CN109502725A - 一种高效低毒的废水除磷剂及其制备方法 - Google Patents
一种高效低毒的废水除磷剂及其制备方法 Download PDFInfo
- Publication number
- CN109502725A CN109502725A CN201811452010.3A CN201811452010A CN109502725A CN 109502725 A CN109502725 A CN 109502725A CN 201811452010 A CN201811452010 A CN 201811452010A CN 109502725 A CN109502725 A CN 109502725A
- Authority
- CN
- China
- Prior art keywords
- water
- dephosphorization agent
- zero
- attapulgite
- valent iron
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种高效低毒的废水除磷剂及其制备方法,废水除磷剂由以下成分按重量百分比含量组成:乙酸钠20%‑35%、聚磷材料8%‑30%、零价铁8%‑14%,凹凸棒土10%‑30%、活性氧化铝5%‑8%、海泡石5%‑12%、粘土10%‑25%、水5%‑7%。按重量百分比选取上述材料,并将零价铁和凹凸棒土混合置于行星式球磨机先行研磨;干式混合后,边搅拌边加入水,阴凉处晾干,得到粉剂的除磷剂;或者直接进入螺杆造粒机中造粒,得到颗粒状除磷剂。本发明具有材料廉价易得、制备简单、且长期高效去除磷的同时避免对处理后的水体造成二次污染。
Description
技术领域
本发明属于环保技术领域,涉及到废水处理剂及其制备方法。
背景技术
由于经济社会的迅猛发展,目前工业化程度越来越高,以及人们的生活水平的提高,含磷废水排放已成为生态环境质量降低的重要原因,一直以来都是重点关注的对象。特别是作为地表水中的磷污染,已严重影响到水环境质量。磷污染最直接的危害是产生水体富营养化现象,主要表现为水体中藻类的大量繁殖,使水体应有的净化功能丧失,影响人类的生产和生活环境。水体富营养化现象的形成危害大、历时短,水体生态系统平衡遭到严重的破坏,藻类缺氧腐烂,水体产生异味,感官性能恶化;水体溶解氧含量降低,大量鱼类死亡,水产养殖业将受到很大影响。地表水主要来源有(1)首先是由于农业磷肥的使用,使在土壤中积累了相当数量营养物质,可随农田排水流入临近的水体;(2)饲养家畜过程所产生的废物中也含有相当数量的营养物质,有可能通过排水进入临近水体;(3)城市污水所含磷的主要来源是粪便、食品污物和合 成洗涤剂。尤其是合成洗涤剂,在一些高消费地区如北美的污水中 50%-70%的总磷来自于此。(4)在污水处理厂很大部分的磷通过金属磷酸盐(如磷酸钙)沉淀而被除去存在进入水体的风险。另外在处理过程中也用到许多含磷的化学药剂,如磷酸三钠、多聚磷酸钠等。
磷污染的处理技术有多种,生物法、化学沉淀法、结晶法、吸附法、人工湿地法等工艺各自除磷原理及其应用范围不同,存在着不同的优缺点,现今的技术对于废水除磷处理方面的解决方案并不是十分理想,受到诸多环境因素的影响和制约,导致很多工厂为了节约成本将未达标的污水排放到环境中,污染水资源。同时,受污染的地表水除磷技术存在着处置效率低、周期长等不足,严重制约着地表水环境的改善。
发明内容
针对上述现有存在的问题,本发明提供一种高效低毒的废水除磷剂及其制备方法,具有高效、低毒等特点,其制备方法简便可行。
本发明通过以下技术方案实现的。
本发明所述的一种高效低毒的废水除磷剂,由以下成分按重量百分比含量组成:乙酸钠20%-35%、聚磷材料8%-30%、零价铁8%-14%,凹凸棒土10%-30%、活性氧化铝5%-8%、海泡石5%-12%、粘土10%-25%、水5%-7%。
优选的质量百分比为:乙酸钠22%-31%、聚磷材料10%-26%、零价铁10%,凹凸棒土15%-35%、活性氧化铝7.5%、海泡石8%-10%、粘土10%-20%,水6%。
本发明所述的一种高效低毒的废水除磷剂及其制备方法,包括以下步骤。
(1)材料准备:选取乙酸钠、聚磷材料、零价铁、凹凸棒土、活性氧化铝、海泡石、粘土及水,其中乙酸钠呈结晶状;将零价铁和凹凸棒土混合置于行星式球磨机,转速1100r/min,研磨4h后待用。
