Nanoindentation study of Zn-based Pb free solders used in fine pitch interconnect applicationsKumar et al., 2006
View PDF- Document ID
- 13025196575402461804
- Author
- Kumar K
- Kripesh V
- Shen L
- Zeng K
- Tay A
- Publication year
- Publication venue
- Materials Science and Engineering: A
External Links
Snippet
Because of their hazardous nature, conventional Sn–Pb solders are slowly being replaced by Pb free solders. Sn–Zn solder alloys have been identified as a potential alternative because of their low melting point close to that of Sn–Pb solder. However, the high Sn …
- 229910000679 solder 0 title abstract description 87
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/26—Selection of soldering or welding materials proper with the principal constituent melting at less than 400 degrees C
- B23K35/262—Sn as the principal constituent
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/30—Selection of soldering or welding materials proper with the principal constituent melting at less than 1550 degrees C
- B23K35/3013—Au as the principal constituent
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Kumar et al. | Nanoindentation study of Zn-based Pb free solders used in fine pitch interconnect applications | |
Yoon et al. | IMC morphology, interfacial reaction and joint reliability of Pb-free Sn–Ag–Cu solder on electrolytic Ni BGA substrate | |
Lee et al. | Interfacial reaction of Sn‐Ag‐Cu lead‐free solder alloy on Cu: A review | |
Giuranno et al. | Effects of Sb addition on the properties of Sn-Ag-Cu/(Cu, Ni) solder systems | |
Lee et al. | Are intermetallics in solder joints really brittle? | |
Gain et al. | Effects of Ni nanoparticles addition on the microstructure, electrical and mechanical properties of Sn-Ag-Cu alloy | |
Choudhury et al. | Local shear stress-strain response of Sn-3.5 Ag/Cu solder joint with high fraction of intermetallic compounds: Experimental analysis | |
Ho et al. | Strong effect of Cu concentration on the reaction between lead-free microelectronic solders and Ni | |
Chellvarajoo et al. | Effects of diamond nanoparticles reinforcement into lead-free Sn–3.0 Ag–0.5 Cu solder pastes on microstructure and mechanical properties after reflow soldering process | |
Tian et al. | Brittle fracture of Sn-37Pb solder joints induced by enhanced intermetallic compound growth under extreme temperature changes | |
Leinenbach et al. | Wetting and soldering behavior of eutectic Au-Ge alloy on Cu and Ni substrates | |
Tao et al. | Selective interfacial reaction between Ni and eutectic BiSn lead-free solder | |
Fahim et al. | Mechanical characterization of intermetallic compounds in SAC solder joints at elevated temperatures | |
Gnecco et al. | Wetting behaviour and reactivity of lead free Au–In–Sn and Bi–In–Sn alloys on copper substrates | |
Novakovic et al. | Interfacial reactions in the Sb–Sn/(Cu, Ni) systems: wetting experiments | |
Nourani et al. | Combined effect of strain-rate and mode-ratio on the fracture of lead-free solder joints | |
Koo et al. | Effect of substrate metallization on mechanical properties of Sn–3.5 Ag BGA solder joints with multiple reflows | |
Yonekura et al. | Bonding mechanism of lead-free solder and glass plate by ultrasonic assisted soldering method | |
Sharif et al. | Dissolution of electroless Ni metallization by lead-free solder alloys | |
Lee et al. | Interfacial reaction and mechanical properties between low melting temperature Sn–58Bi solder and various surface finishes during reflow reactions | |
Jian et al. | Fatigue properties and microstructure of SnAgCu Bi-based solder joint | |
Islam et al. | Interfacial reactions of Sn–Cu solder with Ni/Au surface finish on Cu pad during reflow and aging in ball grid array packages | |
Koo et al. | Effect of displacement rate on ball shear properties for Sn–37Pb and Sn–3.5 Ag BGA solder joints during isothermal aging | |
Emadi et al. | Microstructural and mechanical characterization of Cu/Sn SLID bonding utilizing Co as contact metallization layer | |
Jeong et al. | Effect of temperature on shear properties of Sn-3.0 Ag-0.5 Cu and Sn-58Bi solder joints |