JPS5613472A - Continuously hot dipping apparatus - Google Patents
Continuously hot dipping apparatusInfo
- Publication number
- JPS5613472A JPS5613472A JP8815779A JP8815779A JPS5613472A JP S5613472 A JPS5613472 A JP S5613472A JP 8815779 A JP8815779 A JP 8815779A JP 8815779 A JP8815779 A JP 8815779A JP S5613472 A JPS5613472 A JP S5613472A
- Authority
- JP
- Japan
- Prior art keywords
- substance
- attached
- gas
- snout
- foreign matter
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To prevent the occurrence of surface defects by spraying a gas upon a substance to be hot dipped to remove foreign matter immediately before the substance enters a molten metal. CONSTITUTION:Foreign matter removing device 4, 4a are attached to a naked portion of snout 1 over the surface of molten metal 2. Devices 4, 4a are composed of two gas feed pipes 5, 5a inserted into snout 1 so that they are positioned at both sides of substance 3 to be hot dipped, valves 6, 6a attached to pipes 5, 5a outside snout 1, respectively, pressure gauges 7, 7a attached to each pipe 5, 5a before and behind each valve 6, 6a, and a plurality of nozzles 8, 8a attached to pipes 5, 5a in line, respectively. When valves 6, 6a are opened to feed an inert gas or the like, the gas is radiately spouted from nozzles 8, 8a against the boundary where substance 3 enters molten metal 2 to remove foreign matter stuck to substance 3.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP54088157A JPS582586B2 (en) | 1979-07-13 | 1979-07-13 | Continuous molten metal plating equipment |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP54088157A JPS582586B2 (en) | 1979-07-13 | 1979-07-13 | Continuous molten metal plating equipment |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5613472A true JPS5613472A (en) | 1981-02-09 |
JPS582586B2 JPS582586B2 (en) | 1983-01-17 |
Family
ID=13935080
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP54088157A Expired JPS582586B2 (en) | 1979-07-13 | 1979-07-13 | Continuous molten metal plating equipment |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS582586B2 (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6141754A (en) * | 1984-07-30 | 1986-02-28 | アームコ、インコーポレーテツド | Control of zinc vapor at cylinder port in applying molten zinc plating to iron base metal strip |
JPH0884793A (en) * | 1994-09-19 | 1996-04-02 | Z Kk | Bat |
JP2018515693A (en) * | 2015-05-27 | 2018-06-14 | ティッセンクルップ スチール ヨーロッパ アクチェンゲゼルシャフトThyssenKrupp Steel Europe AG | Apparatus and method for improved extraction of metal vapor |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5054530A (en) * | 1973-09-14 | 1975-05-14 | ||
JPS5554358U (en) * | 1978-10-04 | 1980-04-12 |
-
1979
- 1979-07-13 JP JP54088157A patent/JPS582586B2/en not_active Expired
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5054530A (en) * | 1973-09-14 | 1975-05-14 | ||
JPS5554358U (en) * | 1978-10-04 | 1980-04-12 |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6141754A (en) * | 1984-07-30 | 1986-02-28 | アームコ、インコーポレーテツド | Control of zinc vapor at cylinder port in applying molten zinc plating to iron base metal strip |
JPH0129866B2 (en) * | 1984-07-30 | 1989-06-14 | Armco Inc | |
JPH0884793A (en) * | 1994-09-19 | 1996-04-02 | Z Kk | Bat |
JP2018515693A (en) * | 2015-05-27 | 2018-06-14 | ティッセンクルップ スチール ヨーロッパ アクチェンゲゼルシャフトThyssenKrupp Steel Europe AG | Apparatus and method for improved extraction of metal vapor |
Also Published As
Publication number | Publication date |
---|---|
JPS582586B2 (en) | 1983-01-17 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EG14710A (en) | Method and apparatus for positionning the point of droplet formation in the jetting fluid of an electroatatic sorting device | |
DE3069421D1 (en) | Apparatus and method for spray metallizing a corrodible metal substrate with a protective metal | |
ES8600487A1 (en) | Method and apparatus for removing protective coating from pipe section. | |
GB2022807B (en) | Method of removing frost deposits from cooling coil batteries or the like in a freezing plant during operation and apparatus for carrying out the method | |
EG12493A (en) | Method and apparatus for the realisation of the distribution of a medium supplied through a pipe line | |
DE3466423D1 (en) | Method of sprinkling bits and/or working-faces by means of a pressurized fluid, and device for carrying out the method | |
JPS5613472A (en) | Continuously hot dipping apparatus | |
DE3165586D1 (en) | A method and apparatus for controlling the centrifugal casting of a metal pipe | |
JPS56107863A (en) | Splash removal device | |
JPS56154233A (en) | Method and device for repairing pipe from inside | |
JPS57156155A (en) | Grinding method | |
CH403136A (en) | Process for removing the liquid from the outlet line of a hydraulic fluid conveying system located behind the shut-off valve at the end of each operating interval and device for carrying out the process | |
JPS57104671A (en) | Continuously spray pickling apparatus for strip | |
JPS5418580A (en) | Method of removing moisture on inner surface of steel pipe | |
JPS55122674A (en) | Scarfing device | |
JPS55141578A (en) | Sealing device of tank | |
JPS5244963A (en) | Method and apparaus for removing accumulated material on hopper surfac e | |
JPS5785720A (en) | Device for truing up end faces of long materials | |
JPS52130155A (en) | Method of and apparatus for pickling elongated small-diametered metal tube | |
JPS531369A (en) | Device for removing magnetic foreign material in cooling water | |
JPS5424239A (en) | Protecting method for spot welding electrode | |
JPS57207569A (en) | Method and apparatus for roll coating | |
JPS5699009A (en) | Removing method for rolling mill oil in cold rolling work for metallic strip | |
JPS57102271A (en) | Method and device for lining of inside wall surface of piping | |
Lu et al. | A Study on Behaviour of the Internal Crack of Continuous Casting Bloom in PPM Process |