FR2541175A1 - PROCESS FOR FORMING A COMPOSITE CONTAINER AND CONTAINER THUS OBTAINED - Google Patents
PROCESS FOR FORMING A COMPOSITE CONTAINER AND CONTAINER THUS OBTAINED Download PDFInfo
- Publication number
- FR2541175A1 FR2541175A1 FR8405922A FR8405922A FR2541175A1 FR 2541175 A1 FR2541175 A1 FR 2541175A1 FR 8405922 A FR8405922 A FR 8405922A FR 8405922 A FR8405922 A FR 8405922A FR 2541175 A1 FR2541175 A1 FR 2541175A1
- Authority
- FR
- France
- Prior art keywords
- ring
- adhesive
- container
- lip
- heat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PROCEDE DE FORMAGE D'UN RECIPIENT COMPOSITE, LEQUEL COMPREND UNE PARTIE BAGUE 12 EN VERRE, LADITE BAGUE AYANT UNE LEVRE SUPERIEURE 14 DE BAGUE, CARACTERISE EN CE QU'IL CONSISTE: A.A APPLIQUER UNE COUCHE 16 D'ADHESIF THERMOSCELLABLE SUR LADITE LEVRE DE BAGUE 14, CET ADHESIF ETANT UN MELANGE D'UN SILANE ET D'UN COPOLYMERE ETHYLENEACIDE ACRYLIQUE, LEDIT COPOLYMERE AYANT UN INDICE D'ECOULEMENT A L'ETAT FONDU DE 300 AU MOINS; ET B.A SECHER CETTE COUCHE DUDIT ADHESIF THERMOSCELLABLE SUR LA LEVRE DE BAGUE. CONDITIONNEMENT ET EMBALLAGE A CHAUD DE DIVERS ALIMENTS, TELS QUE DES JUS DE FRUITS, DES CONFITURES, DES SAUCES TOMATES, ETC.PROCESS FOR FORMING A COMPOSITE CONTAINER, WHICH INCLUDES A GLASS RING PART 12, THE SAID RING HAVING A TOP LIP 14 OF RING, CHARACTERIZED IN THAT IT CONSISTS OF: APPLYING A LAYER 16 OF THERMOS-SEALABLE ADHESIVE ON THE LIP OF THE RING 14, THIS ADHESIVE BEING A MIXTURE OF A SILANE AND AN ACRYLIC ETHYLENE ACID COPOLYMER, THE COPOLYMER HAVING A MELT FLOW INDEX OF AT LEAST 300; AND B.A DRY THIS LAYER OF THE THERMOS-SEALABLE ADHESIVE ON THE RING LIP. PACKAGING AND HOT PACKAGING OF VARIOUS FOODS, SUCH AS FRUIT JUICES, JAMS, TOMATO SAUCES, ETC.
Description
_ _ 2541175_ _ 2541175
Procédé de formage d'un récipient composite et récipient obtenu. Process for forming a composite container and container obtained
La présente invention concerne un procédé de fer- The present invention relates to a method of
meture hermétique sous forme d'un couvercle non-perforé du type mince et flexible venant s'appliquer sur la lèvre de Hermetic seal in the form of a non-perforated lid of the thin and flexible type which is applied to the lip of
la bague d'un récipient en verre, le plus souvent un réci- the ring of a glass container, usually a recipe
pient à large ouverture tel qu'un bocal Normalement, les a large opening such as a jar Normally, the
procédés de ce genre impliquent l'utilisation d'un couver- processes of this kind involve the use of
cle non-perforé, mince et flexible, le plus souvent en feuille d'aluminium métallique, dont le dessous est enduit non-perforated, thin and flexible key, usually made of aluminum foil, the underside of which is coated
d'une matière thermoplastique thermoscellable, un tel cou- of a heat-sealable thermoplastic material, such a cover
vercle venant en prise solide avec la lèvre supérieure de la bague d'un récipient en verre Dans la pratique courante, la lèvre supérieure de la bague du récipient en verre est enduite d'une composition adhésive thermoscellable pouvant établir une interface entre le couvercle nonperforé mince et flexible enduit de thermoplastie et la surface en verre solidly engaging the upper lip of the ring of a glass container In current practice, the upper lip of the ring of the glass container is coated with a heat-sealable adhesive composition capable of interfacing the thin non-perforated lid and flexible coated thermoplastic and glass surface
du récipient.of the container.
Différentes façons d'aborder le problème de fer- Different ways of tackling the iron problem
meture hermétique d'un récipient contenant un aliment sec ou un produit alimentaire chargé à froid, par exemple, des soupes déshydratées, des produits laitiers réfrigérés etc. ont été expérimentées Par exemple, la demande de brevet sealing a container containing a dry food or a cold-loaded food product, for example, dehydrated soups, refrigerated dairy products, etc. have been tried for example, the patent application
britannique 2 030 103 A, décrit une feuille métallique ap- British Patent 2,030,103 A, discloses a metal foil
pliquée sur l'ouverture et la bordure d'un récipient en verre, fixé à la bordure par un adhésif activable par la chaleur, lors de l'application de chaleur et de pression pour établir une liaison entre le récipient de verre et la feuille métallique sans diffusion ou détérioration de la liaison adhésive quand le récipient contient une denrée renfermant de l'eau, un agent favorisant la liaison, tel qu'un composé organique de silicium, par exemple un silane plicated on the opening and the edge of a glass container, attached to the edge by a heat-activatable adhesive, when applying heat and pressure to establish a connection between the glass container and the metal sheet without diffusion or deterioration of the adhesive bond when the container contains a foodstuff containing water, a binding promoting agent, such as an organic silicon compound, for example a silane
ayant une affinité pour le verre, étant appliqué à la bor- having an affinity for glass, being applied to the
dure du récipient ou incorporé dans l'adhésif Il semble hard container or incorporated into the adhesive It seems
que ce procédé ne concerne pas les applications de remplis- that this process does not concern the applications of
sage à chaud.wise to hot.
-2--2-
Le brevet japonais N O J 5 077-447 concernant un ré- Japanese Patent No. 5,077,447 to a patent application
cipient avec un couvercle à ouverture facile, décrit un ré- container with an easy-open lid, describes a
cipient qu'on obtient en recouvrant une pellicule ou feuil- container obtained by covering a film or sheet of
le faite d 'un stratifié comprenant une feuille plastique ou une feuille métallique et une feuille plastique, par exem- made of a laminate comprising a plastic sheet or foil and a plastic sheet, for example
ple une matière plastique liée à chaud La matière plasti- a plastic material bonded to hot plastic material
que liée à chaud et laminée sur la feuille métallique est choisie parmi les résines oléfiniques modifiées, telles qu'une polyoléfine modifiée par un acide, un ionomère, un heat-bonded and laminated on the metal foil is selected from modified olefinic resins, such as an acid-modified polyolefin, an ionomer, a
copolymère éthylène/acétate de vinyle, un copolymère d'aci- ethylene / vinyl acetate copolymer, a copolymer of
de carboxylique à insaturation éthylénique ou de son ester, ou un mélange d'une quelconque matière énumérée, ou encore ethylenically unsaturated carboxylic acid or its ester, or a mixture of any enumerated material, or
un polyamide En outre, on prévoit une ouverture plus pe- In addition, a more
tite que le diamètre de la partie comportant une ligne d'af- tite that the diameter of the part with a line of
faiblissement devant être ouverte en service sur la portion interne du couvercle -à ouverture facile d'une manière telle, weakening to be opened in use on the inner portion of the lid -for easy opening in such a way,
que l'ouverture de petit diamètre de la pellicule ou feuil- the small diameter opening of the film or foil
le soit superposée sur la partie munie d'une ligne d'affai- superimposed on the part equipped with a business line
blissement du couvercle à ouverture facile en tournant son easy opening lid by turning its
côté pellicule plastique à liaison à chaud vers le couvercle à ouver- hot-link plastic film side to the open-top cover
tûre facile- La partie recouverte est liée par chauffage à une portion à l'extérieur de celle comportant la ligne Easy-to-cover part is connected by heating to a portion outside of the line
d'affaiblissement devant être ouverte. weakening to be opened.
La demande de brevet RFA P 28 48 568 9 décrit un procédé de fermeture hermétique des récipients en verre à The German patent application P 28 48 568 9 describes a method of hermetically sealing the glass containers to
l'aide de feuilles métalliques revêtues d'une matière syn- using metal sheets coated with a synthetic material
thétique Le procédé consiste à enduire la bordure du ré- The process consists of coating the border of the
cipient en verre avec un adhésif afin de fixer plus soli- glass container with an adhesive in order to fix more
dement la feuille métallique revêtue de matière synthéti- metal foil coated with synthetic material
que au récipient en verre L'adhésif est une solution pure- glass container The adhesive is a pure solution
ment organique ou aqueuse d'un alkyl-trialcoxy-silane, d'un organic or aqueous solution of an alkyl-trialkoxysilane, a
alkyl-trichlorosilane, dont le radical alkyle porte un sub- alkyl-trichlorosilane, the alkyl radical of which bears a sub-
c+n aç r yçe di épo vinyle, acrylo ou c + n aç r yçe di epo vinyl, acrylo or
méthacrylo ou une solution organique d'un ester d'acide ti- methacrylo or an organic solution of an acid ester
tanique monomère ou polymère On applique le revêtement, on tanic monomer or polymer The coating is applied,
le sèche et ensuite on fixe hermétiquement la feuille étan- dry it and then seal the waterproofing foil
-3 --3 -
che par une technique connue consistant à le presser con- by a known technique of pressing
tre la lèvre supérieure du récipient en verre à l'aide d'une tête de thermosoudure Pour l'alkyl-trialcoxy-silane, be the upper lip of the glass container using a heat-sealing head For the alkyl-trialkoxysilane,
l'alkyl-trichloro-silane ou un mélange d'alkyl-alcoxychlo- alkyl-trichlorosilane or a mixture of alkyl-alkoxychlo-
rosilanes, on mentionne les cétones, et surtout l'acétone, comme solvants organiques préférés Cependant, pour les esters d'acide titanique, on utilise un solvant à base de rosinanes, mention is made of ketones, and especially acetone, as preferred organic solvents. However, for the titanic acid esters, a solvent based on
benzène Chaque solvant exige l'emploi d'un composé orga- benzene Each solvent requires the use of an organic compound
nique volatil.volatile.
