[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

CN108055818A - Anti- galvanic corrosion is electromagnetically shielded seal trim strip - Google Patents

Anti- galvanic corrosion is electromagnetically shielded seal trim strip Download PDF

Info

Publication number
CN108055818A
CN108055818A CN201711024181.1A CN201711024181A CN108055818A CN 108055818 A CN108055818 A CN 108055818A CN 201711024181 A CN201711024181 A CN 201711024181A CN 108055818 A CN108055818 A CN 108055818A
Authority
CN
China
Prior art keywords
rubber strip
cabinet
strip
conductive rubber
middle level
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711024181.1A
Other languages
Chinese (zh)
Inventor
谢义水
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Southwest Electronic Technology Institute No 10 Institute of Cetc
Original Assignee
Southwest Electronic Technology Institute No 10 Institute of Cetc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Southwest Electronic Technology Institute No 10 Institute of Cetc filed Critical Southwest Electronic Technology Institute No 10 Institute of Cetc
Priority to CN201711024181.1A priority Critical patent/CN108055818A/en
Publication of CN108055818A publication Critical patent/CN108055818A/en
Pending legal-status Critical Current

Abstract

The present invention proposes a kind of anti-galvanic corrosion electromagnetic shielding seal trim strip.It can solve the problems, such as to be only capable of realizing the Practical Project of cabinet, cabinet Electromagnetic Shield on Electronic Equipments without being avoided that galvanic corrosion with the compound closed shield pad of single conductive rubber strip using single conductive rubber pad and single rubber bodies using the present invention.The present invention is achieved by following methods:It is electromagnetically shielded sandwich of the seal trim strip by outer layer insulation rubber strip (1) → middle level conductive rubber strip (2) ← primary insulation rubber strip (3) composite molding one, wherein, middle level conductive rubber strip (2) is pressed from both sides in the form of dome to be connected between the groove that outer layer insulation rubber strip (1) and primary insulation rubber strip (3) are formed, middle level conductive rubber strip (2) realizes cabinet, the electromagnetic shielding of cabinet electronic equipment metallic matrix contact, outer layer insulation rubber strip (1) and primary insulation rubber strip (3) realize cabinet with the dome item of middle level conductive rubber strip (2) and its elastic extruded channels of formation, itself water vapor seal of cabinet electronic equipment metallic matrix contact.

Description

Anti- galvanic corrosion is electromagnetically shielded seal trim strip
Technical field
The present invention relates to a kind of electromagnetic shielding seal trim strips for being mainly used for cabinet, cabinet electronic equipment
Background technology
For a long time, the large scale electronic equipments such as cabinet, cabinet, mostly to be kneaded the standby machine of the rubber system of silver powder or aluminium silvering powder Case, cabinet electronic equipment form electromagnetic armouring structure between the single conductive rubber pad of generally use and cabinet lid door.Due to cabinet, Cabinet electronic equipment volume is big, the presence of ventilation and heat structure, and complete machine water vapor seal is poor or even blow-by.In natural environment The electrolyte that has been formed when having adsorbed sulfur dioxide, nitrogen dioxide, nitrogen, carbon dioxide, salt fog etc. of steam, direct invasion, leaching Wet, immersion is using the formation of single conductive rubber pad and cabinet, the electromagnetic armouring structure of rack room, due to the silver in conductive rubber pad Flour gold belongs to and cabinet, cabinet alloy matrix aluminum are there are potential difference, and electrochemical reaction occurs at electromagnetic armouring structure contact interface, leads Send a telegraph the cabinet in magnet shielding structure as anode, cabinet alloy matrix aluminum is corroded, and (i.e. the galvanic couple of different metal compatibility is rotten Erosion), in turn result in cabinet, cabinet electronic equipment electromagnetic shielding failure, anti-electromagnetic interference capability decline, seriously affect cabinet, The Electro Magnetic Compatibility of cabinet electronic equipment, electronic device environment adaptability significantly reduce.Aluminum Alloy Chassis, cabinet are rotten simultaneously Serious local corrosion has occurred in erosion, alloy, and surface has deep etch pit and wide and long corrosion cracking.Due to electronic The anti-galvanic corrosion poor-performing of equipment, and maintenance difficult is dismounted, seriously affect equipment guarantee performance and used life, economy damage It loses serious.
