[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

CN103571388A - 一种耐高温热熔胶 - Google Patents

一种耐高温热熔胶 Download PDF

Info

Publication number
CN103571388A
CN103571388A CN201310505609.XA CN201310505609A CN103571388A CN 103571388 A CN103571388 A CN 103571388A CN 201310505609 A CN201310505609 A CN 201310505609A CN 103571388 A CN103571388 A CN 103571388A
Authority
CN
China
Prior art keywords
parts
melt adhesive
resistant hot
temperature
resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310505609.XA
Other languages
English (en)
Inventor
项孝泓
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhu Zhongli Parts Co Ltd
Original Assignee
Wuhu Zhongli Parts Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhu Zhongli Parts Co Ltd filed Critical Wuhu Zhongli Parts Co Ltd
Priority to CN201310505609.XA priority Critical patent/CN103571388A/zh
Publication of CN103571388A publication Critical patent/CN103571388A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种耐高温热熔胶,其是由下述重量份的原料制得:顺丁烯二酸酐1-2、聚氨酯树脂2-4,丙烯酸树脂3-6、EEA8-10,EVA 38-58,乙烯基三甲氧基硅烷0.3-0.5、交联剂TAC1-2,C9石油树脂15-20,石蜡3-5、甲基丙烯酸锌0.2-0.4、松香138树脂9-12,当归油0.2-0.3,复合纳米填料1-2;本发明配料合理,各原料相容性好,各项性能优异,特别适用于汽车内饰件表面复合机织面料,长期使用耐高温效果好,不会起泡,寿命长。

Description

一种耐高温热熔胶
技术领域
本发明属粘结剂领域,尤其涉及一种耐高温热熔胶。
背景技术
    近几年,复合材料和塑料等新材料在汽车上的应用使得汽车用胶粘剂和密封胶用量也持续增长,其中汽车内饰件是胶粘剂用量迅速增长的一个领域。 汽车内饰件热熔胶的需求越来越多。
发明内容
本发明的目的是提供一种耐高温热熔胶。
为了实现上述目的本发明采用如下技术方案:
    一种耐高温热熔胶,其特征在于,其是由下述重量份的原料制得:
顺丁烯二酸酐1-2、聚氨酯树脂2-4,丙烯酸树脂3-6、EEA 8-10,EVA  38-58,乙烯基三甲氧基硅烷 0.3-0.5、交联剂TAC 1-2,C9石油树脂15-20,石蜡3-5、甲基丙烯酸锌 0.2-0.4、松香138树脂9-12,当归油0.2-0.3,复合纳米填料1-2;
复合纳米填料由下述重量份的原料制得:陶土10-12、水滑石粉2-4、高岭土 5-12,环氧大豆油1.5-2.8、石墨粉1-2、淘洗泥1-2、氧化铝1-2、醇醚糖苷0.2-0.4、磷酸氢二铵0.1-0.2、邻苯二甲酸二正辛酯0.1-0.2、纳米碳粉1-2、烷基酚聚氧乙烯醚0.4-0.6、N-甲基吡咯烷酮1-2、硅烷偶联剂KH550 0.3-0.5,平平加 0.2-0.4;
所述的复合纳米填料的制备方法为:制备方法是将陶土、水滑石粉、高岭土在浓度为15-18%的盐酸中浸泡5-8小时,取出,去离子水洗涤,干燥后,在600-800℃下煅烧1-2小时,取出,与氧化铝、石墨粉一并加入适量水中研磨,加10-15%氢氧化钠溶液调PH为8.5-9.5,研磨浆料至400-500目后,再加盐酸溶液调为中性,干燥,再与剩余原料混合,研磨成纳米粉末后即得。
    所述的一种耐高温热熔胶,其特征在于:
制备步骤是:
(1)将EVA、EEA 放入共混机中混匀备用;
(2)再将甲基丙烯酸锌、聚氨酯树脂、复合纳米填料放入共混机中混匀备用;
(3)再将其余原料放入共混机中混匀后,造粒、冷却和切粒,即得。
本发明的有益效果:本发明配料合理,各原料相容性好,各项性能优异,特别适用于汽车内饰件表面复合机织面料,长期使用耐高温效果好,不会起泡,寿命长。
具体实施方式
   一种耐高温热熔胶,其是由下述重量kg的原料制得:
顺丁烯二酸酐1、聚氨酯树脂4,丙烯酸树脂3、EEA 10,EVA  49,乙烯基三甲氧基硅烷 0.5、交联剂TAC 1,C9石油树脂20,石蜡5、甲基丙烯酸锌 0.4、松香138树脂10,当归油0.3,复合纳米填料2;
复合纳米填料由下述重量kg的原料制得:陶土12、水滑石粉4、高岭土 12,环氧大豆油1.8、石墨粉2、淘洗泥1、氧化铝2、醇醚糖苷0.4、磷酸氢二铵0.2、邻苯二甲酸二正辛酯0.2、纳米碳粉1、烷基酚聚氧乙烯醚0.5、N-甲基吡咯烷酮1、硅烷偶联剂KH550  0.5,平平加 0.4;
所述的复合纳米填料的制备方法为:制备方法是将陶土、水滑石粉、高岭土在浓度为18%的盐酸中浸泡5小时,取出,去离子水洗涤,干燥后,在800℃下煅烧2小时,取出,与氧化铝、石墨粉一并加入适量水中研磨,加15%氢氧化钠溶液调PH为9.5,研磨浆料至400目后,再加盐酸溶液调为中性,干燥,再与剩余原料混合,研磨成纳米粉末后即得。
    所述的一种耐高温热熔胶,制备步骤是:
(1)将EVA、EEA 放入共混机中混匀备用;
(2)再将甲基丙烯酸锌、聚氨酯树脂、复合纳米填料放入共混机中混匀备用;
(3)再将其余原料放入共混机中混匀后,造粒、冷却和切粒,即得。
本实施例的粘结剂的表观粘度为4900MPa.s,剥离强度56N/2.5cm2,初粘力达到5号钢球,开放时间41s,24小时热稳定性状稳定。