Le brevet britannique 1 538 642 décrit un réci- British Patent 1,538,642 discloses a recipe
pient hermétiquement fermé comprenant un bocal en verre ayant une ouverture présentant une surface orientée vers le haut, une membrane en feuille métallique s'étendant sur hermetically sealed container comprising a glass jar having an opening having an upwardly facing surface, a metal foil membrane extending over
l'ouverture du récipient et thermiquement scellée à celle- the opening of the container and thermally sealed to that
ci et un capuchon à déclic en matière plastique déformable ci and a click cap made of deformable plastic material
par la-pression et la chaleur sur l'ouverture et la membra- by pressure and heat on the opening and the membrane
ne en feuille, l'ouverture du récipient comportant un bour- sheet, the opening of the container comprising a bunker
relet surélevé sur sa surface orientée vers le haut et raised on its surface facing upward and
s'étendant continuellement autour de l'ouverture, le capu- continually extending around the opening, the capu-
chon ayant une épaisseur sur la surface orientée vers l'ex- chon having a thickness on the surface facing the
térieur au moins double de la hauteur du bourrelet, le at least twice the height of the bead, the
bourrelet et l'élément feuille étant emboutis dans la ma- bead and the sheet element being embossed into the
tière plastique du capuchon à déclic La membrane en feuil- snap-cap plastic cap The membrane made of
le métallique peut comporter une résine de copolymère éthy- the metal may comprise an ethylene copolymer resin
lène/acide acrylique ayant une température d'activation de à 163 C à titre de sous-couche pour un contact intime lene / acrylic acid having an activation temperature of 163 C as an undercoat for intimate contact
entre la membrane en feuille et le bourrelet du récipient. between the sheet membrane and the bead of the container.
Le brevet RFA DE 3 011 761 Ai intitulé "Method for German Patent DE 3,011,761 Ai entitled "Method for
the joining of Substrates by Heat Sealing" basé sur le dos- the joining of Substrates by Heat Sealing "based on the back-
sier N O P 3 011 761 4-43, décrit un procédé de jonction No. 3,011,761,443, discloses a method of joining
étanche du verre au verre ou du verre au métal afin de for- sealed glass to glass or glass to metal in order to
mer un emballage pouvant contenir des soupes déshydratées, des yaourts ou d'autre produits alimentaires chargés à packaging that may contain dehydrated soups, yogurts or other
froid On fixe ensemble le récipient et le couvercle à l'ai- The container and lid are fixed together
de d'un adhésif thermoscellable qui a été préparé par hy- of a heat-sealable adhesive that has been prepared by
drolyse et polycondensation de: 4 - a) au moins un organosiloxane de formule générale (I): R Si X 4 m (I) dans laquelle R désigne un radical alkyle, alcényle, aryle, alkylaryle ou arylalkyle; X désigne un atome d'hydrogène S ou d'halogène ou un radical hydroxyle, alcoxy, acyloxy ou 11; -NR 12 (R = hydrogène et/ou radical alkyle) et m = 1,2 ou 3, et au moins l'un des composés suivants (b) (c) et/ou (d); b) un ou plusieurs silanes à fonction silicium de formule générale (II): Si X 4 (II) drolysis and polycondensation of: 4 - a) at least one organosiloxane of general formula (I): R Si X 4 m (I) wherein R denotes an alkyl, alkenyl, aryl, alkylaryl or arylalkyl radical; X denotes a hydrogen atom S or halogen or a hydroxyl, alkoxy, acyloxy or 11 radical; -NR 12 (R = hydrogen and / or alkyl radical) and m = 1,2 or 3, and at least one of the following compounds (b) (c) and / or (d); b) one or more silanes with a silicon function of general formula (II): Si X 4 (II)
dans laquelle X est tel que défini plus haut mais les au- where X is as defined above but the
tres ne sont pas tous de l'hydrogène; not all are hydrogen;
c) un ou plusieurs oxydes difficilement volatilisables, so- (c) one or more oxides which are difficult to volatilize,
lubles dans le milieu réactionnel ou bien un ou plusieurs composés d'un élément des groupes principaux Ia à Va ou des in the reaction medium or one or more compounds of an element from main groups Ia to Va or
groupes secondaires I Vb ou Vb de la Classification Pério- secondary groups I Vb or Vb of the Periodic Classification
dique des Eléments, formant un tel oxyde difficilement vo- of the Elements, forming such an oxide with difficulty
latilisable; d) un ou plusieurs silanes à fonction organique répondant à la formule générale (III): Rn(R"Y)psix ( 4-n-p) (III) latilisable; d) one or more organic-functional silanes having the general formula (III): Rn (R "Y) psix (4-n-p) (III)
dans laquelle R et X ont la même signification que ci-des- in which R and X have the same meaning as above
sus; R" représente un radical alkylène à chaîne droite ou ramifiée pouvant être interrompue par des atomes d'oxygène ou de soufre ou par des groupes NH, un radical phénylène, alkylphénylène ou alkylènephénylène; Y désigne un atome addition; R "represents a straight or branched chain alkylene radical which may be interrupted by oxygen or sulfur atoms or by NH groups, a phenylene, alkylphenylene or alkylenephenylene radical; Y denotes an atom
d'halogène ou, dans un cas donné, un groupe amino substi- halogen or, in a given case, a substituted amino group
tué ou, dans un cas donné, un groupe anilino substitué, al- killed or, in any given case, a substituted anilino group,
déhyde, céto, carboxyle, hydroxyle, mercapto, cyano, hydro- dehyde, keto, carboxyl, hydroxyl, mercapto, cyano, hydro-
xyphényle, acide carboxylique, ester alkylique, acide sul- xyphenyl, carboxylic acid, alkyl ester, sulfuric acid,
fonique, acide phosphorique, acryloxy, méthacryloxy, gly- fonic, phosphoric acid, acryloxy, methacryloxy, gly-
cidyloxy, époxyde ou vinyle, N est égal à 0, 1 ou 2, et p cidyloxy, epoxide or vinyl, N is 0, 1 or 2, and p
est égal à 1, 2 ou 3, la somme N + p = 1, 2 ou 3; en pré- is equal to 1, 2 or 3, the sum N + p = 1, 2 or 3; in pre-
sence de la quantité d'eau stoéchiométriquement nécessaire -5- the amount of stoichiometrically required water -5-
pour l'hydrolyse ainsi que, dans un cas donné de condensa- for hydrolysis and, in a given case of condensation,
tion, d'un catalyseur et/ou d'un solvant, alors que dans of a catalyst and / or a solvent, while in
le cas des composants de départ (a) et (b), on peut égale- the case of the starting components (a) and (b), we can also
ment utiliser les oligomères de ces silanes qui sont so- use the oligomers of these silanes which are
lubles dans le milieu de réaction. Un certain nombre de problèmes se sont posés dans luble in the reaction medium. A number of problems have arisen in
les techniques décrites ci-dessus concernant le remplis- the techniques described above concerning the fulfillment
sage à chaud des aliments Par exemple, lorsqu'on effectue de la façondécrite ci-dessus le remplissage à chaud de produits alimentaires acides tels que le jus d'orange, ou le remplissage à chaud d'aliments non acides tels que des gelées, des confitures, des sauces tomate, des ketchups et similaires, dans des récipients en verre en utilisant For example, when performing the above-described manner hot-filling of acidic food products such as orange juice, or hot filling of non-acidic foods such jams, tomato sauces, ketchups and the like, in glass containers using
l'adhésif décrit plus haut et de minces couvercles métal- the adhesive described above and thin metal lids
liques revêtus d'une matière plastique, également comme expliqué plus haut, on se heurte à divers problèmes Un plastic coated, also as explained above, there are various problems
problème critique est la libération prématurée du couver- critical problem is the premature release of
cle de l'adhésif thermoscellable sur la-lèvre de bague du récipient de verre immédiatement après le remplissage, la fermeture hermétique et le tranisfert de l'emballage à un poste de refroidissement Pendant le remplissage à chaud, heat-sealing adhesive on the lip of the glass container ring immediately after filling, sealing and transferring the packaging to a cooling station.
le récipient est chauffé par son contenu introduit à chaud. the container is heated by its hot-introduced contents.
De même, alors que la tête de scellement par la chaleur et Similarly, while the sealing head by heat and
la pression applique hermétiquement le couvercle sur le ré- the pressure tightly applies the lid to the
cipient, cette tête amène une quantité non négligeable de chaleur supplémentaire à l'emballage Cet apport combiné de chaleur provoque l'évaporation d'une partie de leau à container, this head brings a significant amount of additional heat to the packaging This combined heat supply causes the evaporation of some of the water to
l'intérieur de l'emballage Cette pression de vapeur provo- inside the packaging This vapor pressure provokes
que un gouflement vers l'extérieur du couvercle métallique mince Cette force et le gonflement du couvercle provoquent la libération prématurée du couvercle dans un pourcentage inacceptable de cas Pendnat les ultimes stades d'un tel procédé de refroidissement, lorsque la chaleur admise est finalement perdue, un vide partiel s'établit à l'intérieur This force and the swelling of the lid cause the premature release of the lid in an unacceptable percentage of cases. The last stages of such a cooling process occur when the heat admitted is finally lost. a partial vacuum is established inside
du récipient et le couvercle s'affaisse vers l'intérieur. of the container and the lid sinks inwards.
Ce vide provoque une contrainte accrue sur le joint entre -6- This vacuum causes increased stress on the seal between -6-
le couvercle en feuille métallique, l'adhésif thermoscel- the foil lid, the thermoset adhesive
lable appliqué sur la lèvre de bague et la lèvre de bague du récipient en verre On observe de nombreuses ruptures lable applied to the lip of the ring and the lip of the ring of the glass container There are many breaks
du joint lorsqu'on utilise, pour des applications de rem- seal when using, for
plissage à chaud, des adhésifs et des procédés qui con- viennent parfaitement pour les applications de remplissage à froid De telles ruptures du joint sont à l'origine de fuites dans l'emballage et son contenu est contaminé et Hot crimping, adhesives, and processes that are ideal for cold fill applications. Such seal failures cause leakage in the package and its contents are contaminated.
donc invendable.therefore unsellable.
D'autre part, après un stockage de longue durée, On the other hand, after long-term storage,
allant de quelques mois à un an, les emballages font ap- from a few months to a year, packaging
paraitre des fuites par suite de l'instabilité au stockage à long terme des adhésifs utilisés quand ils sont mis en contact avec des aliments très humides, de sorte que la leakage as a result of the long-term storage instability of the adhesives used when they come into contact with very moist foods, so that
contamination atmosphérique pénètre dans l'emballage con- atmospheric contamination enters the packaging
tenant l'aliment et le produit devient encore une fois in- holding the food and the product becomes once again
vendable Ce manque de durabilité au stockage à long terme salable This lack of durability in long-term storage
de l'emballage est particulièrement critique dans les ap- packaging is particularly critical in
plications des aliments chargés à chaud qui, normalement, of hot-loaded foods that normally
peuvent rester longtemps sur les rayons du magasin D'au- can stay on the shelves of the store for a long time
tre part, les emballages alimentaires remplis à chaud lais- on the other hand, hot-filled food packaging
sent apparaître un vide partiel à l'intérieur du récipient ce qui augmente la contrainte mécanique s'exerçant sur la liaison entre le mince couvercle métallique flexible, l'adhésif thermoscellable et la lèvre de bague du récipient there is a partial vacuum inside the container which increases the mechanical stress on the connection between the thin flexible metal lid, the heat-sealable adhesive and the lip of the container ring
en verre.glass.
Egalement, de nombreux adhésifs décrits plus haut Also, many adhesives described above
ne possèdent pas davantage de caractéristiques de résistan- do not have more resistance characteristics
ce à long terme aux produits, surtout quand on les met en contact avec les produits alimentaires très acides, très humides, tels que des jus de fruits et des aliments à base de tomates Ainsi, les adhésifs thermoscellables eux-mêmes perdent leur aptitude à fermer hermétiquementl'emballage pendant un stockage de longue durée sous contrainte et au contact des aliments Par ailleurs, de nombreux procédés d'usage courant exigent l'enduction en couches séparées multiples de solutions différentes, par exemple d'adhésifs, d'agents de réticulation, d'agents de liaison, etc sur la long-term products, especially when put in contact with very acidic, very wet food products, such as fruit juices and tomato-based foods Thus, heat-sealable adhesives themselves lose their ability to close In addition, many commonly used methods require multiple layer coatings of different solutions, for example adhesives, crosslinking agents, and the like. liaison officers, etc. on the
lèvre de bague du récipient Ceci nécessite des stades sup- container ring lip This requires additional stages
plémentaires de traitement et une mise de fonds initiale sensiblement plus élevée pour l'achat des machines et aussi un grand nombre de solutions différentes Ces solutions additional processing and a significantly higher initial investment for the purchase of the machines and also a large number of different solutions
exigent du temps pour les mélanger, sont fréquemment ins- require time to mix, are frequently
tables au stoc 1 çage et contiennent le plus souvent des sol- storing tables and most often contain
vants organiques Dans de nombreux cas, ces solvants ne In many cases, these solvents
sont pas acceptés pour le contact avec les aliments D'au- are not accepted for contact with food
tre part, les composés adhésifs à base de solvants obli- on the other hand, the solvent-based adhesive compounds
gent à créer une protection spéciale pour le personnel et. to create special protection for the staff and.
des moyens pour le contrôle de l'environnement, des'équipe- means for the control of the environment, the team
ments et des techniques spéciaux qui militent contre leur emploi dans de nombreux cas Il est évident que l'emploi and special techniques that militate against their use in many cases It is obvious that employment
d'un équipement de contrôle de la pollution de l'environ- environmental pollution control equipment
nement est fâcheux sur le plan de la fabrication à peu de frais de produits alimentaires chargés à chaud Il existe donc un besoin dans cette industrie pour un procédé et des compositions supplémentaires d'adhésifs thermoscellables There is therefore a need in this industry for an additional process and compositions of heat-sealable adhesives.
permettant le remplissage à chaud des aliments, de carac- allowing the hot filling of foodstuffs,
tère simple, fiable, exempt de vapeurs organiques et per- simple, reliable, free from organic vapors and
mettant d'obtenir après refroidissement un emballage sta- to obtain after cooling a stable packaging
ble et restant stable pendant une longue durée de conser- and stable for a long period of storage.
vation.vation.
La présente invention a pour but de fournir un ré- The object of the present invention is to provide a
cipient hermétiquement fermé et un procédé de fabrication hermetically sealed container and method of manufacture
de celui-ci, approprié pour contenir des produits alimen- of it, suitable for containing food products
taires chargés ou conditionnés à chaud, ce récipient pos- charged or hot-packed, this receptacle
sédant une-résistance accrue à l'apparition de fuites après sedating an increased resistance to the appearance of leaks after
avoir été rempli d'un produit alimentaire chaud, après l'ap- filled with a hot food product, after the application
plication du couvercle et le refroidissement à la tempéra- lid and cooling at room temperature.
ture ambiante.ambient temperature.
L'invention a encore pour objet un récipient fer- Another subject of the invention is a closed container
mé et son procédé de fabrication, approprié pour contenir des produits alimentaires conditionnés à chaud, récipient -8- qui possède une meilleure résistance aux contraintes lors du stockage à long terme sans faire apparaître de fuites entre la couche adhésive thermoscellable et le récipient en and its method of manufacture, suitable for containing hot-packaged food products, which container has better resistance to stress during long-term storage without causing leakage between the heat-sealable adhesive layer and the container.
verre ou son mince couvercle flexible. glass or its thin flexible lid.
Pour réaliser les avantages de l'invention qui ont To realize the advantages of the invention which have
été indiqués et aussi certains autres, on utilise un pro- have been indicated and also some others, we use a
cédé de fermeture hermétique d'un récipient en verre, ré- hermetically sealed closure of a glass container,
cipient qui présente une partie supérieure de bague se container which has an upper part of a ring
terminant par une partie bordure ou lèvre de bague, le pro- ending with a border portion or lip of a ring, the
cédé consistant à chauffer au moins la partie lèvre de ba- to heat at least the lip portion of
gue du récipient en verre à une température élevée pendant une durée suffisante et à une température suffisante pour glass vessel at a high temperature for a sufficient time and at a temperature sufficient to
oxyder les matières organiques éventuelles formant un en- to oxidize any organic matter forming a
duit sur la lèvre de la bague Ultérieurement, on applique duit on the lip of the ring Subsequently, apply
au moins une couche d'un adhésif thermoscellable sur la lè- at least one layer of heat-sealable adhesive on the
vre supérieure de la bague, ledit adhésif thermoscellable devant ultérieurement établir une liaison entre un mince couvercle métallique flexible ayant reçu un revêtement top of the ring, said heat-sealable adhesive to be subsequently bonded between a thin, flexible metal cover having been coated
d'une matière organique thermoplastique et la lèvre supé- of a thermoplastic organic material and the upper lip
rieure de bague du récipient en verre L'adhésif thermo- the glass container ring
scellable, selon la présente invention, est un mélange sealable, according to the present invention, is a mixture
aqueux d'un silane et d'un copolymère éthylène/acide acry- of a silane and an ethylene / acrylic acid copolymer.
lique, ledit copolymère ayant un indice d'écoulement à same, said copolymer having a flow index at
l'état fondu d'environ 300 ou plus faible Après l'appli- the molten state of about 300 or lower After the application
cation de l'adhésif thermoscellable, on sèche l'adhésif et cation of the heat-sealable adhesive, the adhesive is dried and
on presse un couvercle mince non-perforé qui est un stra- a thin, non-perforated lid is pressed which is a
tifié métal/plastique contre le récipient en verre et on metal / plastic container against the glass container and
effectue la fermeture hermétique par la chaleur et la pres- hermetically seal with heat and pressure.
sion en utilisant des moyens classiques de scellement ther- using conventional means of heat sealing
mique sous pression.under pressure.