In actual damp and hot and salt fog extreme climate environment, the influence factor of galvanic corrosion includes the influence of galvanic series, ring The influence of the influence, area effect, galvanic couple of border factor to spacing etc..Cabinet, the cabinet electricity of this single conductive rubber pad realization Sub- installation electromagnetical shielding construction, in corrosive medium environment, due to cabinet, the light metal alloy standard electrode potential of cabinet use Very low, chemism is high, and surface can not be formed with protective oxide-film.When being contacted with other metals, it often makees For anode by galvanic corrosion.Galvanic corrosion can also lure in addition to accelerating the corrosion failure of light metal alloy anode member Corrosion failure more dangerous in the engineerings such as spot corrosion, crevice corrosion is sent out, results in cabinet, cabinet galvanic corrosion and capability of electromagnetic shielding The quality accident of failure takes place frequently, and economic loss is serious, it has also become industry engineering challenge urgently to be resolved hurrily.
In nature, the condition generally existing of electrochemical reaction occurs, therefore, galvanic corrosion has generality.To most For number galvanic corrosion, corrosion electrolyte, which is primarily referred to as condensing upon, contains some impurity (chloride, sulfate on material surface Deng) moisture film or solution.Corrosion electrolyte must continuously be present between different materials, and the ion for forming corrosion cell is led Electric branch.Light metal is one of most active metal in metal galvanic series, is always filled when Al alloys andMg alloys are connected with other metals When active anode is corroded at first.In practical applications, due to the requirement of mechanical structure and its electric conductivity, metal parts Between contact directly and can not avoid completely.Galvanic corrosion is actually one kind of macrocorrosion battery, and electricity occurs between metal Chemical reaction, generation galvanic corrosion should be with following three primary conditions, one, and there are enough current potentials of different corrosion potentials Difference, under I classes good environment (indoor environment, outdoor masking environment), potential difference is more than that 0.25V galvanic corrosions also will substantially be sent out Raw, Galvanic Current increases with the increase of potential difference.Potential difference between light metal alloy and the metal coupled with it is bigger, gently Metal alloy is as the more easy accelerated corrosion of anode;Two, corrosion electrolyte must continuously be present between different materials, It contacts directly or is connected by other conductors;Three, the material with the presence of electrolyte and there are different corrosion potentials.Namely It says, as long as lacking any of the above conditions, electrochemical reaction does not occur, and galvanic corrosion would not occur.
In Electromagnetic Shield on Electronic Equipments engineering design, due to being subject to the composite factors such as material, technique, structure, function It limits, conductive gasket must be contacted with cabinet, cabinet metallic matrix in electromagnetic armouring structure, and conductive gasket uses more It is poor that rubber mixes the standard electrode potential that silver powder or aluminium silvering powder are kneaded between sulfidization molding, with cabinet, cabinet alloy matrix aluminum Up to 2.47V, far above standard conditions of the difference in Electrode Potential that galvanic corrosion occurs for above-mentioned I classes good environment more than 0.25V.Cause This, prevent electrochemical reaction generation electrolyte existing for necessary condition be to prevent cabinet, cabinet Electromagnetic Shield on Electronic Equipments knot Galvanic corrosion occurs for structure, the ability for improving electromagnetic armouring structure anti-galvanic corrosion in itself be solve the above problems most directly, One of the most effective ways.
To solve Electromagnetic Shield on Electronic Equipments structure in salt mist environment, corrosive medium, galvanic couple occurs for different metal contact Corrosion, the engineering challenge of environmental suitability difference, engineering specialists devise multiple technologies scheme.Wherein, microwave/ In millimetre-wave circuit component, the technical solution of high-frequency circuit protection is taken into account, mostly with spies such as low temperature brazing, Laser Welding or parallel seam weldings Kind welding encapsulation technology, realizes hermetic seal and the composite protective of electromagnetic shielding.This technical solution quality there are complex process The shortcomings that control is difficult, maintainability is poor or can not repair, is only applicable to the miniaturized electronic devices such as microwave/millimeter wave circuit unit Electromagnetic shielding and weather environmental protection.
