CN212097866U - Plastic uptake moulded board and furniture - Google Patents
Plastic uptake moulded board and furniture Download PDFInfo
- Publication number
- CN212097866U CN212097866U CN201922101386.6U CN201922101386U CN212097866U CN 212097866 U CN212097866 U CN 212097866U CN 201922101386 U CN201922101386 U CN 201922101386U CN 212097866 U CN212097866 U CN 212097866U
- Authority
- CN
- China
- Prior art keywords
- base plate
- plastic uptake
- edge sealing
- panel
- substrate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model provides a plastic uptake mould pressing panel and furniture has solved current panel because the intermediate substrate after the cutting material is loose, and the artifical unable level and smooth and lead to the panel side after highlight PVC membrane plastic uptake to have the problem of phenomenon such as serious wrinkling, orange peel, wherein, plastic uptake mould pressing panel include the base plate and adhere to through the plastic uptake technology the highlight PVC membrane on substrate surface, the side all around of base plate with be equipped with between the highlight PVC membrane attach to be in seal strake on the base plate, seal the strake and be dorsad the side of base plate is set up to smooth plane. The plastic uptake mould pressing panel seals the side all around of base plate through the banding strip before carrying out the plastic uptake to ensure the roughness of base plate side all around, save the man-hour of artifical polishing, and make phenomenons such as wrinkling, the orange peel of panel sample side behind highlight PVC membrane plastic uptake improve, be favorable to mass production.
Description
Technical Field
The utility model relates to a furniture board field especially relates to a plastic uptake mould pressing panel and furniture.
Background
In the current furniture on the market, for the decoration beauty and durability, diversified veneers are often arranged on the surface of the furniture board, such as decorative films, melamine paper or paint. In addition, a plastic suction molding plate is also available in the market, and the plastic suction molding plate is a name of combining materials and processes, wherein suction refers to a vacuum suction process, molding refers to a PVC film on a surface layer, mold refers to a plate before the PVC film is not pressed after a cutter is milled, pressing refers to a pressing process during the forming of the PVC film, and is simply called as the plastic suction molding plate.
However, after the periphery of the existing substrate is cut, the middle substrate is loose, and the manual polishing cannot be smooth, so that the side edge of a sample subjected to the plastic suction of the highlight PVC film has serious phenomena of wrinkling, orange peel and the like, and meanwhile, the manual waste is caused, and the processing efficiency is low.
SUMMERY OF THE UTILITY MODEL
The main purpose of the utility model is to provide a plastic uptake mould pressing panel that side roughness is high, machining efficiency is high.
Another object of the utility model is to provide a furniture including above-mentioned plastic uptake moulded board.
In order to achieve the above object, the present invention provides the following technical solutions:
as a first aspect, the utility model relates to a plastic uptake mould pressing panel, including the base plate and through the plastic uptake technology adhere to in the highlight PVC membrane on base plate surface, the side all around of base plate with be equipped with between the highlight PVC membrane attach to the banding strip on the base plate, the banding strip is dorsad the side of base plate is set up to smooth plane.
Further setting: the thickness of the edge sealing strip is 4-6mm, and the width of the edge sealing strip is equal to the thickness of the substrate.
Further setting: the end parts of the edge sealing strips are obliquely arranged and are spliced with the end parts of the adjacent edge sealing strips to form a right angle.
Further setting: and the outer side edges of the end part connecting parts of two adjacent edge sealing strips are rounded.
Further setting: the edge sealing strip is positioned on the side far away from the base plate and is arranged along the side edge of the length direction in a rounded manner.
Further setting: the radius of the fillet is 2 mm.
Further setting: the edge banding is made of density boards.
As a second aspect, the present invention relates to a piece of furniture comprising a blister moulded board as described above.
