DE2234902A1 - METHOD AND DEVICE FOR EDGE PROCESSING AND COATING ON PANEL-SHAPED WORKPIECES - Google Patents
METHOD AND DEVICE FOR EDGE PROCESSING AND COATING ON PANEL-SHAPED WORKPIECESInfo
- Publication number
- DE2234902A1 DE2234902A1 DE19722234902 DE2234902A DE2234902A1 DE 2234902 A1 DE2234902 A1 DE 2234902A1 DE 19722234902 DE19722234902 DE 19722234902 DE 2234902 A DE2234902 A DE 2234902A DE 2234902 A1 DE2234902 A1 DE 2234902A1
- Authority
- DE
- Germany
- Prior art keywords
- coating
- glue
- protruding part
- edge
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
dr. ing. H. NEGENDaNK · dipping. H. HAlJCK · βιρι,.-phys. W. SCHMITZ dipping. E. GKAAEFS ■ dipping. W. WEHNERTdr. ing. H. NEGENDaNK · dipping. H. HAlJCK · βιρι, .- phys. W. SCHMITZ dipping. E. GKAAEFS ■ dipping. W. WEHNERT
HAMBURG-MÜNCHEN 2234902HAMBURG-MUNICH 2234902
ZUSTELITJN6SA]SSCHHIFT: ZUSTELITJN6SA] SSCHHIFT: HAMBTJRG 36 · NETTER HAMBTJRG 36 NICE WALL 41WALL 41
TEL·. 30 74 SS TTND 38 41 13TEL ·. 30 74 SS TTND 38 41 13
Böttcher & Gessner München is · mozartsth. 23Böttcher & Gessner Munich is · mozartsth. 23
TEL·. S 38 03 88TEL ·. P. 38 03 88
fiOOO üaniPUrg -?U telegh. nügedapaie»t München fiOOO üaniPUrg -? U telegh. nügedapaie »t Munich
Gasstraße 18 ■ " . .nr7o Gasstrasse 18 ■ " .. Nr7o
Hamburg, 14. Juli 1972Hamburg, July 14, 1972
Verfahren und Vorrichtung zur Kantenbearbeitung' und -beschichtung an plattenförmigen WerkstückenMethod and device for edge processing and coating on plate-shaped workpieces
Die Erfindung bezieht sich auf ein Verfahren zur Kantenbearbeitung und -beschichtung an plattenförmigen Werkstükken mit mindestens einer geradlinigen Kante, daren Oberfläche eine Beschichtung aufweist, bei dem nach einer spangebenden Bearbeitung der geradlinigen Kante diese mit einer Beschichtung verleimt wird.The invention relates to a method for edge processing and coating on plate-shaped workpieces with at least one straight edge, the surface has a coating in which after a machining of the straight edge this with a Coating is glued.
Bei dem bisher bekannten Verfahren zur Kantenbearbeitung und -beschichtung an plattenförmigen Werkstücken wird normalerweise so vorgegangen, daß nach dem spangebenden Kantenbearbeiten und der Leimabgabe getrennte Furnier- oder Kunststoffstreifen auf die Kanten aufgezogen werden. Ein derartiges Verfahren weist jedoch eine Reihe von Nachteilen auf. So sind nach dem Veflßimen infolge von unterschiedlichen Abmessungen zwischen den aufgeleimten Streifen und der Plattenstärke und wegen des Überstands der Streifen an den Vorder- und Hinterkanten zusätzliche Bearbeitungsgänge erforderlich wie Kappen, Bündigschneiden, Fasen usw. DieIn the previously known method for edge processing and coating on plate-shaped workpieces is normally carried out in such a way that after the machining of the edges and the glue dispensing separate veneer or plastic strips are pulled onto the edges. A However, such a method has a number of disadvantages. So are after the flow of different Dimensions between the glued-on strips and the panel thickness and because of the protrusion of the strips the front and rear edges require additional processing steps such as cutting, flush cutting, bevelling, etc. The
— 2 —- 2 -
309885/0153309885/0153
einzelnen Arbeitsgänge können von nacheinander angeordneten Einzelmaschinen oder auch von Maschinenkombinationen durchgeführt werden. Auf jeden Fall ist jedoch der Vorschubgeschwindigkeit, insbesondere im Hinblick auf das Kappen der überstehenden Streifen an der Vorder- und Hinterkante,Grenzen gesetzt. Die hierbei mögliche Geschwindigkeit liegt weit unterhalb der, mit der die für die Verleimung erforderlichen Arbeitsgänge einschließlich der Besäumung plattenförmiger Werkstücke vor sich gehen kann. Werden verhältnismäßig dünne Platten bearbeitet, z.B. wie sie in der Radio- und Fernsehgehäuse Industrie verwendet werden, müssen an den handelsüblichen Streifenbreiten für die Kanten nicht unerhebliche Zerspanungen durchgeführt werden, um die Streifen auf die gewünschte Plattenstärke zu bringen. Abgesehen von dem hierfür erforderlichen Fertigungsaufwand liegt auch eine schlechte Materialausnutzung vor.individual operations can be arranged one after the other Individual machines or machine combinations can be carried out. In any case, however, the feed rate, in particular with regard to the cutting of the protruding strips on the front and rear edges, limits set. The speed possible here is far below the speed required for gluing Operations including the trimming of plate-shaped workpieces can go on. Become relatively thin Plates processed, e.g. as they are used in the radio and television housing industry, must be adapted to the commercially available ones Strip widths for the edges not inconsiderable machining operations are carried out to the strips on the to bring the desired plate thickness. Apart from the manufacturing effort required for this, there is also a bad one Material utilization before.
