[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

CN106046970A - Anticorrosion coating for desk lamp and preparation method thereof - Google Patents

Anticorrosion coating for desk lamp and preparation method thereof Download PDF

Info

Publication number
CN106046970A
CN106046970A CN201610663168.XA CN201610663168A CN106046970A CN 106046970 A CN106046970 A CN 106046970A CN 201610663168 A CN201610663168 A CN 201610663168A CN 106046970 A CN106046970 A CN 106046970A
Authority
CN
China
Prior art keywords
parts
desk lamp
anticorrosion coating
resin
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610663168.XA
Other languages
Chinese (zh)
Inventor
韩梅
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anqing Seven Fairy Electric Appliance Manufacturing Co Ltd
Original Assignee
Anqing Seven Fairy Electric Appliance Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anqing Seven Fairy Electric Appliance Manufacturing Co Ltd filed Critical Anqing Seven Fairy Electric Appliance Manufacturing Co Ltd
Priority to CN201610663168.XA priority Critical patent/CN106046970A/en
Publication of CN106046970A publication Critical patent/CN106046970A/en
Pending legal-status Critical Current

Abstract

The invention discloses an anticorrosion coating for a desk lamp. The anticorrosion coating is prepared from the following raw materials: fluorocarbon resin, elastic emulsion, hydroxyethyl cellulose, epoxy resin, adipic acid, bamboo charcoal powder, polyester glycol, dipropylene glycol monomethyl ether, a proper amount of water, a catalyst, a corrosion inhibitor, nanometer titanium dioxide, lauryl acrylate and rosin resin. A preparation method for the anticorrosion coating comprises the following steps: (1) preparing preliminarily mixed liquid; (2) preparing intermediate liquid; (3) preparing mixed liquid; and (4) adding the mixed liquid obtained in the step (3) into a ball mill for grinding and carrying out sieving so as to obtain the anticorrosion coating. The preparation method in the invention is scientific and reasonable, improves the corrosion resistance of the composition by using organic polymer materials with good performance and carrying out optimized combination, and is low in cost, short in production period and suitable for industrial mass production.