In the 1990s, for electronic equipment anti-adverse environment general requirement, relevant criterion is proposed " when using a kind of When sealing element cannot meet airtight (watertight) and two kinds of functions of electromagnetic shielding simultaneously, water vapor seal and electromagnetic shielding should respectively into Row, water vapor seal body should be arranged on outer layer, and electromagnetic armouring structure body should be arranged on internal layer, and fastener is arranged on outermost layer " it is close Envelope property design requirement.But the solution that this water vapor seal and electromagnetic shielding are implemented respectively, then it is big there is volume is occupied, it is real The Practical Project problem of dress property difference.On this basis, it is to adapt to electronics miniaturization and lightweight requirements, outside steam is close Electromagnetic shield Integrated manufacture composite integrated on the inside of Feng Tihe, formed a kind of water vapor seal that can realize electronic equipment and The electromagnetic leakage of electronic equipment is occurred " closed shield pad " that energy plays attenuation.It is this to possess compact-sized, dimension " the closed shield pad " that repairing property is good, real equipment is good, applied to non-tight cabinet, cabinet electromagnetic armouring structure in when, be located at Electromagnetic shielding on the inside of cabinet, cabinet know from experience be subject to from cabinet, interior of equipment cabinet electrolyte infiltrated, soaked, impregnated, will also lead Send a telegraph the galvanic corrosion of magnet shielding structure.Therefore, this " closed shield pad " is only capable of solving the small electricals such as permanent seal module The water vapor seal of sub- equipment and electromagnetic shielding environmental suitability problem, it is impossible to solve non-tight cabinet, the electricity of cabinet electronic equipment Magnetic screen and environmental suitability problem.
The content of the invention
To meet cabinet, cabinet electronic equipment Electro Magnetic Compatibility and environmental suitability requirement, the purpose of the present invention is be directed to It can not achieve conductive rubber pad water vapor seal existing for the single conductive rubber pad of the prior art, closed shield pad and cause machine The shortcoming of galvanic corrosion occurs for electromagnetic armouring structure in case, cabinet electronic equipment, and it is strong to provide a kind of resistance to corrosion, electromagnetism Shield effectiveness is high, and compact-sized small, the reliability high life is long, itself can realize that the anti-galvanic couple of conductive rubber cushion water vapor seal is rotten Erosion electromagnetic shielding seal trim strip, to solve the cabinet, the cabinet electronics that come using single conductive rubber pad or closed shield cushioning strip The generality engineering problem of galvanic corrosion existing for installation electromagnetical shielding construction.
To achieve the above object, it is provided by the invention it is a kind of prepare anti-galvanic corrosion electromagnetic shielding seal trim strip, including with Cabinet, the electromagnetic shielding seal trim strip of cabinet metallic matrix contact, it is characterised in that:The electromagnetic shielding seal trim strip is by outer The sandwich of 1 → middle level of layer electro-insulating rubber item, 2 ← primary insulation of conductive rubber strip rubber strip, 3 composite molding one, wherein, in Layer conductive rubber strip 2 press from both sides in the form of dome be connected in the formation of outer layer insulation rubber strip 1 and primary insulation rubber strip 3 groove it Between, middle level conductive rubber strip 2 realizes cabinet, the electromagnetic shielding of cabinet electronic equipment metallic matrix contact, outer layer insulation rubber strip 1 Cabinet, cabinet are realized with the elastic extruded channels of the dome item and its formation of primary insulation rubber strip 3 and middle level conductive rubber strip 2 Itself water vapor seal of electronic equipment metallic matrix contact.
A kind of method for the electromagnetic shielding seal trim strip for preparing above-mentioned anti-galvanic corrosion, has following technical characteristic:First Using high conductivity silver powder or aluminium silvering powder intermediate alloy and rubber mix, by conductivity≤3 Ω/m, insulation resistance >=300M The control intermediate alloy ingredient of Ω demands and the addition of silicon rubber are kneaded conductive rubber, and semi-solid preparation pre-molding is kneaded conductive rubber Glue;Secondly, by above-mentioned preforming semi-solid preparation conductive rubber strip be placed on the composite molding die upper mold 6 of composite molding die with In the raised line model of composite molding die lower die 7;Finally, 50 DEG C~60 DEG C, 0.5 it is small when~1.0 it is small when under the conditions of, semi-solid preparation Conductive rubber strip, will in the composite molding die upper mold 6 of composite molding die and the raised line model of composite molding die lower die 7 Outer layer insulation rubber strip 1, middle level conductive rubber strip 2 and 3 compression moulding of primary insulation rubber strip one.