Compared with the prior art, the utility model discloses a scheme has following advantage:
the utility model discloses a plastic uptake mould pressing panel is before carrying out the plastic uptake, carry out the banding through the banding strip to the side all around of base plate, solved panel after the cutting material, the middle part is comparatively loose and lead to polishing can't be to smooth problem, the roughness of base plate side all around has not only been guaranteed, make wrinkling, phenomenon such as orange peel of panel side obtain improving after highlight PVC membrane plastic uptake, and need not to polish to the side of base plate, the man-hour of artifical polishing has been saved, the production efficiency is improved, be favorable to mass production.
Additional aspects and advantages of the invention will be set forth in part in the description which follows and, in part, will be obvious from the description, or may be learned by practice of the invention.
Drawings
The above and/or additional aspects and advantages of the present invention will become apparent and readily appreciated from the following description of the embodiments, taken in conjunction with the accompanying drawings of which:
fig. 1 is a schematic structural view of an embodiment of the plastic-absorbing molded plate of the present invention;
fig. 2 is a schematic view of the split structure of the base plate and the edge strip of the plastic molded plate of the present invention.
In the figure, 1, a substrate; 2. an edge banding; 3. high gloss PVC films.
Detailed Description
Reference will now be made in detail to embodiments of the present invention, examples of which are illustrated in the accompanying drawings, wherein like reference numerals refer to the same or similar elements or elements having the same or similar function throughout. The embodiments described below by referring to the drawings are exemplary only for explaining the present invention, and should not be construed as limiting the present invention.
Referring to fig. 1 and 2, the present invention discloses a plastic molded board, which has a side edge with good flatness and high processing efficiency, and can be used as a door panel or applied to various cabinet-type furniture such as a wardrobe, a locker, a vestibule cabinet, a shoe cabinet, etc., in order to solve the problems that after the existing board is cut and cut, the middle part is loose and cannot be flattened by manual polishing, so that the side edge of the existing board is seriously wrinkled and orange peel after the high-gloss PVC film plastic molding.
The plastic suction molding plate comprises a substrate 1 and a highlight PVC film 3 coated on the surface of the substrate 1, wherein the highlight PVC film 3 is formed on the surface of the substrate 1 through a plastic suction process, and the plastic suction process is that after flat highlight PVC materials are heated and transformed, the flat highlight PVC materials are adsorbed on the surface of the substrate 1 in a vacuum mode and are formed after cooling.
The highlight PVC film 3 has the functions of easy cleaning, light weight and non-flammability, and the highlight PVC film 3 has good glossiness, so that the surface of the plate subjected to the plastic suction molding of the highlight PVC film 3 has good glossiness, and is easy to clean, light in weight and non-flammability.
Before the highlight PVC film 3 is carried out on the base plate 1, the side edges of the periphery of the base plate 1 after cutting can be sealed. Specifically, be equipped with all around of base plate 1 and cover in the banding strip 2 of its side completely, banding strip 2 with base plate 1 is colded pressing with the bonding through piecing together gluey and is fixed, banding strip 2 keep away from with the side that base plate 1 bonded sets up to smooth plane for base plate 1 after carrying out the banding processing is carrying out the plastic uptake back, and its side orange peel phenomenon is improved, is guaranteeing simultaneously under the circumstances of the roughness of base plate 1 side, has saved the step of artifical polishing again, has saved man-hour, has improved work efficiency.
Please combine fig. 2, the utility model provides a length of banding 2 and its side length phase-match that corresponds base plate 1 of being connected, the thickness of banding 2 with the thickness of base plate 1 equals, the thickness scope of banding is at 4-6mm, and the thickness of banding 2 is preferred 5mm in this embodiment, and the banding 2 of this thickness is thinner, can avoid the size increase of base plate 1 behind the banding too much, and banding 2 after 5mm has certain compressive strength simultaneously to avoid banding 2 to receive extrusion, collision etc. in the course of working and lead to the rupture of banding 2, thereby ensure the structural stability and the maneuverability of banding 2. The edge banding 2 in the embodiment is made of a density board, the density board is a board which is made of wood fibers or other plant fibers through the steps of preparing fibers, applying synthetic resin, pressing under the condition of heating and pressurizing, and can be divided into a high-density fiberboard, a medium-density fiberboard and a low-density fiberboard according to the density, the density board is uniform in structure, fine and dense in material, stable in performance, impact-resistant and easy to process, the edge banding 2 made of the density board is flat in surface and low in cost.
In addition, the end of each edge sealing strip 2 along the length direction is obliquely arranged, and the end of each two adjacent edge sealing strips 2 can be spliced to form a right angle matched with the corner end of the substrate 1, so that the gap between each edge sealing strip 2 and the side edge of the substrate 1 is reduced, and the generation of an orange peel phenomenon caused by the gap in the plastic suction process is avoided. In other embodiments, one end of each edge sealing strip 2 is provided with a mortise, and the other end of each edge sealing strip is provided with a tenon matched and clamped with the mortise at the end of the adjacent edge sealing strip 2, so that the installation and connection of the two adjacent edge sealing strips 2 can be realized.
Further, please combine fig. 1, the outside edge radius angle of the end connection of two adjacent edge sealing strips 2 is set, the edge sealing strip 2 is far away from two edges of the side surface of the substrate 1, the side edge extending along the length direction of the edge sealing strip 2 is also set in a radius angle manner, and the radius angles of the outside edge of the connection part and the two side edges along the length direction of the edge sealing strip 2 are 2mm, the edge sealing strip 2 has a slight radius angle, the edge angle of the plate can be reduced, so that the plastic uptake is facilitated, and the phenomena of wrinkling and orange peel existing after the plastic uptake due to the existence of the edge angle can be reduced.
The utility model discloses a plastic uptake mould pressing panel is right before carrying out the plastic uptake the side all around of base plate 1 carries out the banding, has solved base plate 1 and after cutting out the material, and the middle part is loose and lead to the artifical smooth problem of polishing, has not only ensured the roughness of base plate 1 side all around has improved the phenomenon such as wrinkling, orange peel of panel sample side after 3 plastic uptake of highlight PVC membrane, has then ensured the roughness of plastic uptake mould pressing panel side need not right moreover the side of base plate 1 is polished, and passes through after 2 sealed limits of edge banding strip, only need gently fall the water caltrop limit again can, the side periphery that need not polish again, has saved the man-hour of artifical polishing, has improved production efficiency, is favorable to mass production.
The utility model discloses still relate to a furniture, it includes as above plastics sucking moulding panel, make and adopt the surface smoothness of the furniture that plastics sucking moulding panel made is high to need not the workman and polish the furniture panel side, saved man-hour, improved work efficiency.
The foregoing is only a partial embodiment of the present invention, and it should be noted that, for those skilled in the art, a plurality of modifications and decorations can be made without departing from the principle of the present invention, and these modifications and decorations should also be regarded as the protection scope of the present invention.
Claims (8)
1. The utility model provides a plastic uptake moulded board, characterized by: the high-gloss PVC film is attached to the surface of the substrate through a plastic suction process, edge sealing strips attached to the substrate are arranged between the peripheral side edges of the substrate and the high-gloss PVC film, and the side faces, back to the substrate, of the edge sealing strips are set to be smooth planes.
2. The blister molded panel of claim 1, wherein: the thickness of the edge sealing strip is 4-6mm, and the width of the edge sealing strip is equal to the thickness of the substrate.
3. The blister molded panel of claim 1, wherein: the end parts of the edge sealing strips are obliquely arranged and are spliced with the end parts of the adjacent edge sealing strips to form a right angle.
4. The blister molded panel of claim 1, wherein: and the outer side edges of the end part connecting parts of two adjacent edge sealing strips are rounded.
5. The blister molded panel of claim 1, wherein: the edge sealing strip is positioned on the side far away from the base plate and is arranged along the side edge of the length direction in a rounded manner.
6. The blister molded board of claim 4 or 5, wherein: the radius of the fillet is 2 mm.
7. The blister molded panel of claim 1, wherein: the edge banding is made of density boards.
8. A piece of furniture is characterized in that: comprising the blister-molded board according to any one of claims 1 to 7.