JPS5781863A - Method and apparatus for coating antifriction material to inner peripheral face of wiring tube - Google Patents
Method and apparatus for coating antifriction material to inner peripheral face of wiring tubeInfo
- Publication number
- JPS5781863A JPS5781863A JP15779480A JP15779480A JPS5781863A JP S5781863 A JPS5781863 A JP S5781863A JP 15779480 A JP15779480 A JP 15779480A JP 15779480 A JP15779480 A JP 15779480A JP S5781863 A JPS5781863 A JP S5781863A
- Authority
- JP
- Japan
- Prior art keywords
- wiring tube
- antifriction material
- inner peripheral
- tube
- peripheral face
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To coat antifriction material to inside face of a wiring tube uniformly and at high efficiency by injecting antifriction material into inside of a wiring tube, fitting a slide piece made of an elastic body and moving it using compressed air.
CONSTITUTION: After injecting antifriction material M from an end of a wiring tube P to inside P' of the tube, a slide piece 1 made of an elastic body soaked in antifriction material M is fitted inside P' of the wiring tube P. A hose H is connected to the wiring tube P and compressed air is blown in to move the slide piece 1 to the tip of the wiring tube P. In this way, the antifriction material can be applied to inside of the wiring tube uniformly and at high efficiency.
COPYRIGHT: (C)1982,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15779480A JPS5781863A (en) | 1980-11-10 | 1980-11-10 | Method and apparatus for coating antifriction material to inner peripheral face of wiring tube |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15779480A JPS5781863A (en) | 1980-11-10 | 1980-11-10 | Method and apparatus for coating antifriction material to inner peripheral face of wiring tube |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5781863A true JPS5781863A (en) | 1982-05-22 |
Family
ID=15657424
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15779480A Pending JPS5781863A (en) | 1980-11-10 | 1980-11-10 | Method and apparatus for coating antifriction material to inner peripheral face of wiring tube |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5781863A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH04208425A (en) * | 1990-11-30 | 1992-07-30 | Aaru Pii Toupura Kk | Manufacture of hollow body |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS54132986A (en) * | 1978-04-04 | 1979-10-16 | Osaka Gas Co Ltd | Body movable in pipe |
JPS54134751A (en) * | 1978-04-07 | 1979-10-19 | Taylor Industries | Liquid coating on pipe internal surface and apparatus therefor |
-
1980
- 1980-11-10 JP JP15779480A patent/JPS5781863A/en active Pending
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS54132986A (en) * | 1978-04-04 | 1979-10-16 | Osaka Gas Co Ltd | Body movable in pipe |
JPS54134751A (en) * | 1978-04-07 | 1979-10-19 | Taylor Industries | Liquid coating on pipe internal surface and apparatus therefor |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH04208425A (en) * | 1990-11-30 | 1992-07-30 | Aaru Pii Toupura Kk | Manufacture of hollow body |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS56158167A (en) | Method and device for spraying powder | |
DE3066513D1 (en) | Method, apparatus and spray nozzle for coating the inner surface of long tubes of small diameter | |
ES457042A1 (en) | Method for rust-protecting treatment | |
JPS5781863A (en) | Method and apparatus for coating antifriction material to inner peripheral face of wiring tube | |
JPS57157927A (en) | Soot blower equipment | |
JPS5748352A (en) | Powdery body change-over apparatus | |
JPS5525365A (en) | Mold | |
JPS555755A (en) | Spray coating method | |
JPS57127853A (en) | Partial injection | |
JPS5742378A (en) | Lining method for interior wall surface of pipe | |
JPS578006A (en) | Cleaning device for workpiece gripper | |
JPS5447767A (en) | Inner surface treatment of conduit already constructed | |
JPS5518322A (en) | Nozzle for sand blasting inner surface of tube and method of using the same | |
JPS54112725A (en) | Multiihead air spray gun apparatus | |
JPS5387085A (en) | Method of shot peening | |
JPS5264778A (en) | Removing method for clogging powder of pneumatic powder supplier | |
JPS5229832A (en) | Method and apparatus for the coating and wiping of liquid substance | |
JPS51126517A (en) | Rubber hose | |
JPS5736613A (en) | Lining method for internal wall of pipe | |
JPS5781862A (en) | Method and apparatus for coating | |
JPS5419580A (en) | Lighting apparatus with air duct | |
JPS56147655A (en) | Inside surface painting machine for small-diameter pipe | |
JPS5313650A (en) | Method of electrostatic coating | |
JPS5347697A (en) | Method of forming film of coating under the water | |
JPS539841A (en) | Method and apparatus for coating water paint |