Present invention conductive rubber pad single compared with the prior art and " closed shield pad " have the advantages that:
1 resistance to corrosion is strong, and electromagnet shield effect is high.The present invention uses insulation resistance >=1 He of 300M Ω outer layer insulations rubber strip Primary insulation rubber strip 3, realizes the water vapor seal to conductivity≤3 Ω/m middle levels conductive rubber strip 2, good insulation preformance, hydrophobic Property good, performance stablize.The conductive rubber of rubber and matrix homogeneity compounding rubber silver powder or the low-resistivity of aluminium silvering powder is combined into Type one forms the electromagnetic screen of 1 → middle level of outer layer insulation rubber strip, 2 ← primary insulation of conductive rubber strip rubber strip, 3 sandwich Seal trim strip is covered, reduces the active site on 2 alloy corrosion surface of middle level conductive rubber strip.
2 realize cabinet, the electromagnetic shielding of cabinet electronic equipment, and outer layer insulation rubber strip 1 and primary insulation rubber strip 3 are realized Be electromagnetically shielded middle level conductive rubber strip 2 water vapor seal of itself in seal trim strip, prevented middle level conductive rubber strip 2 and cabinet, The presence of cabinet metallic matrix contact site electrolyte, and then prevent cabinet, cabinet Electromagnetic Shield on Electronic Equipments structure galvanic couple The generation of corrosion.In cabinet, cabinet Electromagnetic Shield on Electronic Equipments in electromagnetic shielding seal trim strip realization, by controlling two outer layers 25%~30% decrement of outer layer insulation rubber strip 1 and primary insulation rubber strip 3 realizes the water to middle level conductive rubber strip 2 Steam packing has prevented electromagnetic shielding seal trim strip interlayer middle level conductive rubber strip 2 and cabinet, cabinet metallic matrix 4,5 electromagnetism Electroless liquid exists at shield gasket, lacks electrochemical reaction between middle level conductive rubber strip 2 and cabinet, cabinet metallic matrix 4,5 " electrolyte presence " necessary condition occurred, so as between interlayer middle level conductive rubber strip 2 and cabinet, cabinet metallic matrix 4,5 Galvanic corrosion do not occur, resistance to corrosion is strong;Seal trim strip interlayer middle level conductive rubber strip 2 is electromagnetically shielded by controlling 20%~25% decrement, middle level conductive rubber strip 2 and cabinet, the electrical contact of cabinet metallic matrix 4,5 are good, electromagnetic shielding Efficiency >=60dB (frequency≤10GHz), electromagnet shield effect is high, ensure that cabinet, the high shield effectiveness of cabinet electronic equipment is wanted It asks.Solve cabinet, cabinet electronic equipment electromagnetism that the prior art is come using single conductive rubber pad or closed shield cushioning strip The generality engineering problem of galvanic corrosion existing for shielding construction.
3 is compact-sized small, and the reliability high life is long.The present invention is using good insulation preformance, hydrophobicity is good, performance is stablized Rubber and matrix homogeneity compounding rubber silver powder or aluminium silvering powder low-resistivity conductive rubber composite molding one, formed outer The electromagnetic shielding seal trim strip of 1 → middle level of layer electro-insulating rubber item, 2 ← primary insulation of conductive rubber strip rubber strip, 3 sandwich.By It is identical with the rubber matrix of outer layer insulation rubber strip 1 and primary insulation rubber strip 3 in middle level conductive rubber strip 2, after composite molding The rubber matrix of outer layer insulation rubber strip 1, middle level conductive rubber strip and primary insulation rubber strip 3 integrally combines, exhausted with outer layer The technical characteristic of 1 → middle level of edge rubber strip, 2 ← primary insulation of conductive rubber strip rubber strip, 3 sandwich composite molding one, it is whole Body lear energy is strong, and this rubber extensibility is high, modulus is low, and performance is stablized, can be long-term at a temperature of -60 DEG C~180 DEG C Work 15 years or more, the reliability high life is long.It can be used safely under the conditions of salt air corrosion, disclosure satisfy that cabinet, cabinet electronics Installation electromagnetical compatibility, protective, maintainability, reliability, real equipment and cost-effectivenes.