Le récipient formé selon la présente invention con- The container formed according to the present invention
vient particulièrement pour recevoir des produits alimen- comes especially to receive food products
taires conditionnés à chaud et il fait preuve d'une résis- hot-rolled and shows resistance
tance élevée à l'apparition des fuites pendant le remplis- high level of leakage during filling
sage, la fermeture hermétique et le procédé de refroidis- the hermetic seal and the cooling process
sement, et il est, d'autre part, d'une remarquable résis- and, on the other hand, is remarkably resilient
99 _ tance à l'apparition des fuites pendant le stockage à long 99 _ tance to the appearance of leaks during long storage
terme ou la manutention.term or handling.
D'autres buts, caractéristiques et avantages de Other goals, features and benefits of
l'invention ressortiront de la description détaillée qui the invention will emerge from the detailed description which
va suivre en regard des dessins annexés sur lesquels: la figure 1 est une vue éclatée d'un couvercle will follow with reference to the accompanying drawings, in which: FIG. 1 is an exploded view of a lid
flexible en un stratifié d'une feuille métallique non-per- flexible in a laminate of a non-per-
forée et d'une pellicule thermoplastique et montrant éga- drilled and a thermoplastic film and also showing
lement la lèvre de bague supérieure, enduite de l'adhésif thermoscellable, d'un récipient en verre; za figure 2 est une vue schématique du procédé de la présente invention pour préparer, remplir et fermer hermétiquement l'emballage selon la présente invention; et la figure 3 est une vue schématique du procédé pour refroidir les récipients remplis à chaud comportant l'adhésif thermoscellable perfectionné qui fait l'objet de the upper ring lip, coated with the heat-sealable adhesive, of a glass container; Fig. 2 is a schematic view of the process of the present invention for preparing, filling and sealing the package according to the present invention; and Fig. 3 is a schematic view of the method for cooling hot filled containers having the improved heat sealable adhesive which is the subject of
la présente invention.the present invention.
Le mode de réalisation préféré de la présente in- The preferred embodiment of the present invention
vention est représenté à titre d'exemple sur les figures 1 à 3 Sur la figure 1, on voit un récipient en verre, en coupe partielle, portant la référence d'ensemble 10 Le The invention is illustrated by way of example in FIGS. 1 to 3. FIG. 1 shows a partially cut glass container with the reference numeral 10.
récipient en verre 10 se termine par une partie bague supé- glass container 10 terminates in an upper ring
rieure 12 qui définit une ouverture dans le récipient 10. 12 which defines an opening in the container 10.
Dans sa partie la plus haute, la partie bague 12 se termine par une partie lèvre 14 de la bague Normalement, la partie In its highest part, the ring portion 12 ends with a lip portion 14 of the ring.
lèvre 14 de la bague est une partie plate ou légèrement ar- lip 14 of the ring is a flat or slightly
rondie comme il est courant avec des récipients en verre à rounded as is common with glass containers to
large ouverture Une mince couche d'un adhésif thermoscel- wide opening A thin layer of a thermoset adhesive
lable 16 est placée sur la partie lèvre 14 de la bague du récipient 10 Un couvercle mince non-perforé flexible du type membrane 18 ayant une géométrie complémentaire à celle de la partie bague 12 du récipient 10 est monté au-dessus lable 16 is placed on the lip portion 14 of the container ring 10 A membrane-type flexible non-perforated thin cover 18 having a geometry complementary to that of the ring portion 12 of the container 10 is mounted above
du récipient et peut être fixé à la partie bague 12 du ré- of the container and can be attached to the ring part 12 of the
cipient 10 par contact entre le couvercle 18 et la partie lèvre 14 de la bague Normalement, le couvercle 18 comprend 10 by contact between the cover 18 and the lip portion 14 of the ring Normally, the cover 18 comprises
une partie 20 en feuille métallique et une partie 22 en pel- a metal sheet portion 20 and a pelvic portion 22
- licule thermoplastique thermoscellable La partie 22 en pellicule thermoscellable peut elle-même être un stratifié Thermoseal thermoplastic heat seal Part 22 in heat-sealable film may itself be a laminate
assemblé par stratification comme on le verra plus loin. assembled by stratification as will be seen later.
Dans le mode de réalisation préféré de l'inven- In the preferred embodiment of the invention
tion, l'adhésif thermoscellable 16 comprend un mélange d'un composé de silane et d'un copolymère éthylène/acide In one embodiment, the heat-sealable adhesive 16 comprises a mixture of a silane compound and an ethylene / acid copolymer.
acrylique contenant 80 % d'éthylène et 20 % d'acide acry- acrylic containing 80% ethylene and 20% acrylic acid.
lique, en poids, dans la structure du copolymère et ayant by weight in the copolymer structure and having
un indice d'écoulement à l'état fondu inférieur à 300. a melt flow index of less than 300.
L'indice d'écoulement à l'état fondu particulièrement pré- The melt flow index particularly
féré est d'environ 75 On a établi selon la présente in- is about 75
vention qu'un copolymère éthylène/acide acrylique ayant un indice d'écoulement à I'état fondu de 75 à 300 procure un an ethylene / acrylic acid copolymer having a melt flow index of 75 to 300 provides a
excellent adhésif thermoscellable ayant une résistance éle- excellent heat-sealable adhesive with high resistance
vée de collage à chaud et pouvant servir dans le traitement des aliments conditionnés à chaud sans utiliser de solvants hot-melt glue which can be used in the processing of hot-packaged food without the use of solvents
organiques dans l'adhésif.organic in the adhesive.
Dans le présent mémoire, l'indice d'écoulement à l'état fondu est défini comme la quantité (en grammes) d'une résine thermoplastique qu'on peut forcer à travers un orifice de 2,1 mm quand on la soumet à une force de In this specification, the melt flow index is defined as the amount (in grams) of a thermoplastic resin that can be forced through a 2.1 mm orifice when subjected to strength of
2160 g, en 10 minutes, à 190 C.2160 g, in 10 minutes, at 190 C.
Un composé préféré du silane est le "Silane A 1120 " organo-fonctionnel (marque déposée de l'Union-Carbide) et qui est un N-(e-amino-éthyl)yamino-propyl-triméthoxysilane, qui est un silane à fonction diamino Ce silane préféré A preferred silane compound is the organofunctional "Silane A 1120" (Trade Mark of Union Carbide), which is a N- (e-aminoethyl) -amino-propyltrimethoxysilane, which is a functional silane. diamino This favorite silane
est soluble dans l'eau ce qui le rend particulièrement ap- is soluble in water which makes it particularly suitable
proprié pour les applications dans l'emballage d'aliments à remplissage à chaud, avec impossibilité d'employer des suitable for applications in hot-fill food packaging, with the impossibility of using
solvants organiques dans la composition de l'adhésif ther- organic solvents in the composition of the heat adhesive
moscellable Tous les composants de l'adhésif doivent être de nature à permettre leur contact avec les aliments selon moscellable All components of the adhesive must be such as to allow their contact with food
les règlements de la FDA et la plupart des solvants organi- FDA regulations and most organic solvents
ques ne sont pas acceptés Le silane préféré est un liquide are not accepted The preferred silane is a liquid
de couleur paille ayant une densité de 1,03 à 25 C, un in- of straw color having a density of 1.03 to 25 C, a
dice de réfraction de 1,448 (n D 25 C) et un point éclair de 11 - refractive index of 1.448 (n D 25 C) and a flash point of 11 -
138 C.138 C.
Le copolymère préféré éthylène/acide-acrylique. The preferred ethylene / acrylic acid copolymer.
présente un indice d'écoulement à l'état fondu d'environ has a melt flow index of about
300 ou plus bas et est capable de former à température am- 300 or lower and is able to train at ambient temperature
biante des dispersions à base d'eau exemptes de solvants organiques Une telle résine est abondamment disponible water-based dispersions free of organic solvents Such a resin is abundantly available
chez Dow Chemical Company sous le nom de Produit N O PE 483. at Dow Chemical Company as Product No. PE 483.
Une résine encore plus avantageuse est un copolymère éthy- An even more advantageous resin is an ethylene copolymer
lène/acide acrylique ayant un indice d'écoulement à l'état lene / acrylic acid having a flow index in the state
fondu d'environ 75.melted about 75.
* La feuille métallique 20 du couvercle 18 est en métal aluminium ayant une épaisseur de 38 à 63 microns La pellicule 22 thermoplastique et thermoscellable laminée sur la feuille métallique 20 peut être une matière "Surlyn"The metal foil 20 of the lid 18 is made of aluminum metal having a thickness of 38 to 63 microns. The thermoplastic and heat-sealable film 22 laminated on the metal foil 20 may be a "Surlyn" material.
