CN109324427A - A kind of production method of anti-blue light automatic light-adjusting glasses - Google Patents
A kind of production method of anti-blue light automatic light-adjusting glasses Download PDFInfo
- Publication number
- CN109324427A CN109324427A CN201811350919.8A CN201811350919A CN109324427A CN 109324427 A CN109324427 A CN 109324427A CN 201811350919 A CN201811350919 A CN 201811350919A CN 109324427 A CN109324427 A CN 109324427A
- Authority
- CN
- China
- Prior art keywords
- glass
- blue light
- cleaning
- light
- production method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
A kind of production method of anti-blue light automatic light-adjusting glasses comprising following processing step: production raw material, the cleaning that feeds intake, apply carve optical cement, exposure, development, etching, demoulding, detect whether bad pin hole, cleaning, print frame point, using powder spraying apparatus sprayed interval body on a wherein sheet glass, with full application of brake make-up machine by two panels glass gluing together, the glass heat-pressure curing that will post forms CELL, abnormity cutting, perfusion PN liquid crystal, UV and irradiates, seals, cleans, presses FPC, is assembled into glasses.The anti-blue light glasses made according to the present invention, anti-blue light effect is good, and performance is stablized, and can automatically adjust the light transmittance of glasses.
Description
Technical field
The present invention relates to daily protective eyewear art more particularly to a kind of production sides of anti-blue light automatic light-adjusting glasses
Method.
Background technique
Blue light is the important component of visible light, and for nature itself without individual white light, blue light and green light, yellow light are mixed
Just it is presented white light after conjunction, the energy of green light and yellow light is smaller, and smaller to the injury of eyes, the wavelength of blue light is short, energy is high, special
It is not UV445 shortwave blue light, the through retina of shape body can be penetrated.With popularizing for LED light, blue light becomes injury eyes most
Big arch-criminal, blue light are mainly derived from computer, mobile phone, plate, TV, various LED devices including LED light etc..Present
Child likes playing mobile phone, and prolonged use is especially big to eye injury, to prevent blue light from having invented one kind to the harm of eyes
The production method of anti-blue light automatic light-adjusting glasses reduces injury of numerous electronic products to eyes.
Summary of the invention
The purpose of the present invention is overcoming the deficiencies in the prior art, a kind of system of anti-blue light automatic light-adjusting glasses is provided
Make method.The anti-blue light glasses of the production method production of a kind of anti-blue light automatic light-adjusting glasses according to the present invention, can prevent indigo plant
Harm of the light to eyes, and the transmitance of glasses is not reduced, the efficiency of anti-blue light is greater than 40%, and can be with an automatic light meter, with
The light transmittance of the strong adjust automatically glasses of change of ambient light.
A kind of production method of anti-blue light automatic light-adjusting glasses comprising following processing step: production raw material feed intake clearly
It washes, apply and carve optical cement, exposure, development, etching, demoulding, detected whether bad pin hole, cleaning, printed frame point, having been incited somebody to action using powder spraying apparatus
Spacer sprays on a wherein sheet glass, with full application of brake make-up machine by two panels glass gluing together, the glass that will post
Heat-pressure curing forms CELL, abnormity cutting, perfusion PN liquid crystal, UV and irradiates, seals, cleaning, press FPC, be assembled into glasses.
The anti-blue light glasses made according to the present invention, anti-blue light effect is good, and performance is stablized, and can automatically adjust the light transmission of glasses
Rate.
A kind of production method of anti-blue light automatic light-adjusting glasses comprising following processing step:
S1, production raw material: raw material include two blocks of glass, and one of glass one side plating anti-blue light film, another side plates ITO
Film, in addition one block of glass will wherein plate ito film on one side, and another side is not processed, by the way that two blocks of glass are plated ITO after post-processing
Adaptable being closely pressed together on of film one side is formed together a piece of blue light automatic light-adjusting glasses eyeglass;At 800 nanometers (nm), blue light
Transmitance be 60%.Ito glass plates anti-blue light film and manufactures anti-blue light film using existing membrane equipment, and blue Light Film playback is placed.
S2, feed intake cleaning: will wash in the substrate investment cleaning equipment of LCD;Such as using ultrasonic cleaning apparatus into
Row cleaning, cleaning can be divided into repeatedly, and multiple cleaning includes cleaning agent for optical glass cleaning, one or many RO pure water ultrasonic waves
Rinsing.
Resist coating: S3 uses three-roll coating mode, positive-working photoresist (photosensitive adhesiveness 14S) is uniformly coated on ITO
On glass substrate front, photoresists diluent is volatilized by hot plate preliminary drying, is adhered on ito glass.Three-roll coating mode packet
Applicator roll, support roller are included, the spacing (coating thickness) between applicator roll and glass substrate is adjustable, and applicator roll is equipped with along axis
The groove small to the spiral shape of extension, the spiral groove can effectively keep the thickness of coating fluid, pressure.
S4, exposure: with ultraviolet light (wavelength 365nm) chromium plate good by pre-production, being irradiated to photoresist surface, make by
The photoresist layer of ultraviolet light part reacts, and carries out selective exposure to photoresist under ultraviolet lamp.
S5, development: handling glass surface with developer solution, and the photoresist layer (positive photoresist) decomposed by illumination is removed, is protected
The photoresist layer for staying unexposed portion, with the photoresist by UV illumination part point is dissolved in developer solution, the glass after development is wanted
By the firmly treatment of certain temperature, the concentration 0.7-0.73mol/L of developer solution.
S6, etching: the ito film that unglazed photoresist covers is eroded with harsh liquid (7.5 ± 0.2mol/L) appropriate, in this way
Required ITO electrode figure is just obtained.
S7, demoulding: making liquid parting with high-concentration alkali liquor, and photoresist lift off remaining on glass is fallen, shape on ito glass is made
At the ITO pattern completely the same with film figure.
S8, detected whether that pin hole is bad.
S9, cleaning: using pure water that glass cleaning is clean with cleaning equipment;Such as it is cleaned multiple times using RO pure water ultrasonic wave.
S10, print frame point: edging material (sealant) respectively stamps upper plate and lower glass sheet with the method for silk-screen printing
Frame adhesive and conducting resinl.
S11, spacer/interval body Spacer is sprayed on small sheet glass using powder spraying apparatus.
S12, using Full automatic doubler by two panels glass gluing together.
S13, the glass heat-pressure curing that will be posted form CELL.
S14, abnormity cutting: according to the polymorphic structure of the left and right eyeglass of anti-blue light film (such as irregular polygon or irregular ellipse
It is round) it is cut to obtain required lens shape.
S15, PN liquid crystal is perfused using liquid filling equipment.
S16, it is irradiated using UV.
S17, it is sealed.
S18, cleaning: using pure water that glass cleaning is clean with cleaning equipment;Such as it is cleaned multiple times using RO pure water ultrasonic wave.
S19, compacting FPC is carried out using certain pressure.
S20, glasses are assembled into.
The anti-blue light glasses made according to the present invention, anti-blue light effect is good, and performance is stablized, and can automatically adjust the light transmission of glasses
Rate.
Detailed description of the invention
Fig. 1 is the left and right lens structure schematic diagram of anti-blue light film of the present invention.
Specific embodiment
The present invention is described in further detail below in conjunction with the accompanying drawings.
A kind of production method of anti-blue light automatic light-adjusting glasses comprising following processing step:
S1, production raw material: raw material include two blocks of glass, and one of glass one side plating anti-blue light film, another side plates ITO
Film, in addition one block of glass will wherein plate ito film on one side, and another side is not processed, by the way that two blocks of glass are plated ITO after post-processing
Adaptable being closely pressed together on of film one side is formed together a piece of blue light automatic light-adjusting glasses eyeglass;At 800 nanometers (nm), blue light
Transmitance be 60%.Ito glass plates anti-blue light film and manufactures anti-blue light film using existing membrane equipment, and blue Light Film playback is placed.
The means such as post-processing, pressing are all the existing technological means in this field, are no longer described herein.
S2, feed intake cleaning: will wash in the substrate investment cleaning equipment of LCD;Such as using ultrasonic cleaning apparatus into
Row cleaning, cleaning can be divided into repeatedly, and multiple cleaning includes cleaning agent for optical glass cleaning, one or many RO pure water ultrasonic waves
Rinsing.
Resist coating: S3 uses three-roll coating mode, positive-working photoresist (photosensitive adhesiveness 14S) is uniformly coated on ITO
On glass substrate, photoresists diluent is volatilized by hot plate preliminary drying, is adhered on ito glass.Three-roll coating mode includes applying
Cloth rewinder roll, support roller, the spacing (coating thickness) between applicator roll and glass substrate is adjustable, and applicator roll is equipped with to be prolonged along axial direction
The small groove of the spiral shape stretched, the spiral groove can effectively keep the thickness of coating fluid, pressure.
S4, exposure: with ultraviolet light (wavelength 365nm) chromium plate good by pre-production, being irradiated to photoresist surface, make by
The photoresist layer of ultraviolet light part reacts, and carries out selective exposure to photoresist under ultraviolet lamp.
S5, development: handling glass surface with developer solution, and the photoresist layer (positive photoresist) decomposed by illumination is removed, is protected
The photoresist layer for staying unexposed portion, with the photoresist by UV illumination part point is dissolved in developer solution, the glass after development is wanted
By the firmly treatment of certain temperature, the concentration 0.7-0.73mol/L of developer solution.
S6, etching: the ito film that unglazed photoresist covers is eroded with harsh liquid (7.5 ± 0.2mol/L) appropriate, in this way
Required ITO electrode figure is just obtained.
S7, demoulding: making liquid parting with high-concentration alkali liquor, and photoresist lift off remaining on glass is fallen, shape on ito glass is made
At the ITO pattern completely the same with film figure.
S8, detected whether that pin hole is bad.
S9, cleaning: using pure water that glass cleaning is clean with cleaning equipment;Such as it is cleaned multiple times using RO pure water ultrasonic wave.
S10, print frame point: edging material (sealant) respectively stamps upper plate and lower glass sheet with the method for silk-screen printing
Frame adhesive and conducting resinl.
S11, spacer/interval body Spacer is sprayed on a sheet glass wherein using powder spraying apparatus.
S12, using Full automatic doubler by two panels glass gluing together.
S13, the glass heat-pressure curing that will be posted form CELL.
S14, abnormity cutting: according to the polymorphic structure of the left and right eyeglass of anti-blue light film (such as irregular polygon or irregular ellipse
It is round) it is cut to obtain required lens shape.
S15, PN liquid crystal is perfused to its inside.
S16, it is irradiated using UV.
S17, it is sealed.
S18, cleaning: using pure water that glass cleaning is clean with cleaning equipment;Such as it is cleaned multiple times using RO pure water ultrasonic wave.
S19, compacting FPC is carried out using certain pressure.
S20, glasses are assembled into.
The anti-blue light glasses made according to the present invention, anti-blue light effect is good, and performance is stablized, and can automatically adjust the light transmission of glasses
Rate.
Above embodiment is the description of the invention, is not limitation of the invention, it is possible to understand that is not departing from this hair
A variety of change, modification, replacement and modification, guarantor of the invention can be carried out to these embodiments in the case where bright principle and spirit
Shield range is defined by the appended claims and the equivalents thereof.
Claims (8)
1. a kind of production method of anti-blue light automatic light-adjusting glasses comprising following processing step:
S1, production raw material: raw material include two blocks of glass, and one of glass one side plating anti-blue light film, another side plates ITO
Film, in addition one block of glass will wherein plate ito film on one side, and another side is not processed, by the way that two blocks of glass are plated ITO after post-processing
Adaptable being closely pressed together on of film one side is formed together a piece of blue light automatic light-adjusting glasses eyeglass;
S2, feed intake cleaning: will wash in the substrate investment cleaning equipment of LCD;
S3, resist coating: using three-roll coating mode, and positive-working photoresist is uniformly coated on ito glass substrate front, passes through heat
Plate preliminary drying volatilizees photoresists diluent, is adhered on ito glass;
S4, exposure: with the ultraviolet light chromium plate good by pre-production, it is irradiated to photoresist surface, is made by ultraviolet light part
Photoresist layer react, selective exposure is carried out to photoresist under ultraviolet lamp;
S5, development: handling glass surface with developer solution, and the photoresist layer or positive photoresist that decompose by illumination are removed, retained not
The photoresist layer of exposed portion, with the photoresist by UV illumination part point is dissolved in developer solution, the glass after development will pass through
The firmly treatment of certain temperature;
S6, etching: the ito film of the non-lithography glue covering of upper and lower two sheet glass is eroded with harsh liquid appropriate, is thus obtained
Required ITO electrode figure;
S7, demoulding: making liquid parting with high-concentration alkali liquor, and photoresist lift off remaining on glass is fallen, make on ito glass formed with
The completely the same ITO pattern of film figure;
S8, detected whether that pin hole is bad;
S9, cleaning: using pure water that glass cleaning is clean with cleaning equipment;
S10, print frame point: the method for edging material silk-screen printing is stamped into frame adhesive and conduction to upper plate and lower glass sheet respectively
Glue;
S11, spacer/interval body Spacer is sprayed on a sheet glass wherein using powder spraying apparatus;
S12, using Full automatic doubler by two panels glass gluing together;
S13, the glass heat-pressure curing that will be posted form CELL;
S14, abnormity cutting: it is cut to obtain required lens shape according to the anisotropic approach of the left and right eyeglass of anti-blue light film;
S15, PN liquid crystal is perfused to its inside;
S16, it is irradiated using UV;
S17, it is sealed;
S18, cleaning: using pure water that glass cleaning is clean with cleaning equipment;
S19, compacting FPC is carried out using certain pressure;
S20, glasses are assembled into.
2. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
It in S2, is cleaned using ultrasonic cleaning apparatus, cleaning is divided into repeatedly, and multiple cleaning includes that cleaning agent for optical glass is clear
It washes, one or many RO pure water ultrasonic rinsings.
3. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
In S3, three-roll coating mode includes applicator roll, support roller, and the spacing between applicator roll and glass substrate is adjustable, applicator roll
It is equipped with the spiral groove axially extended, which can effectively keep the thickness of coating fluid, pressure.
4. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
In S4, the wavelength 365nm or 367nm of ultraviolet light.
5. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
In S5, the concentration 0.7-0.73mol/L of developer solution.
6. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
In S6,7.5 ± 0.2mol/L of concentration of harsh liquid.
7. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
It in S9, is cleaned multiple times, is cleaned multiple times between process added with blowing drying process using RO pure water ultrasonic wave.
8. a kind of production method of anti-blue light automatic light-adjusting glasses according to claim 1, which is characterized in that the step
In S14, which is irregular polygon or irregular ellipse.