Sil'man et al., 1982 - Google Patents
Castings From Wear Resistant Complex-Alloy White Cast IronSil'man et al., 1982
- Document ID
- 8379029548639431577
- Author
- Sil'man G
- Frol'tsov M
- Zhukov A
- Publication year
- Publication venue
- Liteinoe Proizvod.
External Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C37/00—Cast-iron alloys
- C22C37/06—Cast-iron alloys containing chromium
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Sil'man et al. | Castings From Wear Resistant Complex-Alloy White Cast Iron | |
NO177503C (en) | Bainitic paint body | |
Kufa | Abrasion Resistant Alloy With High Carbon and Chrome Content | |
FR2297673A1 (en) | Wear resistant parts for crushing machinery - using steel castings contg. white martensitic cast iron inserts for long life | |
Teikh | Effect of Technological Factors on Wear Resistance of Parts in Shot-Peening Apparatus | |
Gahr et al. | Abrasive Wear Resistance of Ductile Iron With Different Secondary Structures | |
SU377405A1 (en) | STEEL | |
Rohrig | Annual Review. Alloyed Cast Iron. 1976 | |
JPS6455321A (en) | Auxiliary material charging chute in steel refining furnace | |
Sil'man et al. | Characteristics of Microstructure and Elements Distribution in Complex-Alloyed White Cast Irons | |
Tishaev et al. | Effect of Alloying on the Fine Structure and Mechanical Properties of Heat Resistant Die Steel | |
Shabatinov et al. | Conditions for the Wear Resistance of Cast Iron | |
Golovanenko | Properties and Susceptibility to Hydrogen Uptake of Steels of Various Antimony Contents | |
Chzhan | High-strength iron production in China[[Previously Titled: Production of high-strength cast irons in the Peoples Republic of China.]] | |
Sil'man et al. | Wear Resistance of High-Strength Cast Irons With Elevated Silicon Content | |
Bushchik et al. | High-Manganese Steel for Cast Parts Operating in the Extreme North | |
Agapova et al. | Structure and Properties of Deformed White Cast Iron Alloyed With Vanadium, Niobium and Titanium | |
Rohrig | Cast abrasion resistant iron base alloys | |
Pyatakova et al. | Wear Resistant Alloy for Increasing Service Life of Mill Lining Parts | |
Berns | Wear resistant steels | |
Adamic et al. | Research into and modelling of the wear of hard faced machine parts | |
Thieme | Manufacture and Installation of Cast Iron CX 300 CrMo 15 3 for Workpieces in the Coal Preparation Industry | |
Cox | Some properties of ductile, nickel-containing, lean-alloy austenitic irons | |
Rohrig | Wear Resistant White Chromium--Molybdenum Cast Iron | |
JPS6043535A (en) | Claw for excavator |