukturze. Następnie dodaje się mieszaninę w ilości od 2% do 10% wagowo w stosunku do masy lepiszcza asfaltowego do gorącego lepiszcza asfaltowego rozgrzanego do temperatury od 145°C do 180°C. W dalszej kolejności miesza się do momentu rozpoczęcia spieniania lepiszcza asfaltowego.The subject of the invention is a method of foaming asphalt binder with the use of zeolite impregnated with water, which allows the viscosity of asphalt to be reduced. This will reduce the production temperature and compaction of asphalt mixtures and improve their compaction. The method of foaming the asphalt binder consists in adding 15 to 40% of engine oil to natural zeolite based on the weight of natural zeolite and mixing until a mixture with a uniform structure is obtained. The mixture is then added in an amount of 2% to 10% by weight based on the weight of the asphalt binder to the hot asphalt binder heated to a temperature of 145 ° C to 180 ° C. It is then mixed until foaming of the asphalt binder begins.

PL429522A 2019-04-04 2019-04-04 Method for foaming bituminous binder using zeolite PL235885B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL429522A PL235885B1 (en) 2019-04-04 2019-04-04 Method for foaming bituminous binder using zeolite

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL429522A PL235885B1 (en) 2019-04-04 2019-04-04 Method for foaming bituminous binder using zeolite

Publications (2)

Publication Number Publication Date
PL429522A1 true PL429522A1 (en) 2019-08-26
PL235885B1 PL235885B1 (en) 2020-11-02

Family

ID=67683662

Family Applications (1)

Application Number Title Priority Date Filing Date
PL429522A PL235885B1 (en) 2019-04-04 2019-04-04 Method for foaming bituminous binder using zeolite

Country Status (1)

Country Link
PL (1) PL235885B1 (en)

Also Published As

Publication number Publication date
PL235885B1 (en) 2020-11-02

Similar Documents

Publication Publication Date Title
PL423255A1 (en) Method for asphalt foaming
EA201071149A1 (en) METHOD OF OBTAINING ASPHALT
MX2009011201A (en) Method for producing bitumen compositions.
MX2016009254A (en) Asphalt mixture, method for producing same and paving method using same.
CN102839587A (en) Marshall design method of Evotherm warm-mix asphalt mixture
PL429522A1 (en) Method for foaming bituminous binder using zeolite
PL429521A1 (en) Method for foaming bituminous binder using zeolite
PL429524A1 (en) Method for foaming bituminous binder using water-soaked zeolite
PL429523A1 (en) Method for foaming bituminous binder using water-soaked zeolite
PL433575A1 (en) Method of asphalt foaming using a mineral additive
PL423256A1 (en) Method for asphalt foaming
PL433574A1 (en) Method of asphalt foaming using a mineral additive
Monu et al. A review paper on warm mix asphalt technologies
PL433576A1 (en) Method of asphalt foaming using a two-ingredient mineral additive
Yadykina et al. Energy Saving Additives «RAA WAC» for Production of Warm Asphalt Concrete
PL433578A1 (en) Method of producing mineral asphalt mixture using a mineral additive
PL433572A1 (en) Method of asphalt foaming using a two-ingredient additive
PL426039A1 (en) Method for producing asphaltic concrete and the asphaltic concrete
PL433577A1 (en) Method of asphalt foaming using a two-ingredient mineral additive
de la Rosa et al. Evaluation of natural additives for warm asphalt mix
PL443605A1 (en) Method of modifying asphalt binders with a two-component additive
PL433573A1 (en) Method of asphalt foaming using a two-ingredient additive
PL443611A1 (en) Method of modifying asphalt binders with a two-component additive
PL431608A1 (en) Method of producing a concrete mix for the production of water-permeable concrete products
PL408012A1 (en) Method for producing asphalt binder