The present invention is suitable for the room atmosphere of the different metal compatibility of metallic matrix contact, control humidity variation;It is indoor Air, humidity do not control;Outdoor weather, rural atmosphere;Outdoor weather, industry/coastal atmospheric environment;Weather in vessel cabin, sea The electromagnetic shielding liner of foreign atmospheric environment, the particularly sealing of cabinet, the electromagnetic shielding of cabinet electronic equipment and environmental protection are used Electromagnetic shielding liner.
Description of the drawings
Fig. 1 is the structure form schematic diagram of the anti-galvanic corrosion electromagnetic shielding seal trim strip of the present invention.
Fig. 2 is the sectional view of Fig. 1.
Fig. 3 is the sectional view for the electromagnetic shielding embodiment that the present invention is contacted in cabinet, cabinet metallic matrix.
Fig. 4 is present invention electromagnetic shielding seal trim strip composite molding die compression molding sectional view.
Fig. 5 is Fig. 4 composite molding die exploded views.
Fig. 6 is composite molding die upper mold bottom view.
Fig. 7 is composite molding die lower die top view.
In figure:1 outer layer insulation rubber strip, 2 middle level conductive rubber strips, 3 primary insulation rubber strips, 4 cabinets, cabinet door, 5 machines Case, cabinet, 6 composite molding die upper molds, 7 composite molding die lower dies, 8 guide pins.
Specific embodiment
Refering to Fig. 1~Fig. 2.In embodiment described below, a kind of anti-galvanic corrosion electromagnetic shielding liner, by outer Layer electro-insulating rubber item 1, middle level conductive rubber strip 2, primary insulation rubber strip 3 form, it has 1 → middle level of outer layer insulation rubber strip 2 ← primary insulation of conductive rubber strip rubber strip, 3 sandwich, wherein, middle level conductive rubber strip 2 is pressed from both sides in the form of dome to be connected in outside Between the groove that layer electro-insulating rubber item 1 and primary insulation rubber strip 3 are formed, middle level conductive rubber strip 2 realizes cabinet, cabinet electronics The electromagnetic shielding of equipment metallic matrix contact, outer layer insulation rubber strip 1 and primary insulation rubber strip 3 and middle level conductive rubber strip 2 Dome item and its formation elastic extruded channels realize cabinet, cabinet electronic equipment metallic matrix contact itself steam it is close Envelope.
Refering to Fig. 3~Fig. 7.First using high conductivity silver powder or aluminium silvering powder intermediate alloy and rubber mix, by conduction The control intermediate alloy ingredient of rate≤3 Ω/m demands and the addition of silicon rubber are kneaded conductive rubber, and semi-solid preparation pre-molding mixes Refine conductive rubber strip.Meanwhile electro-insulating rubber is kneaded by the control raw rubber ingredient of insulation resistance >=300M Ω demands, semi-solid preparation is pre- Molded mixing electro-insulating rubber item;Secondly, by 1 → middle level of outer layer insulation rubber strip, 2 ← primary insulation of conductive rubber strip rubber strip 3 Above-mentioned preforming semi-solid preparation conductive rubber strip and semi-solid preparation electro-insulating rubber item are placed on composite molding die by sandwich form Composite molding die upper mold 6 and composite molding die lower die 7 raised line model in, then closed by the positioning of guide pin 8 compound Molding die upper mold 6;
Finally, 50 DEG C~60 DEG C, 0.5 it is small when~1.0 it is small when under the conditions of, vulcanize in composite molding die, semi-solid preparation conduction rubber Adhesive tape and semi-solid preparation electro-insulating rubber item are in the composite molding die upper mold 6 of composite molding die and composite molding die lower die 7 In raised line model, by outer layer insulation rubber strip 1, middle level conductive rubber strip 2 and 3 compression moulding of primary insulation rubber strip one, shape " mountain peak " being connected between outer layer insulation rubber strip 1 and primary insulation rubber strip 3 is pressed from both sides in the form of dome into middle level conductive rubber strip 2 Shape is electromagnetically shielded seal trim strip.
Intermediate alloy can add in Rare-Earth Ce, by conductivity≤3 using aluminium silvering powder as matrix alloy in the form of aluminium silvering powder It is conductive with rubber mix to prepare aluminium silvering powder-Ce intermediate alloys for the addition of Ω/m demand modeling intermediate alloy Ce ingredients Rubber.
