Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chemie Linz AgfiledCriticalChemie Linz Ag
Priority to AT181860ApriorityCriticalpatent/AT219012B/en
Application grantedgrantedCritical
Publication of AT219012BpublicationCriticalpatent/AT219012B/en
Compounds Of Alkaline-Earth Elements, Aluminum Or Rare-Earth Metals
(AREA)
Description
<Desc/Clms Page number 1>
Verfahren zur Herstellung von Kryolith
EMI1.1
<Desc/Clms Page number 2>
Wird die Ammonfluoridlösung innerhalb einer Stunde langsam zugesetzt, so enthält der Kryolith 0, 9% SO3 in nicht auswaschbarer Form.
<Desc / Clms Page number 1>
Process for making cryolite
EMI1.1
<Desc / Clms Page number 2>
If the ammonium fluoride solution is added slowly within an hour, the cryolite contains 0.9% SO3 in a form that cannot be washed out.
Claims (1)
PATENTANSPRUCH :
EMI2.1
als 50 g/l H2S04 entspricht, durchgeführt wird, dass weiters stets mindestens 3 Mole Fluor auf l Mol Aluminium kommen und die Fällung möglichst rasch, vorzugsweise innerhalb etwa einer Minute, höchstens aber innerhalb etwa 5 Minuten, durchgeführt wird.
PATENT CLAIM:
EMI2.1
than 50 g / l H2S04, it is carried out that there are always at least 3 moles of fluorine per 1 mole of aluminum and the precipitation is carried out as quickly as possible, preferably within about one minute, but at most within about 5 minutes.