[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

CN102326610A - 粉状饼干防霉脱氧保鲜剂 - Google Patents

粉状饼干防霉脱氧保鲜剂 Download PDF

Info

Publication number
CN102326610A
CN102326610A CN 201110199006 CN201110199006A CN102326610A CN 102326610 A CN102326610 A CN 102326610A CN 201110199006 CN201110199006 CN 201110199006 CN 201110199006 A CN201110199006 A CN 201110199006A CN 102326610 A CN102326610 A CN 102326610A
Authority
CN
China
Prior art keywords
antistaling agent
powdery
deoxidizing antistaling
biscuit
mouldproof
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 201110199006
Other languages
English (en)
Other versions
CN102326610B (zh
Inventor
许庆华
许盛英
袁长兵
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU JIAAN FOOD CO Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201110199006A priority Critical patent/CN102326610B/zh
Publication of CN102326610A publication Critical patent/CN102326610A/zh
Application granted granted Critical
Publication of CN102326610B publication Critical patent/CN102326610B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种粉状饼干防霉脱氧保鲜剂,其技术方案的要点是,粉状饼干防霉脱氧保鲜剂由红色膨润土、白云石凹凸棒石粘土、铝矾土、硫酸、还原铁粉、茶多酚和丙酸钙组成。粉状饼干防霉脱氧保鲜剂的生产方法:将红色膨润土、白云石凹凸棒石粘土、铝矾土混合进行酸化、压片及热处理后与还原铁粉、茶多酚和丙酸钙共同粉碎,包装为粉状饼干防霉脱氧保鲜剂。将粉状饼干防霉脱氧保鲜剂放置在饼干的包装容器内,防霉、脱氧和保鲜是同步进行的,能除去饼干包装内的游离氧和部分游离水。粉状饼干防霉脱氧保鲜剂不掺混在饼干原料内,能确保饼干的内在质量,可保持饼干原有的新鲜风味,粉状饼干防霉脱氧保鲜剂适用于放置在饼干的小包装内。