(2)材料混合:按照质量百分比将乙酸钠、聚磷材料、步骤(1)中的零价铁和凹凸棒土混合材料、活性氧化铝、海泡石、粘土加入搅拌机中,采用干式混合后,按比例边搅拌边加入少量水,搅拌叶片转速为20-50r/min,搅拌混匀1-3h后,置于阴凉处晾6h,得到粉剂的除磷剂;或者不晾干直接进入螺杆造粒机中,切刀转速为1200r/min,成型为颗粒状,粒径为0.5mm-3mm,得到颗粒状除磷剂。
本发明具有的优点。
(1)本发明所使用的原材料均属于常规物品,廉价易得、制备简单,可操作性强,且去除磷同时避免对环境的二次污染。
(2)本发明可长期提供碳源以及部分营养物质,降低后续维护材料的投加成本,同时可提供多种形式(粉剂和颗粒剂),提高材料的使用性和适用性。
附图说明
图1为本发明实施例1的总磷去除率。
具体实施方式
本发明实施例中部分材料的选取:将聚磷材料脱水至含水率为10%-20%,颗粒粒径0.5-0.3mm;零价铁粒径为10-150μm;活性氧化铝比表面积230m2/g-410m2/g;粘土矿物的粒径为0.5μm-2.0μm。
实施例1。
按照高效低毒的除磷剂的配方的质量比准备制备材料,其中乙酸钠0.24kg、聚磷材料0.12kg、零价铁0.1kg,凹凸棒土0.15kg、活性氧化铝0.07kg、海泡石0.09kg、粘土0.17kg、水0.06kg。首先分别将零价铁和凹凸棒土混合置于行星式球磨机,转速1100r/min,研磨4h后待用。然后再将乙酸钠、聚磷材料、活性氧化铝、海泡石、粘土、水以及零价铁和凹凸棒土的混合物一起置于搅拌器中搅拌混匀1h,晾干6h,得到粉状除磷剂。
采取纯水配置含磷溶液,其中总磷含量为2.8mg/L,取500mL置于锥形瓶中,分别加入配置后的除磷剂10mg、20mg、50mg以及100mg,并设置不加除磷剂对照。室温20℃环境下,搅拌,并隔5h取样分析,最终除磷剂投加量50mg的总磷去除率达到86%,未加除磷剂为8%。其余效果见图1。
实施例2。
按照高效低毒的除磷剂的配方的质量比准备制备材料,其中乙酸钠2.4kg、聚磷材料1.15kg、零价铁1.0kg,凹凸棒土1.8kg、活性氧化铝0.75kg、海泡石0.8kg、粘土1.5kg,水0.6。首先分别将零价铁和凹凸棒土混合置于行星式球磨机,转速1100r/min,研磨4h后待用。然后再将乙酸钠2.4kg、聚磷材料1.15kg、活性氧化铝0.75kg、海泡石0.8kg、粘土1.5kg,水0.6kg,混合置于搅拌器中搅拌混匀,再将其放入造粒机中挤出造粒,造粒后晾干6h,得到除磷剂。
采取南方某黑臭水体中的水样200L(总磷含量为1.2mg/L),并分为2份,各100kg,将制备的药剂与水按照1:100和5:100质量比投加,投加药剂后,采用机器搅拌,每隔一段时间取样分析总磷,1d后发现1:100的总磷浓度为0.9mg/L,5:100投加量的总磷浓度为0.75mg/L,3天后,前者的总磷浓度为0.4mg/L,后者的浓度为0.21mg/L。
Claims (3)
1.一种高效低毒的废水除磷剂,其特征是由以下成分按重量百分比含量组成:乙酸钠20%-35%、聚磷材料8%-30%、零价铁8%-14%,凹凸棒土10%-30%、活性氧化铝5%-8%、海泡石5%-12%、粘土10%-25%、水5%-7%。
2.根据权利要求1所述的一种高效低毒的废水除磷剂,其特征是由以下成分按质量百分比组成:乙酸钠22%-31%、聚磷材料10%-26%、零价铁10%,凹凸棒土15%-35%、活性氧化铝7.5%、海泡石8%-10%、粘土10%-20%,水6%。
3.权利要求1所述的高效低毒的废水除磷剂的制备方法,其特征是包括以下步骤:
(1)按重量百分比选取乙酸钠、聚磷材料、零价铁、凹凸棒土、活性氧化铝、海泡石、粘土及水,其中乙酸钠呈结晶状;将零价铁和凹凸棒土混合置于行星式球磨机,转速1100r/min,研磨4h后待用;
(2)将乙酸钠、聚磷材料、步骤(1)中的零价铁和凹凸棒土混合材料、活性氧化铝、海泡石、粘土加入搅拌机中,采用干式混合后,按比例边搅拌边加入少量水,搅拌叶片转速为20-50r/min,搅拌混匀1-3h后,置于阴凉处晾6h,得到粉剂的除磷剂;或者不晾干直接进入螺杆造粒机中,切刀转速为1200r/min,成型为颗粒状,粒径为0.5mm-3mm,得到颗粒状除磷剂。