CN107723391A - 一种真皮鞋的皮料表面光亮度的处理方法 - Google Patents
一种真皮鞋的皮料表面光亮度的处理方法 Download PDFInfo
- Publication number
- CN107723391A CN107723391A CN201711006819.9A CN201711006819A CN107723391A CN 107723391 A CN107723391 A CN 107723391A CN 201711006819 A CN201711006819 A CN 201711006819A CN 107723391 A CN107723391 A CN 107723391A
- Authority
- CN
- China
- Prior art keywords
- cladding
- rolling
- diaphragm
- cotton
- hot
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明涉及皮鞋生产技术领域,尤其是一种真皮鞋的皮料表面光亮度的处理方法,具体包括如下步骤:(1)将皮料表面通过棉麻混纺面料进行反复擦拭20‑30次;(2)在擦拭后的皮料表面均匀涂抹一层动物性油脂,动物性油脂的涂抹量控制在3g/m2以内;(3)在涂抹有动物性油脂的皮料表面覆一层保护膜,保护膜与皮料之间通过10N的压力压实;(4)在保护膜上通过热辊对皮料进行加热,皮料在热辊下的移动速度为2m/min,热辊的温度控制在40‑60℃;(5)自然冷却;(6)撕下保护膜;(7)通过涤棉混纺面料对皮料表面进行反复擦拭20‑30次;(8)在将擦拭后的皮料在通风环境下静止30min以上即可。该方法能有效的提升皮料的表面光亮度,使用效果和性能极大的提升。
Description
技术领域
本发明涉及皮鞋生产技术领域,尤其是一种真皮鞋的皮料表面光亮度的处理方法。
背景技术
现在市面上对于皮鞋的要求越来越高,尤其是如何保证皮鞋表面的光亮度已经成为皮鞋生产中的一个难题。现有的真皮皮鞋在使用一定时间后其表面暗淡,需要经常擦拭鞋油以保证一定的光亮度。
发明内容
本发明的目的是为了解决上述技术的不足而提供一种真皮鞋的皮料表面光亮度的处理方法,其能使皮料表面始终处于光亮状态,无需擦拭鞋油。
为了达到上述目的,本发明所设计的一种真皮鞋的皮料表面光亮度的处理方法,具体包括如下步骤:(1)将皮料表面通过棉麻混纺面料进行反复擦拭20-30次,其中棉麻混纺面料中棉与麻的质量比例为3:1;(2)在擦拭后的皮料表面均匀涂抹一层动物性油脂,动物性油脂的涂抹量控制在3g/m2以内;(3)在涂抹有动物性油脂的皮料表面覆一层保护膜,保护膜与皮料之间通过10N的压力压实;(4)在保护膜上通过热辊对皮料进行加热,皮料在热辊下的移动速度为2m/min,热辊的温度控制在40-60℃;(5)自然冷却;(6)撕下保护膜;(7)通过涤棉混纺面料对皮料表面进行反复擦拭20-30次,其中涤纶与棉的质量比例为3:1;(8)在将擦拭后的皮料在通风环境下静止30min以上即可。
本发明所得到的一种真皮鞋的皮料表面光亮度的处理方法,通过棉麻面料的擦拭,能使得皮料表面的微孔舒展,此时涂抹动物性油脂后进行加热,能确保油脂吸收,而后再通过涤棉的擦拭进一步促进吸收,且使其油脂在皮料内部存在更加稳定;故该方法能有效的提升皮料的表面光亮度,且长时间使用后也不会变暗淡,使用效果和性能极大的提升。
具体实施方式
下面通过实施例对本发明作进一步的描述。
实施例1:
本实施例描述的一种真皮鞋的皮料表面光亮度的处理方法,具体包括如下步骤:(1)将皮料表面通过棉麻混纺面料进行反复擦拭25次,其中棉麻混纺面料中棉与麻的质量比例为3:1;(2)在擦拭后的皮料表面均匀涂抹一层动物性油脂,动物性油脂的涂抹量控制在3g/m2以内;(3)在涂抹有动物性油脂的皮料表面覆一层保护膜,保护膜与皮料之间通过10N的压力压实;(4)在保护膜上通过热辊对皮料进行加热,皮料在热辊下的移动速度为2m/min,热辊的温度控制在50℃;(5)自然冷却;(6)撕下保护膜;(7)通过涤棉混纺面料对皮料表面进行反复擦拭30次,其中涤纶与棉的质量比例为3:1;(8)在将擦拭后的皮料在通风环境下静止30min以上即可。
实施例2:
本实施例描述的一种真皮鞋的皮料表面光亮度的处理方法,具体包括如下步骤:(1)将皮料表面通过棉麻混纺面料进行反复擦拭20次,其中棉麻混纺面料中棉与麻的质量比例为3:1;(2)在擦拭后的皮料表面均匀涂抹一层动物性油脂,动物性油脂的涂抹量控制在3g/m2以内;(3)在涂抹有动物性油脂的皮料表面覆一层保护膜,保护膜与皮料之间通过10N的压力压实;(4)在保护膜上通过热辊对皮料进行加热,皮料在热辊下的移动速度为2m/min,热辊的温度控制在60℃;(5)自然冷却;(6)撕下保护膜;(7)通过涤棉混纺面料对皮料表面进行反复擦拭25次,其中涤纶与棉的质量比例为3:1;(8)在将擦拭后的皮料在通风环境下静止30min以上即可。
Claims (1)
1.一种真皮鞋的皮料表面光亮度的处理方法,其特征是:具体包括如下步骤:(1)将皮料表面通过棉麻混纺面料进行反复擦拭20-30次,其中棉麻混纺面料中棉与麻的质量比例为3:1;(2)在擦拭后的皮料表面均匀涂抹一层动物性油脂,动物性油脂的涂抹量控制在3g/m2以内;(3)在涂抹有动物性油脂的皮料表面覆一层保护膜,保护膜与皮料之间通过10N的压力压实;(4)在保护膜上通过热辊对皮料进行加热,皮料在热辊下的移动速度为2m/min,热辊的温度控制在40-60℃;(5)自然冷却;(6)撕下保护膜;(7)通过涤棉混纺面料对皮料表面进行反复擦拭20-30次,其中涤纶与棉的质量比例为3:1;(8)在将擦拭后的皮料在通风环境下静止30min以上即可。