Ein weiterer Nachteil besteht darin, daß für die Beschichtung der Platfcenkanten nicht in allen Fällen der gleiche Werkstoff verwendet werden kann wie für die Beschichtung der Plattenoberfläche. Dadurch kommt es zu Farbunterschieden zwischen der Oberfläche und der Plattenkante, die bei fertigen Teilen deutlich sichtbar sind.Another disadvantage is that the coating of the plate edges is not always the same material can be used as for the coating of the plate surface. This leads to color differences between the surface and the plate edge, which are clearly visible in finished parts.
!509885/015 3! 509885/015 3
Es ist daher Aufgabe der Erfindung, die oben angeführten Nachteile zu überwinden und ein Verfahren-anzugeben, mit dem auf.einfache materialeinsparende Weise eine Kantenbearbeitung und -beschichtung an plattenförmigen Werkstükken vorgenommen werden kann.It is therefore the object of the invention to provide the above Disadvantages to be overcome and a procedure to be specified with edge processing in a simple, material-saving way and coating can be carried out on plate-shaped workpieces.
Bei einem·Verfahren der eingangs genannten Art wird diese Aufgabe dadurch gelöst, daß an der geradlinigen Kante des beschichteten Werkstücks Material so entfernt wird, daß die Beschichtung um einen gewissen Betrag übersteht, daß anschließend an der Kante Leim aufgetragen wird und daß schließlich der überstehende Teil der Beschichtung umgelegt und gegen die Kantenfläche gepr&fc wird.In the case of a method of the type mentioned at the outset, this The object is achieved in that material is removed from the straight edge of the coated workpiece in such a way that the coating protrudes to a certain extent that glue is then applied to the edge and that Finally, the protruding part of the coating is turned over and pressed against the edge surface.
Das erfindungsgemäße Verfahren ist für Werkstücke mit einfächer oder doppelseitiger Beschichtung gleichermaßen geeignet. Im Unterschied zu bekannten Verfahren wird bei der Erfindung die Kante des Werkstücks mit dem gleichen Material beschichtet wie die Oberfläche. Hierzu wird das Material in bekannter, geeigneter Weise so entfernt, daß die Oberflächenbeschichtung um einen gewissen Betrag übersteht, so daß der überstehende Teil um 90° gegen die Plattenkante herum gelegt werden kann. Besteht das BeSchichtungsmaterial aus einem elastischen Werkstoff, wird der überstehende Teil in geeigneter Weise umgebogen, so daß mittels des vorher aufgebrachten Leims ein Verleimen stattfinden kann. Auf diese WeiseThe inventive method is simple for workpieces or double-sided coating is equally suitable. In contrast to known methods, the invention the edge of the workpiece is coated with the same material as the surface. For this purpose, the material is in known, suitably removed so that the surface coating protrudes by a certain amount, so that the protruding part can be placed against the panel edge by 90 °. If the coating material consists of a elastic material, the protruding part is bent in a suitable manner, so that by means of the previously applied Gluing can take place. In this way
309885/0153309885/0153
ist immer gewährleistet, daß Plattenkante und Plattenoberfläche die gleiche Farbgebung besitzen. Ein nachträgliches Bearbeiten, insbesondere eine serspanende Bearbeitung, entfällt beim erfindungsgemäßen Verfahren» Die einzelnen Arbeitsgänge, wie geradlinige zerspanende Bearbeitung der Kante, Aufbringen des Leims und Umlegen des überstehenden Teils der Beschichtung, können mit großer Yorachubgeschwindigkeit durchgeführt werden, Dadurch wird eine hohe Produktionsrate erzielt, denn die Werkstücke können unmittelbar nacheinander aufgegeben werden, entweder von Hand oder automatisch.it is always guaranteed that the panel edge and panel surface have the same color. An afterthought Machining, in particular machining, is not required in the method according to the invention »The individual operations, such as straight machining of the edge, applying the glue and turning over the protruding part of the coating, can be carried out at a high Yorachub speed, this achieves a high production rate, because the workpieces can be fed in immediately one after the other, either manually or automatically.
Gemäß einer Ausführung der Erfindung ist vorgesehen, daß das Material im Bereich der Linie5 um den die Beschichtung umgelegt wird, bis zur Beschichtung entfernt wird. Dies erweist sich besonders dann als vorteilhaft, wenn es sich um eine elastische Beschichtung handelt. Wird hingegen eine steife Beschichtung verwendet, die sich nicht um einen Winkel von 90° verbiegen läßt, wie Furnier, Laminate usw., sieht eine andere Ausführungsform der Erfindung vor, daß auf die Außenseite der Beschichtung im Bereich der Linie, um die die Beschichtung umgelegt wird, eine elastische Folie aufgeklebt wird, daß dann das Material zumindest im Bereich dieser Linie bis auf die Folie entfernt wird, und daß die Folie nach dem Umlegen und Verleimen des übersiehenden Teils der Beschichtung entfernt wird. Bei dieser Ausführungsart des erfindungsgemäßen Verfahrens wird der überstehende Teil der Beschichtung abgetrennt, bleibt jedoch durch den· Folienstreifen an seinem Ort, so daß der überstehende Teil nach dem Aufbringen des Leims dank derAccording to one embodiment of the invention it is provided that the material is folded over in the area of the line 5 around the coating until the coating is removed. This proves to be particularly advantageous when it comes to a elastic coating. If, on the other hand, a stiff coating is used that does not move at an angle of Can bend 90 °, such as veneer, laminates, etc., another embodiment of the invention provides that on the outside an elastic film is glued to the coating in the area of the line around which the coating is wrapped, that the material is then removed, at least in the region of this line, down to the film, and that the film is removed after it has been turned over and gluing the overlaying portion of the coating is removed. In this embodiment of the invention In the process, the protruding part of the coating is cut off, however, remains in place through the film strip, so that the protruding part after the glue has been applied thanks to the
Elastizität des Streifens umgebogen und mit der Kantenfläche verleimt werden kann. Der Folienstreifen wird anschließend entfernt. Die Verwendung einer Folie ist besonders vorteilhaft, wenn diese selbstklebend ist.Elasticity of the strip can be bent and glued to the edge surface. The film strip is then removed. The use of a film is particularly advantageous if it is self-adhesive.