Description

A kind of desk lamp anticorrosive coating and preparation method thereof
Technical field
The invention belongs to coating industry technical field, particularly relate to a kind of desk lamp anticorrosive coating and preparation method thereof.
Background technology
Coating, at the entitled paint of Chinese tradition, refer to coat body surface can form thin film under certain conditions and Play protection, a class I liquid I of decoration or other specific functions (insulation, antirust, mildew-resistant, heat-resisting etc.) or solid material.Because of early stage Coating is mostly with vegetable oil as primary raw material, therefore also referred to as paint.Synthetic resin instead of vegetable oil now, therefore is referred to as being coated with Material.Coating belongs to organic chemical industry's macromolecular material, and the film formed belongs to macromolecular compound type.Current according to the modern times The classification of chemical products, coating belongs to fine chemical product.Modern coating the most progressively becomes a polyfunctional engineering of class Material, is an important industry in chemical industry.At present, the coating industry of China is the most ripe, and market is close to saturated, in addition Green economy globalization overall situation under, people become more concerned with economy the most flourishing after, environment is by great destruction.Along with The environmental protection such as newly " environmental law " promulgates, country " environmental protection, beautiful China " advocate the most no longer to stay on slogan, but real Execute execution, implement to promote energetically the development of green science and technology industry.
At present, the covering with paint of household electrical appliance has had bigger change, and traditional thermohardening lacquer is by the water of environmental protection Property coating etc. substitute, but different electrical equipment has different requirements due to the difference of the aspects such as function to coating, more environmentally friendly, more individual Property has become as the pursuit direction of household electrical appliances coating.Before the market demand huge in the face of household electrical appliances coating and ever-increasing application Scape, strengthens research and development capabilities, and updates and improving product performance, accelerates product quality upgrading, develops technically, cost Above, the household electrical appliances coating more showing powerful competitive advantage in performance has the meaning of reality and the wide market space.
Summary of the invention
The invention aims to overcome the deficiencies in the prior art, it is provided that a kind of desk lamp anticorrosive coating and Preparation method, this coating products excellent performance, there are good Corrosion Protection, and energy-conserving and environment-protective, possess the most economic effect Benefit and social benefit.
For solve above-mentioned technical problem, the present invention by the following technical solutions:
A kind of desk lamp anticorrosive coating, is prepared by the raw materials in: fluorocarbon resin 35~45 parts, elastic emulsion 10 ~15 parts, hydroxyethyl cellulose 2~5 parts, epoxy resin 5~12 parts, adipic acid 8~15 parts, bamboo charcoal powder 2~6 parts, polyester-diol 1~3 part, dipropylene glycol methyl ether 6~12 parts, water are appropriate, catalyst 1.5~3 parts, corrosion inhibiter 1.5~2.5 parts, nanometer titanium dioxide Titanium 1~5 parts, lauryl acrylate 5~10 parts, rosin resin 5~12 parts;
Its preparation method in turn includes the following steps:
(1) adipic acid, bamboo charcoal powder, polyester-diol, dipropylene glycol methyl ether, nano titanium oxide and suitable quantity of water are joined instead Answer in container, be heated to 50~65 DEG C, stir 20~30 minutes under 900~1200 revs/min, obtain the most mixed after mix homogeneously Liquid;
(2) fluorocarbon resin, elastic emulsion, hydroxyethyl cellulose, epoxy resin and lauryl acrylate are mixed to join In the first mixed liquid that step (1) obtains, it is heated to 65~80 DEG C, continues stirring 30~40 minutes, obtain intermediate liquid;
(3) intermediate liquid that step (2) obtains is cooled to 40~50 DEG C, adds catalyst, corrosion inhibiter and rosin resin, Mix and blend 50~80 minutes, obtain mixed liquor;
(4) mixed liquor step (3) obtained puts into grinding in ball grinder and processes, and sieves and gets product.
Preferably, described catalyst is sodium sulfonate.
Preferably, described corrosion inhibiter is pyridine.
The beneficial effects of the present invention is:
Preparation method of the present invention is scientific and reasonable, by using combination property preferably high-molecular organic material and being optimized Combination, improves the Corrosion Protection of compositions, and the coating surface using the present invention to obtain is smooth, fine and smooth, smooth, gloss retention Good, the index such as hot strength is superior to common coating, and can meet coated-body the most comprehensively uses requirement;Cost of the present invention is relatively Low, it is achieved that making full use of of resource and the energy, production process is environment friendly and pollution-free, with short production cycle, is suitable to industrial mass raw Produce, possess preferable economic benefit and social benefit.
Detailed description of the invention
Below in conjunction with embodiment, the invention will be further described.
Embodiment 1:
A kind of desk lamp anticorrosive coating, is prepared by the raw materials in: fluorocarbon resin 35 parts, elastic emulsion 10 parts, Hydroxyethyl cellulose 2 parts, epoxy resin 5 parts, adipic acid 8 parts, bamboo charcoal powder 2 parts, polyester-diol 1 part, dipropylene glycol methyl ether 6 parts, Water is appropriate, catalyst 1.5 parts, corrosion inhibiter 1.5 parts, nano titanium oxide 1 part, lauryl acrylate 5 parts, rosin resin 5 parts;
Its preparation method in turn includes the following steps:
(1) adipic acid, bamboo charcoal powder, polyester-diol, dipropylene glycol methyl ether, nano titanium oxide and suitable quantity of water are joined instead Answer in container, be heated to 50~65 DEG C, stir 20 minutes under 900~1200 revs/min, after mix homogeneously, obtain the most mixed liquid;
(2) fluorocarbon resin, elastic emulsion, hydroxyethyl cellulose, epoxy resin and lauryl acrylate are mixed to join In the first mixed liquid that step (1) obtains, it is heated to 65~80 DEG C, continues stirring 30 minutes, obtain intermediate liquid;
(3) intermediate liquid that step (2) obtains is cooled to 40~50 DEG C, adds catalyst, corrosion inhibiter and rosin resin, Mix and blend 50 minutes, obtains mixed liquor;
(4) mixed liquor step (3) obtained puts into grinding in ball grinder and processes, and sieves and gets product.
Embodiment 2:
A kind of desk lamp anticorrosive coating, is prepared by the raw materials in: fluorocarbon resin 45 parts, elastic emulsion 15 parts, Hydroxyethyl cellulose 5 parts, epoxy resin 12 parts, adipic acid 15 parts, bamboo charcoal powder 6 parts, polyester-diol 3 parts, dipropylene glycol methyl ether 12 Part, water is appropriate, catalyst 3 parts, corrosion inhibiter 2.5 parts, nano titanium oxide 5 parts, lauryl acrylate 10 parts, rosin resin 12 Part;
Its preparation method in turn includes the following steps:
(1) adipic acid, bamboo charcoal powder, polyester-diol, dipropylene glycol methyl ether, nano titanium oxide and suitable quantity of water are joined instead Answer in container, be heated to 50~65 DEG C, stir 30 minutes under 900~1200 revs/min, after mix homogeneously, obtain the most mixed liquid;
(2) fluorocarbon resin, elastic emulsion, hydroxyethyl cellulose, epoxy resin and lauryl acrylate are mixed to join In the first mixed liquid that step (1) obtains, it is heated to 65~80 DEG C, continues stirring 40 minutes, obtain intermediate liquid;
(3) intermediate liquid that step (2) obtains is cooled to 40~50 DEG C, adds catalyst, corrosion inhibiter and rosin resin, Mix and blend 80 minutes, obtains mixed liquor;
(4) mixed liquor step (3) obtained puts into grinding in ball grinder and processes, and sieves and gets product.
In the above embodiment of the present invention:
Described catalyst is sodium sulfonate;
Described corrosion inhibiter is pyridine.
During the present invention implements, by using combination property preferably high-molecular organic material and carrying out optimum organization, improve The Corrosion Protection of compositions, the coating surface using the present invention to obtain is smooth, fine and smooth, smooth, and gloss retention is good, hot strength Being superior to common coating etc. index, can meet coated-body the most comprehensively uses requirement;Cost of the present invention is relatively low, it is achieved that money Making full use of of source and the energy, production process is environment friendly and pollution-free, with short production cycle, is suitable to industrialized mass production.
Finally it should be noted that above example only in order to illustrative not limiting technical scheme, although reference The present invention has been described in detail by above-described embodiment, it will be appreciated by those skilled in the art that and still can carry out the present invention Amendment or equivalent, any modification or partial replacement without departing from the spirit and scope of the present invention, it all should be contained In scope of the presently claimed invention.

