CN2442619Y - High-strength composite bottom non-sticking lining pot - Google Patents
High-strength composite bottom non-sticking lining pot Download PDFInfo
- Publication number
- CN2442619Y CN2442619Y CN 00249695 CN00249695U CN2442619Y CN 2442619 Y CN2442619 Y CN 2442619Y CN 00249695 CN00249695 CN 00249695 CN 00249695 U CN00249695 U CN 00249695U CN 2442619 Y CN2442619 Y CN 2442619Y
- Authority
- CN
- China
- Prior art keywords
- layer
- stainless steel
- stick
- pan
- utility
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model relates to an improvement on a non-stick pan. If the surface of the existing product does not stick with coating or the high temperature lacquer is damaged, aluminium ions are easy to be separated out; an iron face is easy to expose and leak caused by acid etching or abrasion. The concave surface of the iron pan body is made into a roughened surface and is coated with a stainless steel thin layer and non-stick coating in sequence. The stainless steel layer is tightly stuck. The pan bottom is sprayed with a high enamel layer and is difficult to damage. The utility model is good for human body health and has long service life.
Description
The utility model relates to cooker, particularly the improvement of non-stick pan.
Existing commercially available various non-stick pans, the concave surface of its metal pan body applies one deck poly tetrafluoroethylene, convex surface sprays one deck high temperature lacquer, have advantages such as high temperature resistant, sticking juice, but its hardness is low, concave surface is scraped by the meal shovel easily, convex surface makes aluminium or iron pan body directly exposed easily by the kitchen range scratch, can cause aluminium ion to be separated out and enter human body, and be corroded easily or wear and tear, the time has been grown and can make a pot body leakage.
Aluminium or iron-based material that the purpose of this utility model provides pot body are difficult for the directly novel non-stick pan of exposure, in order to health, and increase the service life.
Metal pan body concave surface of the present utility model is coated with high temperature non-viscous paint layer, it is characterized in that the concave surface of pot body is made matsurface, sprays the stainless steel thin layer between itself and the high temperature non-viscous paint layer; Convex surface has sprayed high glaze enamel layer.
The thickness of above-mentioned stainless steel thin layer is 0.1~0.3mm.
Above-mentioned high temperature non-viscous paint layer can be formed by the multilayer spraying.
Above-mentioned enamel layer can be formed by bilayer, and its ectomesoderm is mixed with mica powder.
Advantage of the present utility model: stainless steel material hardness height, corrosion-resistant, meet food hygiene, on its metal pan face that has been sprayed on roughening, because tessellation, make it combine very firm with the pot face, having solved stainless steel is difficult for and the very tight close problem that combines, even surperficial non-viscous paint is scratched, also can not cause the erosion leakage or the aluminium ion of pot body to select, and cost reduce; Enamel surface hardness height, high temperature resistant, be difficult for scratching, and realize that easily colourful pattern beautifies.
In the accompanying drawing, Fig. 1 has represented structure of the present utility model, and Fig. 2 is the partial enlarged drawing of Fig. 1.
With reference to Fig. 2, the concave surface of pot body 3 is made matsurface with the sandblast mode, sprays the stainless steel layer 2 of thick about 0.2mm on it, sprays 2~3 floor height temperature non-viscous paint layers 1 more thereon, such as teflon coating or the senior non-viscous paint of commercially available CCC; The convex surface of pot body 3 spray common enamel layer 4 ', apply thereon again and be mixed with the high glaze enamel layer 4 of mica powder, thereby the fragility of enamel is reduced, impact resistance and peeling resistance improve.
Claims (3)
1, non-stick pan of the compound end of a kind of high strength, the concave surface of metal pan body (3) is coated with high temperature non-viscous paint layer (1), the concave surface that it is characterized in that a pot body (3) is made matsurface, sprays stainless steel thin layer (2) between itself and the non-viscous paint layer (1), and convex surface has sprayed high glaze enamel layer (4).
2, non-stick pan according to claim 1, the thickness that it is characterized in that stainless steel thin layer (2) is 0.1~0.3mm.
3, non-stick pan according to claim 1 and 2 is characterized in that enamel layer can be formed by bilayer, and its ectomesoderm (4) is mixed with mica powder.