Eine weitere Ausfühnhgsart besteht darin, daß das Material so entfernt wird, daß das über den überstehenden Teil ,der Beschichtung gebildete Profil komplementär ist zu dem, das auf der gegenüberliegenden Seite der Linie, um die die Beschichtung umgelegt wird, gebildet ist, so daß nach dem Umlegen kein Hohlraum entsteht. Es ist zwar denkbar, sämtliches Material über einen Endbereich der Beschichtung zu entfernen, so daß diese allein um einen bestimmten Betrag übersteht, damit der überstehende Teil anschließend um 90° nach oben bzw. nach unten umgebogen werden kann. Es muß jedoch weitaus weniger Material durch spangebende Verformung entfernt werden, wenn zwei komplementäre Profile gebildet werden, die sich beim Umlegen des überstehenden Teils der Beschichtung ohne Zwischenraum ineinanderfügen. In diesem Zusammenhang sieht die Erfindung ferner vor, daß über dem überstehenden Teil der Beschichtung ein Vollprofil mit trapezförmigem, dreieckigem, kreisförmigem usw. Querschnitt gebildet wird und daß auf der gegenüberliegenden Seite der Linie ein entsprechend komplementäres Hohlprofil gebildet wird. Es erweist sich in jedem Fall als vorteilhaft, wenn im Bereich der Linie, um die der überstehende Teil der Beschichtung umgelegt bzw. umgebogen wird, durch die beiden Profile eineAnother embodiment is that the material is removed so that the overhanging part, the Coating profile formed is complementary to the one on the opposite side of the line around which the coating is formed is turned over, is formed, so that after turning over no cavity is formed. It is conceivable, everything Remove material over an end portion of the coating, so that this alone protrudes by a certain amount, so that the protruding part then upwards by 90 ° or can be bent downwards. However, it must be far less material will be removed by cutting deformation when two complementary profiles are formed that when the protruding part of the coating is folded over, they fit into one another without a gap. In this context the invention also provides that over the protruding part of the coating a solid profile with a trapezoidal, triangular, circular, etc. cross-section is formed and that a correspondingly complementary hollow profile is formed on the opposite side of the line. It proves in any case to be advantageous if in the area of the line around which the protruding part of the coating is folded or bent over, one through the two profiles
-. 6 109885/0151 -. 6 109885/0151
Nut entsteht, in der eine Leimraupe eingelegt werden kann.A groove is created in which a bead of glue is inserted can.
Eine andere Ausführung der Erfindung besteht darin, daß der überstehende Teil der Beschichtung eine Länge besitzt, die der Stärke des plattenförmigen ¥erkstücks entspricht. Dies ist erforderlich, wenn ein bündiger Abschluß der geradlinigen Kante des plattenförmigen Werkstücks erzielt werden soll. Bei einem Werkstück mit Doppelbeschichtung, muß die andere Beschichtung um den Betrag entfernt werden, um den die erste Beschichtung überstehen soll.Another embodiment of the invention is that the protruding part of the coating has a length which corresponds to the thickness of the plate-shaped part. This is necessary when the rectilinear edge of the plate-shaped workpiece is to be achieved. For a workpiece with double coating, the other coating must be removed by the amount that the first coating is to survive.
In einigen Fällen kann erwünscht sein, daß die Kantenbeschichtung mit einem Randbereich auf einer Oberfläche der Platte zu liegen kommt. Hiafür sieht eine- Ausführung der Erfindung vor, daß das Material so entfernt wird, daß der überstehende Teil der Beschichtung .um zwei parallel im Abstand zueinander verlaufende Linien um jeweils 90° umgelegt werden kann. Die Länge des überstehenden Teils der Beschichtung muß hierbei länger sein als die Stärke der Platte. Für plattenförmige Werkstücke mit beidseitiger Oberflächenbeschichtung wird in diesem Zusammenhang ferner vorgeschlagen, daß die Länge des überstehenden Teils einer Beschichtung so gewählt und die andere Beschichtung soweit entfernt wird, daß nach dem zweimaligen Umlegen das Ende des überstehenden Teils gegen die Kante der anderen Be-In some cases it may be desirable to have the edge coating having a border area on one surface the plate comes to rest. For this purpose, one embodiment of the invention provides that the material is removed in such a way that the protruding part of the coating .um two parallel lines at a distance of 90 ° each can be turned over. The length of the protruding part of the coating must be longer than the thickness the plate. For plate-shaped workpieces with double-sided Surface coating is also used in this context proposed that the length of the protruding part of a coating and the other coating so far removed so that after the two folds the end of the protruding part against the edge of the other
§085/015§085 / 015
schichtung stößt. Hierbei wird eine sogenannte Aufdoppelung auf einer Oberfläche des plattenförmigen Werkstücks erhalten.stratification bumps. This is a so-called doubling obtained on a surface of the plate-shaped workpiece.
