RU2072142C1 - METHOD OF LIFTING AND OPERATION OF INTERMEDIATE DUCKS FOR CONTINUOUS METAL Pouring - Google Patents
METHOD OF LIFTING AND OPERATION OF INTERMEDIATE DUCKS FOR CONTINUOUS METAL Pouring Download PDFInfo
- Publication number
- RU2072142C1 RU2072142C1 RU94005655/02A RU94005655A RU2072142C1 RU 2072142 C1 RU2072142 C1 RU 2072142C1 RU 94005655/02 A RU94005655/02 A RU 94005655/02A RU 94005655 A RU94005655 A RU 94005655A RU 2072142 C1 RU2072142 C1 RU 2072142C1
- Authority
- RU
- Russia
- Prior art keywords
- template
- lining
- tundish
- ducks
- lifting
- Prior art date
Abstract
Способ футеровки и эксплуатации промежуточных ковшей для непрерывной разливки металлов, включающий установку в корпусе промежуточного ковша шаблона с зазором по периметру корпуса ковша, заливку в зазоры жидкой огнеупорной массы, получение монолитной футеровки, удаление шаблона, доведение температуры монолитной футеровки до 1000-1200С, заполнение промежуточного ковша жидким металлом, отличающийся тем, что в зазоры заливают огнеупорную массу при 1400-2000С, расплавленную в нагревательной печи, получение монолитной футеровки и доведение ее температуры до 1000-1200С осуществляют путем замедленного охлаждения, после чего удаляют шаблон, при этом монолитную футеровку выдерживают при 1000-1200С до заполнения промежуточного ковша металлом.A method of lining and operating tundish ladles for continuous casting of metals, including installing a template with a gap around the perimeter of the ladle body in the tundish body, pouring liquid refractory mass into the gaps, obtaining a monolithic lining, removing the template, bringing the temperature of the monolithic lining to 1000-1200C, filling the intermediate ladle with liquid metal, characterized in that a refractory mass is poured into the gaps at 1400-2000C, melted in a heating furnace, a monolithic lining is obtained and its temperature is brought to 1000-1200C by slow cooling, after which the template is removed, while the monolithic lining is maintained at 1000-1200C until the tundish is filled with metal.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
RU94005655/02A RU2072142C1 (en) | 1994-02-17 | 1994-02-17 | METHOD OF LIFTING AND OPERATION OF INTERMEDIATE DUCKS FOR CONTINUOUS METAL Pouring |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
RU94005655/02A RU2072142C1 (en) | 1994-02-17 | 1994-02-17 | METHOD OF LIFTING AND OPERATION OF INTERMEDIATE DUCKS FOR CONTINUOUS METAL Pouring |
Publications (2)
Publication Number | Publication Date |
---|---|
RU94005655A RU94005655A (en) | 1995-10-20 |
RU2072142C1 true RU2072142C1 (en) | 1997-01-20 |
Family
ID=48434273
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
RU94005655/02A RU2072142C1 (en) | 1994-02-17 | 1994-02-17 | METHOD OF LIFTING AND OPERATION OF INTERMEDIATE DUCKS FOR CONTINUOUS METAL Pouring |
Country Status (1)
Country | Link |
---|---|
RU (1) | RU2072142C1 (en) |
-
1994
- 1994-02-17 RU RU94005655/02A patent/RU2072142C1/en active
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3263883D1 (en) | Process for making cast pieces with inserted steel tubes | |
RU2111830C1 (en) | Gear to feed molten metal into plant of continuous vertical casting with drawing billets upwards and machine using this gear | |
ES419282A1 (en) | Method for pouring steel during continuous casting | |
FR2444245A1 (en) | Metallurgical furnace wall unit prodn. process - shapes heat-resistant material into mould wall for cast metal cooling block | |
GB1208333A (en) | Method of apparatus and mould for semicontinuously casting metal ingots | |
JPS61176447A (en) | Starting method of casting and side seal heater in roll type continuous casting installation | |
RU2072142C1 (en) | METHOD OF LIFTING AND OPERATION OF INTERMEDIATE DUCKS FOR CONTINUOUS METAL Pouring | |
JPS564350A (en) | Tundish for continuous casting | |
CA2075484A1 (en) | Process and installation for renewing the refractory lining of foundry ladles | |
SU1234046A1 (en) | Arrangement for heating ceramic moulds and filling them with metal | |
US4506425A (en) | Method for the hot repair of the protective layer provided on the permanent lining of a tundish of a continuous casting plant | |
RU94005655A (en) | METHOD OF LAYING AND OPERATING INTERMEDIATE BUCKETS FOR CONTINUOUS METAL CASTING | |
GB2091399A (en) | Tundish pouring apparatus and method of use | |
SU1740118A1 (en) | Apparatus for casting hollow ingots | |
SU1087254A1 (en) | Fountain for casting steel | |
SU822979A2 (en) | Apparatus for casting hollow ingots | |
SU895110A1 (en) | Method for making mold castings | |
JPS5325210A (en) | Steel refining method | |
Chuprina et al. | Use of cast refractories when repairing steel casting ladles | |
JPS5674352A (en) | Production of thin-walled iron casting | |
Khasin | The Effect of Bottom Pouring Conditions on Ingot Quality | |
SU971910A1 (en) | Apparatus for modifying molten metal in casting mold | |
Podgorskii et al. | Overheating of malleable iron during small castings production | |
JPS5633160A (en) | Die casting method of iron or steel | |
Vandemaele | DEVELOPMENT OF REFRACTORIES FOR THE CONTINUOUS CASTING OF STEEL |