[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

CN1089974A - Polyvinyl-chloride water-proof paint and preparation method - Google Patents

Polyvinyl-chloride water-proof paint and preparation method Download PDF

Info

Publication number
CN1089974A
CN1089974A CN 93110028 CN93110028A CN1089974A CN 1089974 A CN1089974 A CN 1089974A CN 93110028 CN93110028 CN 93110028 CN 93110028 A CN93110028 A CN 93110028A CN 1089974 A CN1089974 A CN 1089974A
Authority
CN
China
Prior art keywords
polyvinyl
raw material
stablizer
preparation
softening agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 93110028
Other languages
Chinese (zh)
Inventor
刘国则
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Construction Engineering Co Shenyang Branch Of Chinese Academy Of Sciences (cn
Original Assignee
Construction Engineering Co Shenyang Branch Of Chinese Academy Of Sciences (cn
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Construction Engineering Co Shenyang Branch Of Chinese Academy Of Sciences (cn filed Critical Construction Engineering Co Shenyang Branch Of Chinese Academy Of Sciences (cn
Priority to CN 93110028 priority Critical patent/CN1089974A/en
Publication of CN1089974A publication Critical patent/CN1089974A/en
Pending legal-status Critical Current

Abstract

This processing method is a kind of preparation method of waterproof paint, be characterized in adopting coal oil-collecting, polyvinyl chloride resin softening agent, stablizer and weighting agent to make raw material, mixed in proportion, softening agent can be used dibutylester, dibutyl ester and calcium stearate, and stablizer adopts carbolineum or edible vegetable oil, above raw material is put into reactor stirred, heat, heated 1~2 hour 130~140 ℃ of temperature, become black clay---waterproof paint at last, can be directly used in the architecture construction surface.Advantage: raw material is cheap, easy to manufacture, good water-proof effect, life-span long, easy to use.

Description

Polyvinyl-chloride water-proof paint and preparation method
The invention belongs to engineering with water-proof material and preparation method.
At present be the pitch prill waterproof layer what building trade was widely used, be placed with lincrusta covers in needs waterproof place, shining pitch prill then outside paper makes inner building structure have water-proof function, there is a kind of method to ooze and lump together again in the concrete grey of building a wall, dosing CaCl2-powder and cement mortar, has very strong water-proof function, this kind water-proof treatment technology complexity, construction is lost time, for using pitch prill that serious pollution is arranged, it is that raw material is made waterproof paint that the plastic ointment of employing is also arranged, and it is synthetic to protect high temperature, and secondary plasticizing, material aging is rapid, does not reach subzero 30 ℃ requirement during low temperature.
For solving above deficiency, purpose of the present invention provides a kind of polyvinyl-chloride water-proof paint, utilizes existing part industrial chemicals synthetic, through suitably processing, make waterproof paint, can be directly used in the surface of buildings, effectively solved the building surface waterproof problem, and easy construction, life-span are long.
The contained raw material and the weight percent of polyvinyl-chloride water-proof paint of the present invention:
Coal tar 35~42%
Polyvinyl chloride (PVC) resin 7~10%
Plasticizer A (dibutylester) 5~8%
Softening agent B(carbolineum) 20~22%
Stablizer (calcium stearate) 0.5~1.5%
Weighting agent (fossil meal) 25~30%
The complete processing of polyvinyl-chloride water-proof paint:
Adopt a plasticizing process moulding of low-temperature mixed.
With coal tar 35~42%
Polyvinyl chloride (PVC) resin 7~10%
Plasticizer A (dibutylester) 5~8%
Softening agent B(scallion oil) 20~22%
Stablizer (calcium stearate) 0.5~1.5%
Weighting agent (fossil meal) 25~30%
Be added in the reactor, in 130~140 ℃ of scopes, heated 1~2 hour, make the interior material roasting of still change into the clay shape, be black, be waterproof paint-waterproof clay.
The present invention's advantage: the waterproof paint raw material sources are extensive, cost is low, production is easy, prescription adopts the dual function of composite elasticizer and one package stabilizer, too early migration and volatilization have been overcome, delayed aging, the life-span is long, be not afraid of the soda acid etch, good water-proof effect, high temperature does not trickle for 80 ℃, 30 ℃ of not embrittlement of low temperature.
The present invention's embodiment:
100 kilograms in coal tar
10.5 kilograms of polyvinyl chloride resins
0.5 kilogram of plasticizer A (dibutylester)
0.1 kilogram of stablizer (calcium stearate)
30 kilograms of weighting agents (fossil meal)
Being put into stirs in the reactor heats 140 ℃, 1 hour black clay-waterproof paint, can be directly used in the building surface coating.

Claims (2)

1, a kind of polyvinyl-chloride water-proof paint is characterized in that contained raw material and weight percent are:
Coal tar 35~42%
Polyvinyl chloride (PVC) resin 7~10%
Plasticizer A (dibutylester) 5~8%
Softening agent B (scallion oil) 20~22%
Stablizer (calcium stearate) 0.5~1.5%
Weighting agent (fossil meal) 25~30%
2, a kind of polyvinyl-chloride water-proof paint preparation method is characterized in that:
Coal tar 35~42%
Polyvinyl chloride (PVC) resin 7~10%
Plasticizer A (dibutylester) 5~8%
Softening agent B(scallion oil) 20~22%
Stablizer (calcium stearate) 0.5~1.5%
Weighting agent (fossil meal) 25~30%
Be put in proportion in the reactor, stir, heat 130~140 ℃, 1~2 hour time, coloring agent mud shape darkly.
CN 93110028 1993-01-12 1993-01-12 Polyvinyl-chloride water-proof paint and preparation method Pending CN1089974A (en)