Manufacture Of Porous Articles, And Recovery And Treatment Of Waste Products
(AREA)
Abstract
A process for producing a plastic material, which mainly comprises: A. mixing raw materials including 0.28%-0.47% of stearate, 0.42%-0.70% of barium stearate, 0.47%-0.65% of lead stearate, etc. in a mixer for 28~32 minutes, in which the temperature in the mixer is maintained at 170 degrees to 180 degrees; B. adding 0.56%-0.93% of sulphur, 92.18%-94.04% of rigid ethylene-vinyl acetate copolymers (EVA), 0.14%-0.23% of asphalt to be mixed for 18~22 minutes, in which the temperature in the mixer is maintained at 170 degrees to 180 degrees; C. adding 0.37%-0.56% of cadmium stearate, 0.33%-0.61% of a cross-linking agent, 0.93%-3.72% of a blowing agent to be mixed for 18~22 minutes, in which the temperature in the mixer is maintained at 170 degrees to 180 degrees; thereby producing a plastic material having a one-time foaming property.
TW086103971A1997-03-281997-03-28Process for producing a plastic material