Claims (3)

1. a desk lamp anticorrosive coating, it is characterised in that be prepared by the raw materials in: fluorocarbon resin 35~45 parts, Elastic emulsion 10~15 parts, hydroxyethyl cellulose 2~5 parts, epoxy resin 5~12 parts, adipic acid 8~15 parts, bamboo charcoal powder 2~6 Part, polyester-diol 1~3 parts, dipropylene glycol methyl ether 6~12 parts, water is appropriate, catalyst 1.5~3 parts, corrosion inhibiter 1.5~2.5 parts, Nano titanium oxide 1~5 parts, lauryl acrylate 5~10 parts, rosin resin 5~12 parts;
Its preparation method in turn includes the following steps:
(1) adipic acid, bamboo charcoal powder, polyester-diol, dipropylene glycol methyl ether, nano titanium oxide and suitable quantity of water join reaction to hold In device, it is heated to 50~65 DEG C, stirs 20~30 minutes under 900~1200 revs/min, after mix homogeneously, obtain the most mixed liquid;
(2) fluorocarbon resin, elastic emulsion, hydroxyethyl cellulose, epoxy resin and lauryl acrylate are mixed to join step (1) in the first mixed liquid obtained, it is heated to 65~80 DEG C, continues stirring 30~40 minutes, obtain intermediate liquid;
(3) intermediate liquid that step (2) obtains is cooled to 40~50 DEG C, adds catalyst, corrosion inhibiter and rosin resin, mixing Stir 50~80 minutes, obtain mixed liquor;
(4) mixed liquor step (3) obtained puts into grinding in ball grinder and processes, and sieves and gets product.
A kind of desk lamp anticorrosive coating the most according to claim 1, it is characterised in that described catalyst is sodium sulfonate.
A kind of desk lamp anticorrosive coating the most according to claim 1, it is characterised in that described corrosion inhibiter is pyridine.
CN201610663168.XA 2016-08-12 2016-08-12 Anticorrosion coating for desk lamp and preparation method thereof Pending CN106046970A (en)