Zum Verleimen der Plattenkante kann irgendein bekannter Leim verwendet werden. Bei einer "bevorzugten Ausführung der Erfindung ist ferner vorgesehen, daß als Leim Schmelzkleber oder andere schnell klebende Leime vor dem Umlegen des überstehenden Teils der Beschichtung aufgebracht werden. Besteht die Beschichtung aus thermoplastischem Werkstoff, sieht die Erfindung in diesem Zusammenhang weiterhin vor, daß zunächst Kaltleim und dann Schmelzleim aufgebracht wird. Der zuerst eingelegte iatleim hat die Aufgabe, die Wärmeausstrahlung des Schmelzklebers zu dämmen, damit "keine Deformierung der Beschichtungsfolien entsteht, die nach dem Umlegen bzw. Falten des überstehenden Teils der Beschichtung zu unsaubären Oberflächen und Faltenbildungen führt. Die weitere Aufgabe des Kaltleims ist es, nach dem Umlegen und dem Pressen für eine einwandfreie Haftung der Beschichtung zu sorgen. Der Schmelzkleber dient zur schnellen Haftung der Mittellagen aller beschichteten Platten und der zu schließenden Kante.Any known glue can be used to glue the panel edge. In a "preferred embodiment the invention is also provided that as Glue Hot melt glue or other quick-stick glue can be applied before folding down the protruding part of the coating. If the coating consists of thermoplastic material, the invention also provides in this context that first cold glue and then melt glue is applied. The iatleim inserted first has the task of radiating heat to insulate the hot melt adhesive, so that "no deformation of the coating film occurs after the Folding or folding the protruding part of the coating to create unclean surfaces and wrinkles leads. The further task of the cold glue is to ensure that it is flawless after folding and pressing Adhesion of the coating to ensure. The hot melt adhesive serves for fast adhesion of the middle layers of all coated panels and the edge to be closed.
iÖS885/0153iÖS885 / 0153
Wie bereits angedeutet, kann das erfindungsgemäße Ve:..-facrsn für alle plattenförmigen Werkstoffe mit einseitiger oder doppelseitiger Beschichtung in Yorteilhafter ■isia3 angewendet -werden», soweit sine gerade Kante vorliegt. Bei Platten alt zwei parallelen geraden Kanten läßt sich die Bearbeitung und Verlsimung der geradlinigen Kanten gleichseitig durchführen. Hierzu können an sicii bekannte Yorrichtungen Verwendung finden. Die Erfindung schlägt in diesem Zusammenhang zur Durchführung des Verfahrens vor«, daß eine Kantenzerspanvorriclrcung vorgesehen ist, mit der an der geradlinigen Kante des boschichteten Werkstücks Material so entfernt wird, daß die Beschichtung um einen gewissen Betrag übersteht, daß ferner sine naehgsschaltete Yerleimvorricntung vorgesehen ist, in der Leim in dem ausgesparten Bereich aufgetragen v/ird, unidaß eine nachgeschaltete Verformung svorrichtung vorgesehen ist, die den überstehenden Teil der Beschichtung umlegt und gegen die Kantenfläche anprdXl·. Is ist natürlich möglich, die einzelnen Verfahret! sschritte mit Hilfe von getrennten Maschinen durchzuführen. Eine Ausführungsform der Erfindung sieht jedoch vor, daß die Zerspanyorrichtung, die Verleimvorrichtung und die Verformungsvorrichtung in Laufrichtung des Werkstücks hintereinander angeordnet sind und eine gemeinsame Vorschubvorrichtung aufweisen. Mit Hilfe einer derartigen Vorrichtung kann das Werkstück mit konstanter 'As already indicated, the Ve: ..- facrsn for all plate-shaped materials with one-sided or double-sided coating in Yorteiler ■ isia3 -be used »as long as it has a straight edge. With old panels, two parallel straight edges can be used to edit and simulate the rectilinear Carry out the edges on the same side. You can do this at sicii known devices are used. The invention suggests in this connection for the implementation of the method that an edge cutting device is provided with which material is removed from the straight edge of the coated workpiece in such a way that that the coating protrudes by a certain amount, that furthermore its attached glue device is provided, in which glue is applied in the recessed area, and a subsequent deformation s device is provided, which folds over the protruding part of the coating and against the edge surface anprdXl ·. Is of course possible to the individual Move! steps with the help of separate machines perform. However, one embodiment of the invention provides that the cutting device, the gluing device and the deformation device are arranged one behind the other in the running direction of the workpiece and one Have common feed device. With the help of such a device, the workpiece can be measured with a constant '
:fi, Q f.i O i-- 1 'jl! : fi, Q fi O i-- 1 'jl!
i- -<J J %J SU j Ui- - <J J% J SU j U
verhältnismäßig hoher Geschwindigkeit nacheinander den einzelnen erforderlichen Arbeitsgängen unterworfen werden. relatively high speed one after the other be subjected to the individual required operations.
In weiterer Ausgestaltung der Erfindung ist vorgesehen, daß die Verleimvorrichtung eine Leimdüse aufweist, mit der eine Leimraupe ausgetragen werden kann. In diesm. Zusammenhang ist ferner vorgesehen, daß eine zweite Leimdüse vorgesehen ist, die in Laufrichtung vor der ersten Leimdüse angeordnet ist und mittels der eine Kaltleimraupe austragbar ist, während mittels der ersten Leimdüse eine Schmelzkleberaupe ausgetragen wird.In a further embodiment of the invention it is provided that the gluing device has a glue nozzle, with which a bead of glue can be discharged. In this Connection is also provided that a second glue nozzle is provided, which is arranged in the running direction in front of the first glue nozzle and by means of a cold glue bead can be discharged while a melt adhesive bead is discharged by means of the first glue nozzle.
Das Umlegen bzw. . Falten des überstehenden Teils der Beschichtung kann auf irgendeine geeignete Weise erfolgen. Eine bevorzugte Ausführungsform der Erfindung sieht hierzu vor, daß die Yerformvorrichtung mehrere in Laufrichtung hintereinander angeordnete zylindrische Rollen aufweist, deren Achsen nacheinander von einer gegenüber der horizontalen' schwach ansteigenden Lage zu einer annähernd senkrechten Lage übergehen. Die gedachte Verbindungslinie zwischen den Anlagepunkten der Kante des plattenförmigen Werkstücks an den zylindrischen Rollen bildet auf diese Weise eine Kurve, entlang der der überstehende Teil fortschJÄtend umgelegt und an die Kantenfläche gepreßt wird. Bei zweimaligem Umlegen, beispMsweise bei der sogenannten Aufdoppelung, müssen weitere zylindrische Rollen vorgesehenThe turning over or. Folding the protruding part of the coating can be done in any suitable manner. A preferred embodiment of the invention provides for this before that the Yerformvorrichtung several in the direction of travel has cylindrical rollers arranged one behind the other, the axes of which are consecutively of one opposite the horizontal 'slightly rising position to a more or less vertical position. The imaginary connecting line between the contact points of the edge of the plate-shaped workpiece on the cylindrical rollers forms on this Make a curve along which the protruding part progresses is folded over and pressed against the edge surface. When flipping it twice, for example with the so-called If doubled up, additional cylindrical rollers must be provided
- 10 -- 10 -
mittels der- das zweite Falten vorgenommen wird. Zwischen den beiden Gruppen von. zylindrischen Rollen ist mindestens eine weitere LeiMöüse angeordnet·by means of which the second folding is carried out. Between the two groups of. At least one additional LeiMöüse is arranged on cylindrical rollers
Anstelle von zylindrischen'Rollen kann auch eine durchgehende entsprechend ausgebildete kurvenförmige Fläche verwendet werden,Instead of cylindrical rollers, a continuous, appropriately designed, curved surface can also be used,
Zum einwandfreien Yerpressen der Leimfuge und zum Nach kalibrieren der oberen$ unteren und seitlichen Kante sieht die Srfindung schließlieh vor, daß der Verform- vorrichtung eine Preßvorrichtung nachgeordnet ist, die wechselweise horizontal und vertikal angeordnete Druck rollen aufweist, dere-n Abstand der Breite bzw· Stärke des Werkstücks entspricht«, For proper pressing of the glue joint and for recalibrating the upper, lower and lateral edge, the invention finally provides that the deforming device is followed by a pressing device which has alternating horizontal and vertical pressure rollers, the width or spacing of which Thickness of the workpiece corresponds to «,
Die Erfindung soll nachfolgend anhand von Zeichnungen näher efäutert werden»The invention is to be elucidated in more detail below with reference to drawings »
Fig. 1 zeigt eine Vorrüitung zur Durchführung des erfindungsgemäßen Verfahrens.Fig. 1 shows a preparation for carrying out the method according to the invention.
Fig· θ zeigt das Verleimen eines unelastischen Werkstoffs.Fig · θ shows the gluing of an inelastic material.
In den Figuren 2 bis 9 ist ausgelmittweise im SchnittIn Figures 2 to 9 is centered in section
z.B. Spanplatte
eine Platte 21/gezeigt, die beidseitig mit einer Folie 22 beschichtet ist, z.B. aus elastischem thermoplastischem
Kunststoff (Fig. 2 Ms 7 land 9) öder einem unelastischen
Furnier (Fig. S). Durch spangebende Yerformung ist die gezeigte Kante der Platte so bearbeitet, daß ein Teil
30 einer Folie 22 um einen bestimmten Betrag übersteht. In den Figuren 2 bis 6 und 8 miß. 9 ' entspricht die Länge
des überstehenden Teils 30 der Stärke der Platte 21 einschließlich
der Folien 22. Wie aus den Figuren zu erkennen, werefeidurch die spangebende Kantenverformung komplementäre
Profile gebildet, die sich beim Umlegen des über-e.g. chipboard
a plate 21 / shown, which is coated on both sides with a film 22, for example made of elastic thermoplastic material (Fig. 2 Ms 7 land 9) or an inelastic veneer (Fig. S). The edge of the plate shown is machined by machining so that a part 30 of a film 22 protrudes by a certain amount. Measure in Figures 2 to 6 and 8. 9 ', the length of the protruding part 30 corresponds to the thickness of the plate 21 including the foils 22. As can be seen from the figures, complementary profiles were formed by the cutting edge deformation, which are formed when the over-
stehenden Teils 30 der Folie 22 enganliegend ineinanderfügen. Zu diesem Zweck wird Material über dem überstehenden Teil 30 belassen zur Bildung eines Vollprofils. Dieses hat in Fig. 2 im Schnitt die Form eines flachen Trapezes, in den Figuren 3, 8 und 9 die Form eines auf seiner Grundseite aufliegenden gleichschenkligen Dre'iecks, in den Figuren 4 und 5 ebenfalls die Form eines Dreiecks und in Fig. 6 die Form eines Kreisabschnitts. Entsprechend diesen Profilen besitzt die Platte 21 eine entsprechend ausgebildete komplementäre Ausnehmung. Die freie Kante des überstehenden Teils'30 der unteren Folie 22 schließt beim Falten um 90° nach oben bündig mit der zugekehrten Kante der oberen Folie bei 28 ab. Das Falten erfolgt dabei um eine in der Ebene der Folie 22 liegendestanding part 30 of the film 22 tightly together. For this purpose, material is placed over the protruding Leave part 30 to form a full profile. This has the shape of a flat in section in FIG. 2 Trapezoid, in Figures 3, 8 and 9 the shape of an isosceles triangle resting on its base, in FIGS. 4 and 5 likewise the shape of a triangle and in FIG. 6 the shape of a segment of a circle. In accordance with these profiles, the plate 21 has a correspondingly designed complementary recess. the free edge of the protruding part'30 of the lower film When folded by 90 ° upwards, 22 closes flush with the facing edge of the upper film at 28. The folding takes place around one lying in the plane of the film 22
- 12 -- 12 -
103885/0153103885/0153
Linie, die mit 23 angedeutet ist. Die Spitze des gleichschenkligen Dreiecks bei den Vollprofilen 27 der.Figuren 3, 8 und 9 ist bei 31 etwas abgeflacht.Line indicated by 23. The top of the isosceles The triangle in the solid profiles 27 der.Figuren 3, 8 and 9 is somewhat flattened at 31.
In Fig. 7 ist eine etwas abgewandelte Ausführung gezeigt, bei der die Länge eines überstehenden Teils 32 der unterBtn Folie 22 langer ist als die Stärke der Platte 21 einschließlich der Folien 22. Die hier gebildeten Profile sind so geformt, daß sie sich nach zweimaligem umlegen um die Linie 23 und eine parallel im Abstand dazu verlaufende Linie 29 wiederum ineinanderfügen, ohne einen wesentlichen Hohlraum zu belassen« Der in Fig. 7 rechts neben der Linie 23 liegende Abschnitt des Überstehenisn Teils 32 der Folie 22 kommt dabei in der Ebene der oberen Folie 22 zu liegen, wobei dann die freien Kanten aneinanderstoßen. Dadurch wird eine sogenannte Aufdoppelung erhalten.In Fig. 7 a somewhat modified embodiment is shown, in which the length of a protruding part 32 of the lower part Foil 22 is longer than the thickness of the plate 21 including the foils 22. The profiles formed here are shaped so that that after they fold twice around the line 23 and a line 29 running parallel at a distance from it again fit into one another without leaving a substantial cavity. The one located to the right of line 23 in FIG Section of the protruding part 32 of the film 22 comes while lying in the plane of the upper film 22, with then the free edges butt against each other. A so-called doubling is obtained in this way.
In Fig» 8 sollen die Folien 22 aus einem nichtjßlasti sehen Furnier bestehen. Es ist daher nicht möglich, den überstehenden Teil 30 um 90° herumzulegen, ohne daß dn Reißen oder ähnliche Erscheinungen im Bereich der Linie 23 auftreten. Deshalb ist zuvor ein selbstklefcender Folienstreifen 24 in diesem Bereich unterklebt. Bei der anschließenden Zerspanung wird auch die untere Folie 22 an der Linie 23 durchtrennt. Die elastische Folie 24 ermöglicht nun ein Falten oder umlegen des überstehenden Teils 30 mit dem Vollprofil 27 zur Beschichtung der in Fig. 8 rechten Kante. Wie manIn Fig. 8 the foils 22 are intended to be seen from a non-elastic Made of veneer. It is therefore not possible to remove the protruding Part 30 to turn around 90 ° without tearing or similar phenomena occur in the area of line 23. Therefore, a self-adhesive film strip 24 is required beforehand glued under in this area. During the subsequent machining, the lower film 22 is also severed at the line 23. The elastic film 24 now enables the protruding part 30 with the full profile to be folded or folded over 27 for coating the right edge in FIG. 8. How one
aus den übrigen Figuren erkennt, erfolgt die Zerspanung bis auf die Oberseite der unteran Folie. Natürlich besteht auch die Möglichkeit, die untere Folie im Bereich der Linie 23 teilweise anzuschneiden, um ein Falten bzw. Umbiegen oder Umlegen zu erleichtern.recognizes from the other figures, the machining takes place except for the upper side of the film below. Of course there is also the possibility of partially cutting the lower film in the area of the line 23 in order to fold or bend or To make relocating easier.
Wie aus den Figuren 2 bis 9 ferner zu erkennen, wird die spanabgebende Verformung der Kante der Platte so vorgenommen, daß über der Umbiegelinie 23 bzw. 29 eine nach oben hin offene Nut gebildet ist. In diese Nut wird, wie aus Fig. 9 zu erkennen, der Leim in Form einer Raupe eingebracht. In Fig. 9 sind zwei übereinander liegende ^eimraupen 25 und 26 zu erkennen, wobei die untere Leimraupe 25 aus Kaltleim und die darüber liegende aus Schmelzkleber besteht. Der zuerst in die Faltnut eingelegte-Kaltleim hat die Aufgabe, bei thermoplastischen Folien die Wärmeausstrahlung des Schmelzklebers 26 zu dämmen, damit keine Deformierung der Folien 22 entsteht, was nach dem Faltvorgang zu unsauberen Oberflächen und Faltenbildungen führt. Die weitere Aufgabe des Kaltleims besteht darin, nach dem FaIt- und Preßvorgang für eine einwandfreie Haftung der Folien 22 zu sorgen. Der Schmelzkleber 26 dient zur schnellen Haftung der Mittellagen aller beschichteten Platten.As can also be seen from FIGS. 2 to 9, the metal-removing deformation of the edge of the plate is carried out in such a way that that an upwardly open groove is formed above the bending line 23 or 29. In this groove, as can be seen from Fig. 9, the glue introduced in the form of a bead. In Fig. 9 two superimposed ^ egg caterpillars 25 and 26 can be seen, wherein the lower bead of glue 25 consists of cold glue and the one above it consists of hot-melt adhesive. The cold glue first inserted into the folding groove has the task of dampening the heat radiation of the hot melt adhesive 26 in the case of thermoplastic films, so that none Deformation of the foils 22 occurs, which leads to unclean surfaces and wrinkles after the folding process. The other The task of the cold glue is to ensure proper adhesion of the foils 22 after the folding and pressing process. The hot-melt adhesive 26 is used for rapid adhesion of the middle layers of all coated panels.
Die in Fig. 1 dargestellte Vorrichtung setzt sich aus einem Zerspanabschnitt 40, zwei Verleimabschnitten 41, 43, zwei Ver-The device shown in Fig. 1 consists of a cutting section 40, two gluing sections 41, 43, two
- 14 -- 14 -
formabschnitten 42, 44 und einem Preß- und Kalibrierabschnitt 45 zusammen« Die Abschnitte 40 bis 45 sind auf einem Fundament 46 angeordnet. Die einzelnen Abschnitte 40 bis 45, die in Laufrichtung eines nicht gezeigten Werkstücks hintereinander angeordnet sind, sind über eine Transportkette 47 miteinander verbunden. Die Oberkante der Kettenebene ist mit dem Bezugsseichen 1 angedeutet. Die Kette 47 wird an den beiden Enden über Kettenräder 48, 49 umgelenkt« Oberhalb des oberen Trumms der Kette 47 sind Oberdrucke 2 in Form von umlaufenden Keilriemen vorgesehen, die in der unteren waagerechten Vorshubrichtung federnd geführt sind. Sie sorgen für eine einwandfreie Einspannung der Werkstücke während der Bearbeitung. Die Keilriemen 2 sind an den Enden über Rollen50, 51 umgelenkt. Eines der Räder 48 und mindestens eine der Rollen 50, 51 können mit Hilfe geeigneter Antriebsvorrichtung angetrieben sein.mold sections 42, 44 and a pressing and sizing section 45 together «The sections 40 to 45 are arranged on a foundation 46. The individual sections 40 to 45, which are arranged one behind the other in the running direction of a workpiece, not shown, are via a Transport chain 47 connected to one another. The upper edge of the chain plane is indicated by reference sign 1. The chain 47 is deflected at both ends via chain wheels 48, 49 above the upper run of the chain 47 overprints 2 are provided in the form of revolving V-belts, which in the lower horizontal Vorshubrichtung are resiliently guided. They ensure that the workpieces are properly clamped during processing. The V-belts 2 are deflected at the ends via rollers 50, 51. One of the wheels 48 and at least one of the rollers 50, 51 can with the aid of a suitable drive device be driven.
Bei der Vorrichtung nach Fig. 1 sind nur die Teile zur Bearbeitung einer geradlinigen Kante eines Werkstücks dargestellt. Die zur gleichzeitigen Bearbeitung der gegenüberliegenden Kante erforderlichen Teile sind in dieser Ansicht nicht zu sehen. Der Zerspanabschnitt 40 weist eine erste Arbeitswelle 3 auf, die durch Sägen und Zerspanen die Werkstücke auf das eingestellte Breitenmaß besäumt. Mit Hilfe von in Laufrichtung nachgeordneten Arbeits-In the device of FIG. 1, only the parts for machining a straight edge of a workpiece shown. The parts required to machine the opposite edge at the same time are in this one View not to be seen. The cutting section 40 has a first working shaft 3, which is cut by sawing and cutting the workpieces are trimmed to the set width. With the help of downstream working
- 15 309885/0153 - 15 309885/0153
wellen 4, 5 und 6 werden Profile hergestellt, wie sie in den Figuren 2 bis 7 dargestellt sind. Je nacla dem geforderten Profil können auch, "weitere Arbeitsstellen vorgesehen sein. Die Arbeitswellen 3 Us 6 sind mit Hilfe nicht bezeichneter "iorrichteigen nach Höhe und Seite verstellbar. In den einseinen Zerspanungsbereichen des Zerspanungsabschnitts 40 sind Braekrollen 7 und Gleittische 9 vorgesehen, die die Werkstücke auf darunter angeordnete Stützrollen 8 drücken« Am Einlaufende der Vorrichtung befindet sich eine Schalttafel 52, die über einen Ausleger 53 an· einem festen Teil der Vorrichtung angebracht ist. .shafts 4, 5 and 6, profiles are produced as shown in FIGS. 2 to 7. Je nacla dem Required profile can also, "other jobs be provided. The working shafts 3 Us 6 are with the help unmarked "iorrichteigen according to height and side adjustable. In the one-of-a-kind machining areas of the Zerspanungsabschnitts 40 are brake rollers 7 and slide tables 9 provided, which press the workpieces onto support rollers 8 arranged underneath Device is a control panel 52, which over a boom 53 on a fixed part of the device is appropriate. .
In Laufrichtung hinter der letzten Arbeitswelle 6 befindet sich eine sogenannte Luftschleuse 10 mit eingebauter rotierender Bürste 54. Die Aufgabe dieser Luftschleuse 10 besteht darin, die Profilquerschnitte von Zerspanungsresten zu reinigen. Der Luftschleuse 10 ist eine erste Leimdüse 11 nachgeordneir, mittels der eine Kaltleimraupe 25 in die im Bereich der Linie 23 vorgesehene Nut eingelegt wird (Fig. 9). Dahinter ist eine weitere Leimdüse 12 angeordnet, mittels der die Schmelzleimraupe 26 eingelegt wird. Beide Leimdüsen 11, 12 sind sowohl hinsichtlich ihres Ortes als auch im Hinblick auf die Abgabemenge steuerbar.In the running direction behind the last working shaft 6 there is a so-called air lock 10 with a built-in one rotating brush 54. The job of this airlock 10 consists in cleaning the profile cross-sections of machining residues. The airlock 10 is a first glue nozzle 11 nachgeordneir, by means of which one Cold glue bead 25 into the one provided in the area of line 23 Groove is inserted (Fig. 9). A further glue nozzle 12 is arranged behind it, by means of which the melt glue bead 26 is inserted. Both glue nozzles 11, 12 are both in terms of their location and in terms of the delivery amount controllable.
- 16 -- 16 -
ÖftfölNAL 1NSPICH&ÖftfölNAL 1NSPICH &
Der Ve rf ο rmat» schnitt 42 hat die Aufgabe, den überstehenden Teil 30 der Beschichtungsfolie um die Linie 23 umzulegen und das Vollprofil 27 in das Hohlprofil einzufügen. Hierzu sind zylindrische Rollen 16 vorgesehen, die auf einem senkrecht zur.Vorschubrichtung verstellbaren Schlitten 15 angeordnet sind. Mit Hilfe dieser Rollen 16, deren Achse von einer etwas schräg zur Horizontalen geneigten Lage (in Laufrichtung erste Rolle) sich bis zu einer vertikalen Lage (in Laufrichtung letzte Rolle) ändert, wird der überstehende Teil 30 allmählich von der waagerechten in&ie senkrechte Lage umgelegt. Die Rollen 16 sorgen außerdem dafür, daß eine angemessene Pressung der Profile erzeugt wird.The task of verf ο rmat »section 42 is to remove the protruding Part 30 of the coating film to fold over the line 23 and insert the solid profile 27 into the hollow profile. For this purpose, cylindrical rollers 16 are provided, which are mounted on a slide that can be adjusted perpendicular to the direction of advance 15 are arranged. With the help of these rollers 16, the axis of which is inclined slightly obliquely to the horizontal Position (in the direction of travel first roll) changes up to a vertical position (in direction of travel last roll), the protruding part 30 is gradually turned over from the horizontal to the vertical position. The roles 16 provide also that an adequate compression of the profiles is generated.
Die in Fig. 1 gezeigte Vorrichtung ist in der Lage, ein Profil herzustellen und zu verarbeiten, wie es in Fig.7 wiedergegeben ist. Daher nehmen die Rollen 16 die erste Faltung vor. Anschließend erfolgt mit Hilfe von zwei weiteren Leimdüsen 19 ein erneuter Leimauftrag entlang der Linie 29 in Fig. 7. Die Leimdüsen 19 sind ebenfalls in gleicher Weise Me die Leimdüsen 11, 12 steuerbar und bestehen ebenfalls aus einer Kaltleim- und einer Schmelzkleberdüse. Daran schließt sich ein weitere*· Verformungsabschnitt 44 an, der ebenfalls zylindrische Rollen 20 aufweist, die genauso wie im Verformungsabschnitt 42 auf einen senkrecht zur Vorschubrichtung verstellbaren Schlitten angeordnet sind. Im Verformungsabschnitt 44 haben dieThe device shown in Fig. 1 is able to a Produce and process profile, as shown in Fig.7. Therefore, the rollers 16 take the first Folding before. Then, with the help of two further glue nozzles 19, another application of glue takes place along the Line 29 in FIG. 7. The glue nozzles 19 are also controllable and exist in the same way Me the glue nozzles 11, 12 also from a cold glue and a hot melt glue nozzle. This is followed by a further * · deformation section 44, which also has cylindrical rollers 20, which just as in the deformation section 42 a slide which can be adjusted perpendicular to the feed direction is arranged. In the deformation section 44 have the
- 17 £09885/015-3 - £ 17 09885 / 015-3
Rollen 20 jedoch einen größeren Abstand voneinander als die Rollen 16 im Verformungsabschnitt 42. Der größere Rollenabstand ist durch das jetzt steifere Profil erforderlich, damit auch hier über den Bereich der elastischen Verformung eine Kurve erzielt wird, mit der die gewünschte Faltung vorgenommen werden kann.However, rollers 20 a greater distance from each other than the rollers 16 in the deformation section 42. Der larger roller spacing is required due to the now stiffer profile, so here too over the area the elastic deformation a curve is obtained with which the desired folding can be made can.
Im anschließenden Kalibrier- und Preßabschnitt sind in gleichen Abständen Druckrollenpaare 18 vorgesehen, die auf einem senkrecht zur Vorschubrichtung bewegbaren Schlitten 17 angeordnet sind. Die Achsen der Druckrollenpaare 18 verlaufen abwechselnd horizontal und vertikal und dienen zur einwandfreien Verpressung der Leimfuge und zum Nachkalibrieren der oberen, unteren und seitlichen Kante.In the subsequent calibration and pressing section, pressure roller pairs 18 are provided at equal intervals, which are arranged on a slide 17 movable perpendicular to the feed direction. The axes of the pressure roller pairs 18 run alternately horizontally and vertically and are used for perfect pressing the glue line and for recalibrating the top, bottom and side edges.
- 18 -- 18 -
309385/01^3309385/01 ^ 3
Claims (17)