JPS63131752U - - Google Patents
Info
- Publication number
- JPS63131752U JPS63131752U JP2358387U JP2358387U JPS63131752U JP S63131752 U JPS63131752 U JP S63131752U JP 2358387 U JP2358387 U JP 2358387U JP 2358387 U JP2358387 U JP 2358387U JP S63131752 U JPS63131752 U JP S63131752U
- Authority
- JP
- Japan
- Prior art keywords
- metal
- base material
- ceramic coating
- thermal spraying
- sprayed surface
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は本考案の一実施例を示す平面図、第2
図はそのA―A拡大断面図、第3図は本考案のも
のの製造を示す断面図、第4図、第5図はそれぞ
れ本考案の他の実施例の拡大断面図、第6図は従
来の製造法を示す断面図である。
1……金属母材、2……セラミツク被膜、3…
…溶射面、5,5a……溝(周縁溝)。
Fig. 1 is a plan view showing one embodiment of the present invention;
The figure is an enlarged cross-sectional view taken along line A-A, FIG. 3 is a cross-sectional view showing the manufacture of the device of the present invention, FIGS. 4 and 5 are enlarged cross-sectional views of other embodiments of the present invention, and FIG. 6 is a conventional FIG. 2 is a sectional view showing a manufacturing method. 1...metal base material, 2...ceramic coating, 3...
... Sprayed surface, 5, 5a... Groove (peripheral groove).
Claims (1)
に形成した金属とセラミツクスの接合構造におい
て、上記金属母材の溶射面周縁に溝を設け、溶射
によりその周縁溝を含む溶射面上にセラミツク被
膜を形成してなることを特徴とする金属とセラミ
ツクスの接合構造。 In a metal-ceramics joint structure in which a ceramic coating is partially formed on a metal base material by thermal spraying, a groove is provided at the periphery of the sprayed surface of the metal base material, and a ceramic coating is formed on the sprayed surface including the peripheral groove by thermal spraying. A bonded structure of metal and ceramics characterized by: