CN103849323A - Grinding wheel and plate tire bonding method - Google Patents
Grinding wheel and plate tire bonding method Download PDFInfo
- Publication number
- CN103849323A CN103849323A CN201210556689.7A CN201210556689A CN103849323A CN 103849323 A CN103849323 A CN 103849323A CN 201210556689 A CN201210556689 A CN 201210556689A CN 103849323 A CN103849323 A CN 103849323A
- Authority
- CN
- China
- Prior art keywords
- bonding
- grinding wheel
- plate
- emery wheel
- prior
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a grinding wheel and plate tire bonding method which solves the shortcomings of the background technology that although lots of bonding methods exist in the prior art for shoe bonding, glass bonding and the like, a grinding wheel and plate tire bonding method is unavailable in the prior art. The method is characterized by comprising the following steps: uniformly mixing epoxy resin and dibutyl ester, adding ethidene diamine and stirring uniformly (the three substances are stirred uniformly for sure); pouring the mixture onto the cleaned grinding wheel plate and smearing uniformly, and putting a grinding wheel to be bonded (the bonding surface of the grinding wheel is clean without dust, water or impurity) onto the grinding wheel plate, centering and aligning; pressing the grinding wheel with a 100kg weight; if adhesive is squeezed out around, immediately smearing cement. Compared with the prior art, the method disclosed by the invention has the advantages of simple process, convenient use and short bonding time of generally 2-3 days. The bonding is firm and durable. The method disclosed by the invention is used for bonding a grinding wheel and a plate tire.
Description
Technical field
The present invention is a kind of adhering method, particularly the adhering method of a kind of emery wheel and plate tire.
Background technology
Adhering method of the prior art is a lot, as sticky footwear, sticky glass etc., but there is no in the adhering method prior art of emery wheel of the present invention and plate tire.
Summary of the invention
In order to fill up above-mentioned blank part of the prior art, the object of this invention is to provide the adhering method of a kind of emery wheel and plate tire.Technical solution of the present invention is: after first epoxy resin being mixed with dibutylester, add quadrol again stirring, be then poured on after smearing evenly on the emery wheel plate of having cleaned out and put and treat bonding emery wheel, centering, centering; On emery wheel, press weight; If periphery has caking agent to be extruded, should spread with cement immediately.
The advantage that the present invention had is compared to existing technology: technique is simple, easy to use, and the bonding time is short, within general 2 to 3 days, can use.Bonding is firm, durable.
Embodiment
The present invention is described in further detail below in conjunction with embodiment: after first epoxy resin being mixed with dibutylester, add quadrol and again stir (three kinds of mixtures must stir), then be poured on to put after smearing evenly on the emery wheel plate of having cleaned out and treat bonding emery wheel (bonding plane of emery wheel must be clean, must dustless, anhydrous, inclusion-free) centering, centering; On emery wheel, press the weight of double centner; If periphery has caking agent to be extruded, should spread with cement immediately.
The present invention is for bonding between emery wheel and plate tire.
Claims (1)
1. an adhering method for emery wheel and plate tire, is characterized in that: after first epoxy resin being mixed with dibutylester, add quadrol again stirring, be then poured on after smearing evenly on the emery wheel plate of having cleaned out and put and treat bonding emery wheel, centering, centering; On emery wheel, press weight; If periphery has caking agent to be extruded, should spread with cement immediately.The present invention is for bonding between emery wheel and plate tire.