(marque déposée) fournie par E I du Pont de Nemours & Com- (registered trademark) provided by E I du Pont de Nemours & Com-
pany) à savoir un copolymère éthylène/acide acrylique ayant un indice d'écoulement à l'état fondu désiré quelconque ou pany) namely an ethylene / acrylic acid copolymer having any desired melt flow index or
une structure stratifié comportant un polymère de nitrocel- a laminate structure comprising a nitrocel-
lulose en contact avec la pellicule d'aluminium et lui- lulose in contact with the aluminum film and
même revêtu avec un polymère de polyvinyl-butyral pour éta- even coated with a polyvinyl butyral polymer for
blir un stratifié aluminium/nitrocellulose/polyvinylbuty- aluminum / nitrocellulose / polyvinylbuty-
ral Une matière préférée est le "Surlyn" qualité N O 1652 qui est une résine ionomère ayant des contre-ions de zinc avec un indice d'écoulement à l'état fondu de 5,0 Les trois couvercles 18 décrits ci-dessus conviennent tous pour utilisation avec l'adhésif thermoscellable perfectionné A preferred material is "Surlyn" grade No. 1652 which is an ionomeric resin having zinc counter-ions with a melt flow index of 5.0. The three lids 18 described above are all suitable for use with advanced heat seal adhesive
selon l'invention Chaque couvercle peut former d'excel- According to the invention, each lid can form excel-
lents emballages remplis à chaud avec le nouvel adhésif décrit, faisant preuve d'une stabilité à court terme lors slow, hot-filled packaging with the new adhesive described, showing short-term stability
du refroidissement depuis la température élevée du remplis- cooling since the high temperature of the
sage à chaud jusqu'à la température ambiante et aussi une excellente durabilité à long terme sans faire apparaître wise to warm up to room temperature and also excellent long-term durability without showing up
une proportion importante de fuites dans les récipients. a significant proportion of leaks in the containers.
Le procédé selon la présente invention pour pré- The method according to the present invention for
parer et remplir des récipients 10 est plus clairement re- parry and fill containers 10 is more clearly
présenté sur la figure 2 Un poste 24 de distribution de 12- shown in Figure 2 A 24 Distribution Station 12-
récipients traités procure une distribution continue de ré- treated containers provides a continuous distribution of
cipients en verre 10 pour utilisation dans le procédé de la présente invention Les récipients 10 fournis par le poste 24 sont traités selon les techniques classiques de fabrication de récipients en verre, c'est-à- dire que la surface a été traitée sur l'extérieur du récipient 10 par Glass containers 10 for use in the process of the present invention The containers 10 provided by the station 24 are processed according to conventional glass container manufacturing techniques, i.e. the surface has been treated on the outside the container 10 by
des combinaisons d'enduits transparents minces Fréquem- combinations of thin transparent coatings Frequency-
ment, de tels récipients sont traités avec le tétrachlo- such containers are treated with tetrachloro-
rure d'étain pour former ce que l'on appelle un "revêtement terminal à chaud" pendant que les récipients 10 possèdent une chaleur considérable de fabrication Les récipients 10 This is known as a "hot end coating" while the containers 10 have a considerable heat of manufacture. The containers 10
sont encore enduits de couches de polyéthylène, acide olé- are still coated with layers of polyethylene,
ique ou autre matière organique lubrifiante qu'on applique or other organic lubricant that is applied
sous forme de ce que l'on appelle des "traitements termi- in the form of what are known as "terminating
naux à froid" pour améliorer la résistance à la rayure par contact On a découvert selon la présente invention que les According to the present invention, it has been discovered that
récipients doivent être avantageusement traités, pour abou- containers must be advantageously treated, in order to
tir à des résultats optimaux, afin d'enlever ou sensible- firing at optimal results, in order to remove or
ment oxyder les matériaux des traitements terminaux à froid tels que l'acide oléique, avant l'application de la oxidation of cold end-processing materials such as oleic acid, before application of the
couche adhésive thermoscellable 16. heat sealable adhesive layer 16.
Le stade de traitement à la flamme 26 termine l'en- The stage of flame treatment 26 ends the
lèvement oxydant total ou partiel des matières lubrifiantes des traitements terminaux à froid en soumettant au moins la partie lèvre 14 de la bague du récipient 10 à une flamme à total or partial oxidative removal of the lubricating materials of the cold end treatments by subjecting at least the lip portion 14 of the ring of the container 10 to a flame at
haute teneur en oxygène pour oxyder les matières des trai- high oxygen content to oxidize the materials of the
tements terminaux à froid Normalement, on élève la tempé- cold endings Normally, the temperature is raised
rature de la partie lèvre 14 de la bague à environ 1490 C pendant quelques secondes pour éliminer efficacement une erase the lip portion 14 of the ring at about 1490 C for a few seconds to effectively eliminate a
quantité importante de la matière des traitements termi- significant amount of the material of the terminating
naux à froid On a également déterminé, selon la présente invention, qu'on améliore la stabilité au stockage à long terme et la résistance aux fuites de l'emballage si l'on soumet la partie lèvre 14 de la bague à plusieurs flammes en série Par exemple, la partie lèvre 14 de la bague ou ce qu'on appelle l'ouverture du récipient 10 passe sous une 13- série linéaire de brûleurs à gaz du type à rampe produisant une flamme de gaz riche en oxygène pour oxyder ou brûler les composants organiques du traitement terminal à froid précité sur la partie lèvre 14 de la bague Dans le mode de mise en òuvre préféré de l'invention, trois brûleurs à gaz du type à rampe dirigés contre la partie lèvre 14 de la bague enlèvent suffisamment de la matière du traitement terminal à froid pour faciliter la possibilité d'action de According to the present invention, it has also been determined that the long-term storage stability and leakage resistance of the package is improved by subjecting the lip portion 14 of the multi-flame ring in series. For example, the lip portion 14 of the ring or so-called opening of the container 10 passes under a linear 13-series of ramp-type gas burners producing a flame of oxygen-rich gas to oxidize or burn the gases. In the preferred embodiment of the invention, three ramp-type gas burners directed against the lip portion 14 of the ring remove sufficient organic material from the aforementioned cold end treatment on the lip portion 14 of the ring. cold end-processing to facilitate the possibility of
la couche adhésive thermoscellable 16 pendant le remplis- the heat-sealable adhesive layer 16 during filling
sage ultérieur, le refroidissement et le stockage à long terme. Après le stade 26 de traitement à la f lamme, on place avantageusement les récipients 10 dans un stade de subsequent wise, cooling and long-term storage. After the stage of treatment with the flame, the containers 10 are advantageously placed in a stage of
refroidissement 28 o la partie lèvre 14 de la bague se re- cooling 28 o the lip portion 14 of the ring is
froidit depuis environ 3000 C jusqu'à une température d'en- has been cold since about 3000 C to a temperature of
viron 50 à 600 C Une telle température plus basse facilite l'application de l'adhésif thermoscellable décrit mais ne retarde pas notablement le traitement des récipients 10 comme il serait nécessaire si les récipients 10 devaient This lower temperature facilitates the application of the heat-sealable adhesive described but does not significantly delay the treatment of the containers 10 as would be necessary if the containers 10 were to be heated.
revenir à la température ambiante. return to room temperature.
Après le stade de refroidissement 28, les réci- After the cooling stage 28, the reci-
pients 10 sont transférés à un stade 30 d'application de 10 are transferred to an application stage of
l'adhésif o une couche d'adhésif thermoscellable est ap- the adhesive o a layer of heat-sealable adhesive is
pliquée sur la partie lèvre 14 de la bague pour former une fine pellicule ayant environ 50 microns d'épaisseur On plicated on the lip portion 14 of the ring to form a thin film having about 50 microns thick On
peut utiliser toutes les techniques classiques d'applica- can use all the standard techniques of application
tion; cependant, un dispositif d'enduction aérien à rou- tion; however, a roll-over air coating device
leaux, approprié pour une application continue d'adhésif sur une rangée linéaire de récipients 10 est préféré Un Suitable for continuous application of adhesive on a linear row of containers is preferred.
tel dispositif d'enduction aérien à rouleaux comprend nor- such a roller air coating device normally comprises
malement un rouleau cylindrique en caoutchouc ou en un au- wrongly a cylindrical rubber roller or a
tre matériau élastique, qui est tiré vers le bas par un res- elastic material, which is drawn downwards by a res-
sort pour venir en contact forcé avec la partie 14 de la bague durécipient lors de son passage sous le rouleau Les to come into forced contact with the portion 14 of the container ring during its passage under the roller
rouleaux sont normalement montés transversalement à la di- rollers are normally mounted transversely to the di-
rection de la progression des récipients et sont étudiés 14 - pour appliquer environ 0,025 mg/m M 2 équivalent d'enduit séché par contact avec la partie lèvre 14 de la bague On peut utiliser des poids d'enduit aussi faibles que 0,0075 recency of the progression of the containers and are studied 14 - to apply about 0.025 mg / m 2 M equivalent of dried coating by contact with the lip portion 14 of the ring Can be used coating weights as low as 0.0075
mg/mm 2 mais une charge aussi faible ne compense pas tou- mg / mm 2 but such a low load does not always compensate
jours les irrégularités de surface dans la géométrie de la lèvre de la bague Des poids de plus de 0,015 mg/mm 2 sont préférés Une limite supérieure pratique est d'environ days surface irregularities in the geometry of the lip of the ring Weights greater than 0.015 mg / mm 2 are preferred A practical upper limit is about
0,08 mg/mm 2.0.08 mg / mm 2.