Description

粉状饼干防霉脱氧保鲜剂
技术领域
本发明涉及防霉保鲜剂,具体涉及一种粉状饼干防霉脱氧保鲜剂。
背景技术
饼干的特点是甜味纯正、酥松香脆、食之爽口和有咬劲,饼干已成为人们日常生活中一种零食。
质量合格的饼干水分在4~6%,但是饼干具有不同程度的吸湿性。当空气中相对湿度超过70%时,饼干即开始吸湿,致使其受潮发软,表现为饼干折断无声、入口不脆,且极易发霉变质。 
饼干由于受日晒或高温作用,会引起脂肪氧化酸败而发生哈喇味,饼干也极易受其他物品气味的污染而变味。 
发明内容
本发明的目的是克服现有技术中不足之处,提供一种具有防霉、脱氧和保鲜多功能粉状饼干防霉脱氧保鲜剂。
粉状饼干防霉脱氧保鲜剂由红色膨润土、白云石凹凸棒石粘土、铝矾土、硫酸、还原铁粉、茶多酚和丙酸钙组成。
粉状饼干防霉脱氧保鲜剂的生产方法:将红色膨润土、白云石凹凸棒石粘土、铝矾土混合进行酸化、压片及热处理后与还原铁粉、茶多酚和丙酸钙共同粉碎,包装为粉状饼干防霉脱氧保鲜剂。
红色膨润土中的氧化铁含量≥14%,三氧化二铝含量≥10%;白云石凹凸棒石粘土中氧化钙的含量≥24%,氧化镁的含量≥12%;铝矾土中的三氧化二铝含量≥55%,将红色膨润土、白云石凹凸棒石粘土和铝矾土混合为矿物混合物,矿物混合物经过酸化处理后生成部分硫酸钙、硫酸镁、硫酸亚铁和硫酸铝等硫酸盐混合物,硫酸钙、硫酸镁、硫酸亚铁和硫酸铝都具有较高的吸湿能力,再将酸化处理的矿物混合物进行活化热处理,大大提高了酸化处理的矿物混合物的吸湿效果。
红色膨润土产于江苏省盱眙县桂五镇跑马山矿区,主要成分有石英、蒙脱石、高岭石、赤铁矿和长石,氧化铁含量≥14%,三氧化二铝含量≥10%,矿区储量有100万吨以上,是一座露天矿,由于用途不广泛,目前尚未能大面积开采。
还原铁粉能够吸收空气中的氧气,1克还原铁粉除氧能力为300mL,折合空气1500mL,除氧效果好,本发明选用的还原铁粉颗粒细度≤0.074毫米。
茶多酚具有很强的抗氧化作用,易溶于水,稳定性极强,对饼干中的色素和维生素类有保护作用,使饼干在较长时间内保持原有色泽与营养水平,能有效防止饼干的腐败,并能消除异味。
丙酸钙溶于水,是酸型食品防腐剂,在酸性条件下,产生游离丙酸,具有抗菌作用,其抑菌作用受环境pH值的影响,在pH值5.0时霉菌的抑制作用最佳。
白云石凹凸棒石粘土、铝矾土和还原铁粉是常见的商品。
本发明通过下述技术方案予以实现:
1、粉状饼干防霉脱氧保鲜剂的配料按重量百分比由下列组分组成:防霉剂40~85%、还原铁粉14~58%、茶多酚0.01~2%和丙酸钙0.01~2%;
粉状饼干防霉脱氧保鲜剂的生产方法:将粉状饼干防霉脱氧保鲜剂的配料混合后输入粉碎机进行粉碎,粉碎后的颗粒细度≤0.074毫米,密封包装为粉状饼干防霉脱氧保鲜剂;
所述防霉剂的生产方法:①矿物混合物的配料按重量百分比由下列组分组成:红色膨润土25~55%、白云石凹凸棒石粘土20~50%和铝矾土15~40%;②将矿物混合物的配料混合后进行粉碎,粉碎后的颗粒细度≤0.50毫米;③稀硫酸的配制按重量百分比由下列组分组成:浓度98﹪的硫酸2~20%和水80~98%;④酸化处理的配料按重量百分比由下列组分组成:粉碎后的矿物混合物55~75%和稀硫酸25~45%;⑤将稀硫酸缓慢加入粉碎后的矿物混合物中进行酸化处理,经过酸化处理的矿物混合物堆放24~72小时后,输入对辊机中挤压为片状物,片状物的厚度控制在1~3毫米;⑥将片状物输入回转式烘干机中进行热处理后为防霉剂,热处理时的温度控制在250~320℃,时间控制在60~180分钟,防霉剂的含水量≤1.0%。
本发明的酸化处理工艺没有废水排放,方法简单,环保无污染。
将防霉剂加入称量瓶后,置于盛有氯化钠饱和水溶液的干燥器内,在温度为35℃的条件下,24小时的静态水吸附≥20%。
还原铁粉能够吸收空气中的氧气,1克还原铁粉除氧能力为300mL,折合空气1500mL,除氧效果好,这是本领域技术人员的公知常识,但是单独使用还原铁粉不能同时达到防霉脱氧保鲜的效果;在本发明中采用还原铁粉、防霉剂、茶多酚和丙酸钙共同粉碎后,包装为具有防霉、脱氧和保鲜多功能粉状饼干防霉脱氧保鲜剂。
将粉状饼干防霉脱氧保鲜剂放置在饼干的包装容器内,防霉、脱氧和保鲜是同步进行的,能除去饼干包装内的游离氧和部分游离水。
根据不同饼干的含水量,选择粉状饼干防霉脱氧保鲜剂不同的配料重量百分比,在保持一定量的水分时进行防霉、脱氧和保鲜,粉状饼干防霉脱氧保鲜剂能有效的防止饼干成分氧化和抑制微生物的生长和繁殖。
粉状饼干防霉脱氧保鲜剂不掺混在饼干原料内,能确保饼干的内在质量,可保持饼干原有的新鲜风味,在保质期内不会出现干裂,也不会产生酸味、腐败变质味、霉味或其他不良异味。
粉状饼干防霉脱氧保鲜剂使用后,当一般垃圾处理,可降解,没有环境污染。
粉状饼干防霉脱氧保鲜剂适用于放置在饼干的小包装内。
具体实施方式
下面结合实施例对本发明作进一步的描述: 
1、粉状饼干防霉脱氧保鲜剂的配料按重量百分比由下列组分组成:防霉剂66%、还原铁粉33.5%、茶多酚0.3%和丙酸钙0.2%;
粉状饼干防霉脱氧保鲜剂的生产方法:将粉状饼干防霉脱氧保鲜剂的配料混合后输入粉碎机进行粉碎,粉碎后的颗粒细度≤0.074毫米,密封包装为粉状饼干防霉脱氧保鲜剂;
所述防霉剂的生产方法:①矿物混合物的配料按重量百分比由下列组分组成:红色膨润土40%、白云石凹凸棒石粘土34%和铝矾土26%;②将矿物混合物的配料混合后进行粉碎,粉碎后的颗粒细度≤0.50毫米;③稀硫酸的配制按重量百分比由下列组分组成:浓度98﹪的硫酸8%和水92%;④酸化处理的配料按重量百分比由下列组分组成:粉碎后的矿物混合物65%和稀硫酸35%;⑤将稀硫酸缓慢加入粉碎后的矿物混合物中进行酸化处理,经过酸化处理的矿物混合物堆放48小时后,输入对辊机中挤压为片状物,片状物的厚度控制在1.5毫米;⑥将片状物输入回转式烘干机中进行热处理后为防霉剂,热处理时的温度控制在280~300℃,时间控制在120分钟,防霉剂的含水量≤1.0%。
经过现场测试,将防霉剂加入称量瓶后,置于盛有氯化钠饱和水溶液的干燥器内,在温度为35℃的条件下,24小时的静态水吸附≥24%。

Claims (1)

1.一种粉状饼干防霉脱氧保鲜剂,其特征在于,粉状饼干防霉脱氧保鲜剂的配料按重量百分比由下列组分组成:防霉剂40~85%、还原铁粉14~58%、茶多酚0.01~2%和丙酸钙0.01~2%;
粉状饼干防霉脱氧保鲜剂的生产方法:将粉状饼干防霉脱氧保鲜剂的配料混合后输入粉碎机进行粉碎,粉碎后的颗粒细度≤0.074毫米,密封包装为粉状饼干防霉脱氧保鲜剂;
所述防霉剂的生产方法:①矿物混合物的配料按重量百分比由下列组分组成:红色膨润土25~55%、白云石凹凸棒石粘土20~50%和铝矾土15~40%;②将矿物混合物的配料混合后进行粉碎,粉碎后的颗粒细度≤0.50毫米;③稀硫酸的配制按重量百分比由下列组分组成:浓度98﹪的硫酸2~20%和水80~98%;④酸化处理的配料按重量百分比由下列组分组成:粉碎后的矿物混合物55~75%和稀硫酸25~45%;⑤将稀硫酸缓慢加入粉碎后的矿物混合物中进行酸化处理,经过酸化处理的矿物混合物堆放24~72小时后,输入对辊机中挤压为片状物,片状物的厚度控制在1~3毫米;⑥将片状物输入回转式烘干机中进行热处理后为防霉剂,热处理时的温度控制在250~320℃,时间控制在60~180分钟,防霉剂的含水量≤1.0%。
CN201110199006A 2011-07-17 2011-07-17 粉状饼干防霉脱氧保鲜剂 Expired - Fee Related CN102326610B (zh)