Rare-Earth Ce can reduce the physical dimension of α and β phases in aluminium silvering powder alloy, and crystal grain thinning promotes alloying element closing Being uniformly distributed in gold reduces harmful element and the content and the porosity that are mingled with, and under the comprehensive function of above-mentioned factor, alloy is rotten The potential difference lost between each phase in surface reduces, and the active site of corrosion surface is reduced, and makes the corrosion resistance of aluminium silvering powder alloy itself It can be improved.
In embodiment described below, for the control of 2 decrement of middle level conductive rubber strip in 20%~25% scope, outer layer is exhausted Edge rubber strip 1 and the control of 3 decrement of primary insulation rubber strip are in 25%~30% scope.
Anti- galvanic corrosion electromagnetic shielding seal trim strip is installed on the electromagnetism in cabinet, cabinet Electromagnetic Shield on Electronic Equipments structure 2 decrement of middle level conductive rubber strip of shield gasket press strip is controlled in 20%~25% scope, outer layer insulation rubber strip 1 and internal layer 3 decrement of electro-insulating rubber item is controlled in 25%~30% scope.
Above-described is only the preferred embodiment of the present invention.It should be pointed out that come for those of ordinary skill in the art It says, without departing from the principle of the present invention, several modifications and improvements can also be made.

Claims (4)

1. seal trim strip is electromagnetically shielded in a kind of anti-galvanic corrosion, including the electromagnetic shielding contacted with cabinet, cabinet metallic matrix Pad, it is characterised in that:The electromagnetic shielding seal trim strip is by outer layer insulation rubber strip (1) → middle level conductive rubber strip (2) The sandwich of ← primary insulation rubber strip (3) composite molding one, wherein, middle level conductive rubber strip (2) is in the form of dome Folder is connected between the groove that outer layer insulation rubber strip (1) and primary insulation rubber strip (3) are formed, and middle level conductive rubber strip (2) is real Existing cabinet, the electromagnetic shielding of cabinet electronic equipment metallic matrix contact, outer layer insulation rubber strip (1) and primary insulation rubber strip (3) cabinet, cabinet electronic equipment metal are realized with the dome item of middle level conductive rubber strip (2) and its elastic extruded channels of formation Itself water vapor seal of substrate contact.
2. a kind of preparation method of galvanic corrosion electromagnetic shielding seal trim strip anti-according to claim 1, has following technology Feature:First using high conductivity silver powder or aluminium silvering powder intermediate alloy and rubber mix, by the control of conductivity≤3 Ω/m demands The addition of intermediate alloy ingredient and silicon rubber processed is kneaded conductive rubber, and semi-solid preparation pre-molding is kneaded conductive rubber strip;Meanwhile Electro-insulating rubber is kneaded by the control raw rubber ingredient of insulation resistance >=300M Ω demands, semi-solid preparation pre-molding is kneaded electro-insulating rubber Item;It secondly, will be above-mentioned pre- by outer layer insulation rubber strip → middle level conductive rubber strip ← primary insulation rubber strip sandwich form Shaping semi-solid preparation conductive rubber strip and semi-solid preparation electro-insulating rubber item are placed on the composite molding die upper mold (6) of composite molding die With in the raised line model of composite molding die lower die (7);Finally, 50 DEG C~60 DEG C, 0.5 it is small when~1.0 it is small when under the conditions of, half Curing conductive rubber strip and semi-solid preparation electro-insulating rubber item are in the composite molding die upper mold (6) of composite molding die and composite molding In the raised line model of lower mould (7), by outer layer insulation rubber strip (1), middle level conductive rubber strip (2) and primary insulation rubber strip (3) compression moulding one.
3. anti-galvanic corrosion electromagnetic shielding seal trim strip method according to claim 2, which is characterized in that intermediate alloy with Aluminium silvering powder is matrix alloy, Rare-Earth Ce is added in the form of aluminium silvering powder, by conductivity≤3 Ω/m demand modeling intermediate alloys Ce The addition of ingredient prepares aluminium silvering powder-Ce intermediate alloys and rubber mix conductive rubber.
4. anti-galvanic corrosion electromagnetic shielding seal trim strip method according to claim 2, which is characterized in that middle level conduction rubber Adhesive tape (2) decrement is controlled in 20%~25% scope, outer layer insulation rubber strip (1) and primary insulation rubber strip (3) decrement Control is in 25%~30% scope.
CN201711024181.1A 2017-10-27 2017-10-27 Anti- galvanic corrosion is electromagnetically shielded seal trim strip Pending CN108055818A (en)