JPS577571B2 - - Google Patents
Info
- Publication number
- JPS577571B2 JPS577571B2 JP1901977A JP1901977A JPS577571B2 JP S577571 B2 JPS577571 B2 JP S577571B2 JP 1901977 A JP1901977 A JP 1901977A JP 1901977 A JP1901977 A JP 1901977A JP S577571 B2 JPS577571 B2 JP S577571B2
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Glass Melting And Manufacturing (AREA)
- Glass Compositions (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1901977A JPS53102916A (en) | 1977-02-22 | 1977-02-22 | Production of glass having constant water content |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1901977A JPS53102916A (en) | 1977-02-22 | 1977-02-22 | Production of glass having constant water content |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS53102916A JPS53102916A (en) | 1978-09-07 |
JPS577571B2 true JPS577571B2 (en) | 1982-02-12 |
Family
ID=11987759
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1901977A Granted JPS53102916A (en) | 1977-02-22 | 1977-02-22 | Production of glass having constant water content |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS53102916A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6227672U (en) * | 1985-08-05 | 1987-02-19 | ||
JPH01159877U (en) * | 1987-11-14 | 1989-11-06 |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP3156375B1 (en) | 2014-06-12 | 2019-04-10 | AGC Inc. | Method for manufacturing molten glass and method for manufacturing glass product |
CN108793716A (en) * | 2018-06-21 | 2018-11-13 | 明光康诚伟业机电设备有限公司 | A kind of constant temperature and humidity mobile phone camera glass production device |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3617231A (en) * | 1968-06-10 | 1971-11-02 | Brockway Glass Co Inc | Method of controlling the softening point and working temperature of soda-lime glass by regulating the water content of the glass melt |
JPS51146509A (en) * | 1975-05-29 | 1976-12-16 | Philadelphia Quartz Co | Method of manufacturing alkaline metal silicate glass |
JPS5218715A (en) * | 1975-08-04 | 1977-02-12 | Nippon Electric Glass Co | Method of homogenizing glass |
-
1977
- 1977-02-22 JP JP1901977A patent/JPS53102916A/en active Granted
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3617231A (en) * | 1968-06-10 | 1971-11-02 | Brockway Glass Co Inc | Method of controlling the softening point and working temperature of soda-lime glass by regulating the water content of the glass melt |
JPS51146509A (en) * | 1975-05-29 | 1976-12-16 | Philadelphia Quartz Co | Method of manufacturing alkaline metal silicate glass |
JPS5218715A (en) * | 1975-08-04 | 1977-02-12 | Nippon Electric Glass Co | Method of homogenizing glass |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6227672U (en) * | 1985-08-05 | 1987-02-19 | ||
JPH01159877U (en) * | 1987-11-14 | 1989-11-06 |
Also Published As
Publication number | Publication date |
---|---|
JPS53102916A (en) | 1978-09-07 |