Après le stade 30 d'application de l'adhésif, on transfère les récipients à un stade de séchage 32 o à After the adhesive application stage, the containers are transferred to a drying stage 32 o.
lieu un séchage forcé de la couche adhésive thermoscella- forced drying of the heat-sealing adhesive layer
ble 16 Dans la mise en oeuvre préférée de l'invention, on utilise une rangée de dispositifs de chauffage I R au quartz fournissant de l'énergie rayonnante de 1,15 micron aux récipients 10 pour les élever en un très bref laps de temps, par exemple de 6 secondes à environ 720 C Une telle température déshydrate thermiquement le composé adhésif et l'oblige à former un joint tenace avec la partie lèvre 14 In the preferred embodiment of the invention, a row of quartz IR heaters providing radiant energy of 1.15 micron is used to the containers 10 to raise them in a very short time, for example. example of 6 seconds at about 720 C Such a temperature thermally dehydrates the adhesive compound and forces it to form a stubborn seal with the lip portion 14
de la bague.of the ring.
Après l'enduction initiale et les stades de sé- After the initial coating and the stages of
chage, l'article résultant est un récipient en verre por- the resulting article is a glass container
tant un revêtement en adhésif thermoscellable séché sur la both a heat sealable adhesive coating dried on the
lèvre de la bague Un tel article est un récipient compo- lip of the ring Such an article is a container made
site qui est stable au stockage et peut être expédié comme un article commercial séparé à un atelier de remplissage site that is stable in storage and can be shipped as a separate commercial item to a filling shop
ou bien il peut être rempli immédiatement. or it can be filled immediately.
Pour de nombreuses applications, lorsqu'on doit For many applications, when
utiliser des produits alimentaires très difficiles à con- use food products that are very difficult to
server, on préfère que les récipients séchés et enduits, à leur sortie du stade de séchage 32, soient recyclés par it is preferred that the dried and coated containers, on leaving the drying stage 32, be recycled by
une boucle de retour 33 au poste d'application 30 de l'adhé- a return loop 33 at the application station 30 of the adhesive
sif pour une seconde application d'adhésif qui, séché, équi- for a second application of adhesive which, when dried,
vaut à une couche de 0,025 mg/mm 2, avec ensuite un nouveau is equivalent to one layer of 0.025 mg / mm 2, followed by a new
passage par le stade de séchage 32 pour effectuer une se- passing through the drying stage 32 to perform a se-
conde opération de séchage au cours de laquelle la seconde couche d'adhésif est séchée pour venir en contact tenace et - étanche avec la première couche d'adhésif Alors que pour drying process during which the second layer of adhesive is dried to come into tough and sealed contact with the first layer of adhesive;
de nombreuses applications il n'est pas nécessaire d'effec- many applications it is not necessary to
tuer un double revêtement de la partie lèvre 14 de la ba- kill a double coating of the lip part 14 of the
gue si la lèvre est très plate, quand les lèvres de bague sont un peu irrégulières, comme il est courant avec les if the lip is very flat, when the ring lips are a little irregular, as is common with
récipients d'usage normal, une seconde application d'adhé- containers for normal use, a second application of adhesion
sif'est nécessaire pour aboutir au meilleur résultat con- it is necessary to achieve the best result
cernant une excellente durabilité de la fermeture herméti- the excellent durability of the hermetic closure
que lors du refroidissement et aussi les meilleurs condi- that during cooling and also the best conditions
tions de stockage à long terme du récipient Avec cette long-term storage of the container with this
double couche on obtient des récipients qui peuvent conte- double layer, containers are obtained that can contain
nir des aliments très acides et à forte teneur en humidité introduits à chaud, par exemple des jus de fruits, pendant high-moisture and high-moisture foods, such as fruit juices, during
le refroidissement et au cours d'un stockage de longue du- cooling and during long-term storage
rée, avec un minimum de fuites.with a minimum of leaks.
Après que les récipients 10 sortent du-stade de séchage 32, on les transfère à un stade 34 de remplissage à chaud et d'application du couvercle, comme on le voit sur la figure 3 Au stade 34, un produit alimentaire chaud à une température de 770 à 100 C environ est placé dans le récipient 10 Après le remplissage du récipient 10 avec le produit alimentaire chaud, le couvercle 18 est appliqué sur la partie lèvre 14 de la bague et hermétiquement uni After the containers leave the drying stage 32, they are transferred to a hot filling and lid-filling stage 34, as seen in FIG. 3. At stage 34, a hot food product at a temperature of 30.degree. approximately 770 to 100 C is placed in the container 10 After filling the container 10 with the hot food product, the lid 18 is applied to the lip portion 14 of the ring and hermetically united
avec cette dernière à l'aide d'une tête classique de sou- with the latter with the help of a classic head of sou-
dure Une telle tête applique la chaleur et la pression di- Such a head applies the heat and pressure
rigée vers le bas sur le couvercle 18 pour forcer la pel- down on the cover 18 to force the pel-
licule thermoplastique thermoscellable 22 du couvercle 18 thermoplastic heat sealable hose 22 of lid 18
à venir en prise tenace avec la couche adhésive thermoscel- to come in tenacious grip with the adhesive layer thermoscel-
lable 16 qui est en contact intime avec la partie lèvre 14 de la bague Après que les récipients ont été remplis et lable 16 which is in intimate contact with the lip portion 14 of the ring After the containers have been filled and
hermétiquement fermés, on les transfère à un stade de re- hermetically sealed, they are transferred to a
froidissement 36 à phases multiples o ils sont refroidis depuis la température de remplissage 77 à 1000 C jusqu'à la multiphase cooling 36 where they are cooled from the filling temperature 77 to 1000 C to the
température ambiante.ambient temperature.
On traite les récipients remplis à chaud dans le stade de remplissage à phases multiples 36 pour aboutir à 16 - un stade 3 8 de distribution de récipients remplis à chaud The hot-filled containers are treated in the multi-stage filling stage 36 to result in a hot-filled container dispensing stage 38.
qui place les récipients en une rangée linéaire pour trans- which places the containers in a linear row for trans-
fert à un stade 40 de traitement primaire à l'eau chaude. at a stage 40 of primary treatment with hot water.
Les récipients qui arrivent de la distribution 38 des ré- Receptacles coming from the distribution 38 of the
cipients remplis à chaud contiennent un produit qui est normalement à une température de 77-à 1000 C Le stade 40 de traitement primaire à la vapeur d'eau chaude soumet ces Hot-filled containers contain a product that is normally at a temperature of 77- to 1000 C. Stage 40 primary steam treatment hot water submits these
récipients à la vapeur d'eau chaude à une température d'en- containers with hot water vapor at a temperature of
viron 600 à 820 C pendant 1 à 10 minutes, normalement pen- 600 to 820 C for 1 to 10 minutes, normally
dant environ 3 minutes à une température d'eau de 820 C Les récipients sont transférés du traitement 40 primaire à l'eau chaude à un stade 42 de traitement secondaire à l'eau chaude dans lequel ils sont soumis à une pulvérisation The containers are transferred from the primary treatment to hot water at a stage 42 of secondary treatment with hot water in which they are sprayed for about 3 minutes at a water temperature of 820 C.
d'eau chaude à une température de 270 à 490 C pendant envi- hot water at a temperature of 270 to 490 C during
ron 1 à environ 10 -minutes, normalement pendant 3 minutes 1 to about 10 minutes, normally for 3 minutes
à une température de pulvérisation d'eau d'environ 27 çC. at a water spray temperature of about 27 ° C.
Les récipients à 490 C sont transférés du stade 42 de trai- Receptacles at 490 C are transferred from stage 42 of processing
tement secondaire à l'eau chaude à un stade 44 de traite- secondary to hot water at a stage 44 of treatment.
ment à l'eau froide o les récipients fermés hermétique- with cold water or closed hermetically sealed
ment sont plongés dans un bain d'eau froide ou reçoivent une pulvérisation d'eau froide à une température de 190 à are immersed in a cold water bath or receive a spray of cold water at a temperature of
250 C pendant 20 à 30 minutes.250 C for 20 to 30 minutes.
On a constaté que lorsque des remplissages à chaud sont indispensables pour des aliments tels que le jus d'oranges, le ketchup, la moutarde, la purée et les sauces It has been found that when hot fillings are essential for foods such as orange juice, ketchup, mustard, puree and sauces
tomates, les gelées, les conditures et des produits alimen- tomatoes, jellies, condiments and food products
taires analogues exigeant le remplissage à chaud, le pro- similar requirements requiring hot filling, the
cédé de la présente invention, utilisant l'adhésif thermo- according to the present invention, using the thermal adhesive
scellable décrit, permet d'obtenir des récipients herméti- described sealant, makes it possible to obtain hermetically sealed
quement fermés qui offrent une excellente résistance aux closed which offer excellent resistance to
fuites pendant le stade de refroidissement 3 6 à phases mul- during the cooling stage 3 6 with multiple phases
tiples, que l'on voit en détail dans les sous-stades 38 à 44, which can be seen in detail in sub-stages 38 to 44,
ainsi qu'une excellente résistance à l'apparition des fui- as well as an excellent resistance to the appearance of
tes lors d'un stockage à long terme, de quelques mois jus- during long-term storage, from a few months
qu'à un an.than a year.