Claims (2)

1.一种耐高温热熔胶,其特征在于,其是由下述重量份的原料制得:
顺丁烯二酸酐1-2、聚氨酯树脂2-4,丙烯酸树脂3-6、EEA 8-10,EVA  38-58,乙烯基三甲氧基硅烷 0.3-0.5、交联剂TAC 1-2,C9石油树脂15-20,石蜡3-5、甲基丙烯酸锌 0.2-0.4、松香138树脂9-12,当归油0.2-0.3,复合纳米填料1-2;
复合纳米填料由下述重量份的原料制得:陶土10-12、水滑石粉2-4、高岭土 5-12,环氧大豆油1.5-2.8、石墨粉1-2、淘洗泥1-2、氧化铝1-2、醇醚糖苷0.2-0.4、磷酸氢二铵0.1-0.2、邻苯二甲酸二正辛酯0.1-0.2、纳米碳粉1-2、烷基酚聚氧乙烯醚0.4-0.6、N-甲基吡咯烷酮1-2、硅烷偶联剂KH550 0.3-0.5,平平加 0.2-0.4;
所述的复合纳米填料的制备方法为:制备方法是将陶土、水滑石粉、高岭土在浓度为15-18%的盐酸中浸泡5-8小时,取出,去离子水洗涤,干燥后,在600-800℃下煅烧1-2小时,取出,与氧化铝、石墨粉一并加入适量水中研磨,加10-15%氢氧化钠溶液调PH为8.5-9.5,研磨浆料至400-500目后,再加盐酸溶液调为中性,干燥,再与剩余原料混合,研磨成纳米粉末后即得。
2.根据权利要求1所述的一种耐高温热熔胶,其特征在于:
制备步骤是:
(1)将EVA、EEA 放入共混机中混匀备用;
(2)再将甲基丙烯酸锌、聚氨酯树脂、复合纳米填料放入共混机中混匀备用;
(3)再将其余原料放入共混机中混匀后,造粒、冷却和切粒,即得。
CN201310505609.XA 2013-10-24 2013-10-24 一种耐高温热熔胶 Pending CN103571388A (zh)