[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

JPS5666371A - Die casting method of aluminum alloy casting - Google Patents

Die casting method of aluminum alloy casting

Info

Publication number
JPS5666371A
JPS5666371A JP14035579A JP14035579A JPS5666371A JP S5666371 A JPS5666371 A JP S5666371A JP 14035579 A JP14035579 A JP 14035579A JP 14035579 A JP14035579 A JP 14035579A JP S5666371 A JPS5666371 A JP S5666371A
Authority
JP
Japan
Prior art keywords
casting
aluminum alloy
die
dies
cooling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP14035579A
Other languages
Japanese (ja)
Inventor
Ryoichi Shibata
Kazuyoshi Harafuji
Masatoshi Harada
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Proterial Ltd
Original Assignee
Hitachi Metals Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Metals Ltd filed Critical Hitachi Metals Ltd
Priority to JP14035579A priority Critical patent/JPS5666371A/en
Publication of JPS5666371A publication Critical patent/JPS5666371A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To obtain aluminum alloy castings of good airtightness and mechanical properties by specifying die temp., cooling water flow and cooling starting time.
CONSTITUTION: After die heating temp. is kept at 200W400°C, the dies are water- cooled at water flow rates of 60W500l/min.m2 before molten metal is poured into the dies. Before the water cooling effect reaches the inside surface of the dies, the molten metal is poured and the cooling is continuted until after the completion of the freezing of the casting. This makes possible the production of the aluminum alloy casting which is free from any surface defects, has fine crystal grain sizes of the casting surface and casting inside and has consequently superior airtightness and mechanical properties. In addition, the good casting is produced without being affected by die ratios.
COPYRIGHT: (C)1981,JPO&Japio
JP14035579A 1979-10-30 1979-10-30 Die casting method of aluminum alloy casting Pending JPS5666371A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP14035579A JPS5666371A (en) 1979-10-30 1979-10-30 Die casting method of aluminum alloy casting

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14035579A JPS5666371A (en) 1979-10-30 1979-10-30 Die casting method of aluminum alloy casting

Publications (1)

Publication Number Publication Date
JPS5666371A true JPS5666371A (en) 1981-06-04

Family

ID=15266891

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14035579A Pending JPS5666371A (en) 1979-10-30 1979-10-30 Die casting method of aluminum alloy casting

Country Status (1)

Country Link
JP (1) JPS5666371A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6030569A (en) * 1983-07-29 1985-02-16 Mitsubishi Motors Corp Production of cylinder head
JPH01143752A (en) * 1987-11-30 1989-06-06 Kobe Steel Ltd Casting for compressor and its manufacture

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6030569A (en) * 1983-07-29 1985-02-16 Mitsubishi Motors Corp Production of cylinder head
JPH01143752A (en) * 1987-11-30 1989-06-06 Kobe Steel Ltd Casting for compressor and its manufacture
JPH0358823B2 (en) * 1987-11-30 1991-09-06 Kobe Steel Ltd

Similar Documents

Publication Publication Date Title
JPS61169149A (en) Continuous casting method
JPS57127553A (en) Hot top continuous casting method for aluminum
JPS5666371A (en) Die casting method of aluminum alloy casting
GB1256058A (en) Apparatus and method for single cyrstal casting
JP3536559B2 (en) Method for forming semi-solid metal
US3225399A (en) Casting process using borax-silica slag
JPS57109546A (en) Casting method for hollow billet
JPS5592260A (en) Steel manufactured by continuous casting method and production thereof
JPS55149771A (en) Production of aluminum alloy casting
JPS57160567A (en) Purifying method for metal
JPS5561365A (en) Production of molding of fe-a -si base alloy
Berezhiani et al. Effect of Casting Under a High Gas Pressure on the Structure and Properties of Aluminum and Copper Alloys
JPS5739164A (en) Preparation of heat resistant aluminum alloy conductor
JPS61176454A (en) Continuous casting device
JPS61169139A (en) Continuous casting device
SU1135547A1 (en) Method of low-pressure die casting
JPS6087963A (en) Method and device for continuous casting of metallic casting ingot having smooth surface
JPS54110118A (en) Treating method for molten metal
JPS57134235A (en) Production of polycrystalline silicon semiconductor
JPH0191948A (en) Method and apparatus for semi-continuously casting cast billet
SU1242294A1 (en) Method of producing ingot
JPS56122662A (en) Preventing method of casting crack of antiferromagnetic chromium invar alloy ingot
SU1678509A1 (en) Method for semicontinuous casting nickel
US1867804A (en) Method of producing magnetic alloys
JPS5536030A (en) Molten metal forging method