Comme décrit précédemment, l'adhésif thermoscel- As previously described, the thermoset adhesive
Z 541175Z 541175
17 - lable selon la présente invention est un composé de silane mélangé avec un copolymère éthylène/acide acrylique ayant un indice d'écoulement à l'état fondu inférieur à 300, une teneur en éthylène de 80 % et une teneur en acide acrylique de 20 % Un tel copolymnère éthylène/acide acrylique qui convient parfaitement, est vendu par Dow Chemicals USA sous la marque déposée produit "PE 483 " ayant les propriétés According to the present invention, a silane compound mixed with an ethylene / acrylic acid copolymer having a melt flow index of less than 300, an ethylene content of 80% and an acrylic acid content of 20%. Such an ideal ethylene / acrylic acid copolymer is sold by Dow Chemicals USA under the trademark "PE 483" having the properties
physiques suivantes quand on l'achète sous forme d'une dis- following physical characteristics when purchased in the form of a
persion: Teneur en matières solides (%) 25 Viscosité Brookfield, 50 t/min 100-200 p H 9-10 Tension superficielle,dynes/cm 46-49 Poids par litre (kg) 1 Masse spécifique, liquide, g/cm 3 à 25 C 0,985 Masse spécifique, solides, g/cm 3 à 25 C 0,960 Véhicule eau ammoniaquée Composés organiques volatils Néant Indice d'acide (Dow) 156 Indice d'écoulement à l'état fondu (ASTM D-1238) 300 g/10 min Point de fusion (Dow, DSC) 85 C Point de ramollissement Vicat Persion: Solid content (%) Brookfield Viscosity, 50 rpm 100-200 p H 9-10 Surface tension, dynes / cm 46-49 Weight per liter (kg) 1 Specific gravity, liquid, g / cm 3 at 25 ° C 0.985 Specific gravity, g / cm 3 at 25 ° C 0.960 Ammonia water vehicle Volatile organic compounds None Acid number (Dow) 156 Melt flow rate (ASTM D-1238) 300 g / 10 min Melting point (Dow, DSC) 85 C Vicat softening point
(ASTM D-1525) 50 C(ASTM D-1525) 50 C
Résistance à la traction (ASTM D-638) 112 da N/cm 2 (pour échantillons moulés par compression) Limite élastique (ASTM D-638) 63 da N/cm 2 (pour échantillons moulés par compression) Allongement % (ASTM D-63 8) 3 00 Tensile strength (ASTM D-638) 112 da N / cm 2 (for compression molded samples) Elastic limit (ASTM D-638) 63 da N / cm 2 (for compression molded samples) Elongation% (ASTM D- 63 8) 3 00
Normalement, le composant silane de l'adhésif ther- Normally, the silane component of the heat adhesive
moscellable constitue de 4 à 12 % en poids du total de la moscellable constitutes from 4 to 12% by weight of the total
pellicule d'adhésif séchée.film of dried adhesive.
L'adhésif contenant le solvant non-organique selon la présente invention comprend normalement environ 25 g du copolymère en dispersion dans 100 g d'eau avec environ 2 g de silane incorporé Normalement, l'adhésif ne contenant 18 - The adhesive containing the non-organic solvent according to the present invention normally comprises about 25 g of the copolymer dispersed in 100 g of water with about 2 g of silane incorporated.
pas de solvant est préparé comme dans l'exemple suivant. no solvent is prepared as in the following example.
La dispersion aqueuse contenant le copolymère, de préfé- The aqueous dispersion containing the copolymer, preferably
rence le produit "Dow 483 " dont il a été question, est pla- the "Dow 483" product referred to, is
cée dans un récipient mélangeur et est agitée à une vites- in a mixing container and is stirred at a rapid rate
se tout juste suffisante pour former un tourbillon Un is just enough to form a whirlwind A
tourbillon minimal est souhaitable car l'action d'un tour- minimal tourbillon is desirable because the action of a tour-
billon violent provoque l'emprisonnement de beaucoup trop violent billon causes the imprisonment of far too much
d'air dans la dispersion, ce qui est fâcheux Après l'éta- of air in the dispersion, which is unfortunate
blissement d'un léger tourbillon dans l'eau de dispersion a slight swirl in the dispersion water
du copolymère, on ajoute 3 parties en volume d'une solu- of the copolymer, 3 parts by volume of a solution of
tion à 58 % en volume d'hydroxyde d'ammonium pour 100 par- at 58% by volume of ammonium hydroxide per 100 parts
ties en volume de la dispersion de copolymère Tout d'abord, by volume of the copolymer dispersion First of all,
on verse l'hydroxyde d'ammonium lentement dans le tourbil- ammonium hydroxide is poured slowly into the swirl
lon pour faciliter le malaxage correct de l'hydroxyde d'am- lon to facilitate the proper mixing of the amide hydroxide
monium dans la dispersion du copolymère afin de contribuer à la formation d'une émulsion stable Ensuite, on ajoute lentement 2 parties en volume du silane, de préférence, du silane "A 1120 " d'Union-Carbide, pour 100 parties en volume de la dispersion de copolymère en versant le silane dans le tourbillon du mélange On agite lentement le mélange avec un minimum de tourbillonnement pendant 2 à 3 minutes in the dispersion of the copolymer in order to contribute to the formation of a stable emulsion Then, 2 parts by volume of the silane, preferably Union-Carbide "A 1120" silane, are slowly added, per 100 parts by volume of The dispersion of the copolymer by pouring the silane into the vortex of the mixture The mixture is stirred slowly with a minimum of swirling for 2 to 3 minutes.
pour former une dispersion stable contenant un solvant non- to form a stable dispersion containing a non-solvent
organique, qu'on peut ensuite appliquer sur la partie lèvre de la bague du récipient en verre pour former une couche organic, which can then be applied to the lip portion of the glass container ring to form a layer
adhésive thermoscellable 16 selon la présente invention. heat-sealable adhesive 16 according to the present invention.
Pour des chaînes d'enduction à grande vitesse, le mélange For high speed coating lines, the mixture
adhésif décrit ci-dessus mousse parfois lors de l'applica- adhesive described above foam sometimes during the application
tion par des rouleaux à grande vitesse Dans un tel cas, après l'addition du silane, on incorpore par agitation un supplément de 4 parties en volume d'hydroxyde d'ammonium In such a case, after the addition of the silane, an additional 4 parts by volume of ammonium hydroxide is incorporated by stirring.
à 1 % et on agite l'adhésif résultant pendant 2 à 3 minutes. at 1% and the resulting adhesive is stirred for 2 to 3 minutes.
Pour démonter l'excellente durabilité d'un embal- To dismantle the excellent durability of a packaging
lage selon l'invention, on effectue les essais suivants: sur 11 récipients en verre à large ouverture, on applique à deux reprises un revêtement d'adhésif ayant la composition suivante, en volume: 100 parties de copolymère 19 - 483 de Dow Chemical USA; 3 parties d'hydroxyde d'ammonium According to the invention, the following tests are carried out: on 11 wide-opening glass containers, an adhesive coating having the following composition is applied twice, by volume: 100 parts of copolymer 19-483 from Dow Chemical USA ; 3 parts of ammonium hydroxide
à 58 % (dit concentré); 2 parties de silane A 1120 d'Union- at 58% (said concentrate); 2 parts silane A 1120 from Union-
Carbide et 4 parties d'une solution à 1 % d'hydroxyde d'am- Carbide and 4 parts of a 1% solution of ammonium hydroxide
monium dans l'eau désionisée, tous les ingrédients étant ajoutés dans l'ordre indiqué et dans les conditions décri- tes plus haut On enduit les 11 récipients avec le mélange adhésif. On chauffe les récipients enduits à 60 'C pendant Monium in deionized water, all ingredients being added in the order indicated and under the conditions described above. The 11 containers are coated with the adhesive mixture. The coated containers are heated at 60 ° C. for
minutes après le premier stade 30 d'application de - minutes after the first stage 30 application of -
l'adhésif Après la seconde application de l'adhésif avec the adhesive After the second application of the adhesive with
passage par la boucle de retour 33, on chauffe les réci- passing through the return loop 33, heat the reci-
pients à 5 o C pendant 45 minutes.at 5 o C for 45 minutes.
On plonge les récipients revêtus dans un bain d'eau à 60 'C pour simuler les appareils de préchauffage de récipients dans une chaîne industrielle de remplissage à chaud On remplit ensuite les récipients à ras bord avec du jus d'oranges à 100 'C Des couvercles préfaçonnés en aluminium de 50 microns ayant une sous-couche en "Surlyn" The coated containers are immersed in a water bath at 60 ° C. to simulate the preheating apparatus of containers in an industrial hot-filling line. The containers are then filled to the brim with orange juice at 100 ° C. Pre-formed 50 micron aluminum lids with "Surlyn" underlay
sont placés sur les récipients et sondés à chaud à l'ai- placed on the containers and hot-tempered with the help of
de d'une tête classique de soudure à chaud sous pression. of a conventional hot pressurized welding head.
Les conditions de travail de la tête de soudure sont température de la surface élastique du joint 197-2080 C Pression de soudure 6 bars Pression de sertissage sur le bord de la lèvre 3,5 bars The working conditions of the welding head are temperature of the elastic surface of the joint 197-2080 C Welding pressure 6 bar Pressing pressure on the edge of the lip 3.5 bar
Durée de soudure 1 seconde.Weld duration 1 second.
Après fermeture hermétique, on refroidit les réci- After sealing, the containers are cooled
pients pendant 3 minutes dans une chambre de vapeur d'eau à 820 C Puis on refroidit les récipients pendant 3 minutes pients for 3 minutes in a steam chamber at 820 C. Then the containers are cooled for 3 minutes
dans une pulvérisation d'eau à 490 C Finalement, on refroi- in a spray of water at 490 C Finally, we cool
dit les récipients pendant 3 minutes dans un courant d'eau says the containers for 3 minutes in a stream of water
à 230 C On ne détecte aucune fuite. at 230 C No leaks are detected.
Après refroidissement à 23 C, on place les réci- After cooling to 23 ° C, the recipes are
pients fermés hermétiquement dans un exsiccateur sous vi- hermetically sealed in an exsiccator under
de On applique un vide égal à 234 millibars au exsicca- A vacuum equal to 234 millibars is applied to the exsicca-
-20 --20 -
teur et on le maintient pendant 1 minute On augmente en- and hold it for 1 minute.
suite le vide à 878 millibars pendant 5 secondes On ne following the vacuum at 878 millibars for 5 seconds
détecte aucune fuite.detects no leakage.
Ce test démontre la durabilité au refroidissement et la durabilité sous un vide élevé appliqué à l'emballage This test demonstrates the durability to cooling and durability under a high vacuum applied to the packaging
selon l'invention.according to the invention.
On effectue un second test pour mettre en évidence la durabilité d'un emballage selon la présente invention quand on le soumet au remplissage à chaud à un traitement primaire et secondaire par la chaleur et à un traitement à l'eau froide pour simuler approximativement une opération A second test is carried out to demonstrate the durability of a package according to the present invention when subjected to heat-filling to primary and secondary heat treatment and cold water treatment to simulate approximately one operation.
industrielle de conditionnement d'aliments. industrial food packaging.
On prépare une dispersion adhésive thermoscella- A heat-sealing adhesive dispersion is prepared
ble comme suit: on agite 3500 ml d'un copolèmère éthylène/ ^ 15 acide acrylique du type PE-483 pour former un tourbillon ble as follows: 3500 ml of an ethylene / PE-483 acrylic acid copolymer were stirred to form a vortex
comme il a été décrit plus haut et ensuite on ajoute len- as described above and then we add
tement à ce tourbillon de la dispersion de copolymère, 105 to this whirlwind of the copolymer dispersion, 105
ml d'une solution à 58 % en volume d'hydroxyde d'ammonium. ml of a 58% by volume solution of ammonium hydroxide.
On incorpore dans le tourbillon par agitation 70 ml de si- 70 ml of silica are added to the vortex by stirring.
lane organo-fonctionnel du type A 1120 (Union-Carbide) Ul- Organo-functional lane type A 1120 (Union-Carbide)
térieurement on ajoute à la solution 280 ml d'une solution de 1 partie en volume d'hydroxyde d'ammonium et 100 parties en volume d'eau distillée, pour-réduire le moussage lors de l'application par le système à rouleau du type décrit 280 ml of a solution of 1 part by volume of ammonium hydroxide and 100 parts by volume of distilled water are subsequently added to the solution, in order to reduce the foaming during the application by the roller system of the type described
ci-dessus.above.
On revêt à deux reprises 13 récipients à large ou- Twice 13 containers are covered with large
verture avec le même dispositif d'enduction au rouleau à l'aide de la dispersion adhésive pour établir une couche d'environ 0,05 mg/mm 2 d'adhésif séché On sèche la première couche d'adhésif thermoscellable pendant 15 minutes à 60 'C with the same roller coating device using the adhesive dispersion to establish a layer of about 0.05 mg / mm 2 of dried adhesive The first layer of heat-sealable adhesive is dried for 15 minutes at 60.degree. 'C.
et la seconde couche pendant 45 minutes à 93 O C, et on re- and the second layer for 45 minutes at 93 ° C, and
froidit les récipients à température ambiante après chaque chills the containers at room temperature after each
cycle de séchage d'adhésif.adhesive drying cycle.
Avant le remplissage avec un produit conditionné à chaud, on plonge chaque récipient dans un bain d'eau à 60 'C pour simuler un dispositif à chauffer les bouteilles dans 21 - une chaîne industrielle de remplissage Ensuite, on remplit les récipients jusqu'au débordement avec de la gelée de Before filling with a hot-packaged product, each container is immersed in a water bath at 60 ° C. to simulate a device for heating the bottles in an industrial filling line. Then, the containers are filled up to the overflow. with jelly
fraises à 770 C On place ensuite sur l'ouverture du réci- strawberries at 770 ° C. Then place on the opening of the container.
pient un couvercle en feuille d'aluminium du type décrit avec une souscouche de résine ionomère de qualité "Surlyn" du type 1652 On scelle à la chaleur le couvercle à l'aide d'une tête classique de soudure à chaud et sous pression a type aluminum foil lid of the type described with an undercoat of "Surlyn" quality ionomer resin type 1652 is sealed. The lid is heat-sealed using a conventional hot and press-welded head.
dans les mêmes conditions que dans l'exemple précédent. under the same conditions as in the previous example.
Après fermeture, on refroidit à force les récipients dans un premier stade 40 de traitement à l'eau chaude à 820 C pendant 3 minutes On transfère ensuite les récipients au After closing, the containers are first cooled in a first stage of treatment with hot water at 820 C for 3 minutes. The containers are then transferred to
stade de traitement secondaire 42 à l'eau chaude o ils re- secondary treatment stage 42 with hot water where they
çoivent une pulvérisation d'eau à 490 C pendant 3 minutes. water spray at 490 C for 3 minutes.
On déplace les récipients au stade 44 de traitement à l'eau froide o on les soumet à un courant d'eau froide à 260 C The containers are moved to the stage 44 of treatment in cold water or subjected to a current of cold water at 260 ° C.
pendant 3 minutes Finalement, on refroidit tous les réci- for 3 minutes Finally, we cool all the reci-
pients à la température ordinaire dans l'air ambiant. at room temperature in the ambient air.
Après le refroidissement à température ambiante, After cooling to room temperature,
on place les récipients fermés hermétiquement dans un exsic- hermetically sealed containers are placed in an exsic-
cateur sous vide pour des essais Au cours de l'essai, toute rupture du joint devient évidente par l'échappement des bulles d'air -provenant de l'emballage On place chaque récipient dans un exsiccateur sous vide rempli d'eau et on expose à un vide égal à 234 millibars qu'on applique et qu'on maintient pendant 1 minute Après cette minute, on augmente le vide jusqu'à 878 millibars et on maintient ce Vacuum tester for tests During the test, any rupture of the seal becomes evident by the escape of the air bubbles from the package. Each container is placed in a vacuum desiccator filled with water and exposed. at a vacuum equal to 234 millibars applied and maintained for 1 minute After this minute, we increase the vacuum to 878 millibars and we maintain this
vide pendant 5 secondes.empty for 5 seconds.
A la suite de cet essai, 12 des 13 récipients sur- As a result of this test, 12 of the 13
vivent aussi bien sous un faible vide que sous vide poussé dans les conditions de l'essai; le seul récipient qui ne supporte pas l'essai est cassé par suite d'une fissuration live as well under a low vacuum as under high vacuum under the conditions of the test; the only container that does not support the test is broken due to cracking
dans la paroi de verre du récipient lui-même. in the glass wall of the container itself.
On effectue un autre essai pour déterminer la du- Another attempt is made to determine the
rabilité au stockage à long terme de l'emballage Dans cet essai, on remplit 14 récipients comme décrit ci-dessus avec long-term storage of the packaging In this test, 14 containers are filled as described above with
du jus d'oranges à 1000 C et on ferme hermétiquement On sou- orange juice at 1000 C and seal
22 - met les récipients d'abord à l'essai sous un vide de 234 millibars comme décrit ci-dessus pendant une minute puis sous un vide de 878 millibars pendant 5 secondes On ne constate aucune rupture On stocke ensuite les récipients fermés hermétiquement pendant 22 jours à 380 C dans une chambre à vieillissement accéléré Une journée dans la chambre à vieillissement accéléré à 380 C correspond à peu 22 - first test the containers under a vacuum of 234 millibars as described above for one minute and then under a vacuum of 878 millibars for 5 seconds There is no breakage is then stored hermetically closed containers for 22 days at 380 C in a room accelerated aging A day in the accelerated aging chamber at 380 C corresponds to little
près à 3 jours dans des conditions normales d'utilisation. within 3 days under normal conditions of use.
Après le stockage à long terme, on soumet de nouveau tous les récipients à la dessiccation sous vide de 234 millibars pendant 1 minute On ne constate aucune fuite dans aucun After long-term storage, all the containers are again subjected to vacuum desiccation of 234 millibars for 1 minute.
des récipients après la longue période de stockage décrite. containers after the long storage period described.
Claims (4)