CN107310139A - A kind of drafting system of fluorine carbon reducing fishing line and preparation method thereof - Google Patents

A kind of drafting system of fluorine carbon reducing fishing line and preparation method thereof Download PDF

Info

Publication number
CN107310139A
CN107310139A CN201710653141.7A CN201710653141A CN107310139A CN 107310139 A CN107310139 A CN 107310139A CN 201710653141 A CN201710653141 A CN 201710653141A CN 107310139 A CN107310139 A CN 107310139A
Authority
CN
China
Prior art keywords
fishing line
reducing
finished product
heating roller
reducing fishing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201710653141.7A
Other languages
Chinese (zh)
Other versions
CN107310139B (en
Inventor
吕从慧
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Lianyun Harbour Lun Yang Monofilament Science And Technology Ltd
Original Assignee
Lianyun Harbour Lun Yang Monofilament Science And Technology Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lianyun Harbour Lun Yang Monofilament Science And Technology Ltd filed Critical Lianyun Harbour Lun Yang Monofilament Science And Technology Ltd
Priority to CN201710653141.7A priority Critical patent/CN107310139B/en
Publication of CN107310139A publication Critical patent/CN107310139A/en
Application granted granted Critical
Publication of CN107310139B publication Critical patent/CN107310139B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of drafting system of fluorine carbon reducing fishing line and preparation method thereof, including frame and the drawing-off roller group that is arranged in frame, described drawing-off roller group include heating roller and the draw roll being arranged side by side along inlet wire direction, and what heating roller was arranged on draw roll enters line side;Draw forming distance is formed between the heating roller and draw roll, the pressure regulating mechanism being additionally provided with the pressure roller for being used to compress reducing fishing line coordinated with it, frame for adjusting platen pressure is equipped with above heating roller and draw roll.The present invention is by setting heating roller and draw roll, by pressure roller by will the fishing line of reducing be pressed on heating roller and draw roll, obtain draw forming distance, realize correspondence reducing drawing-off, to ensure that the thick section and thin segment of reducing fishing line do not obtain drawing-off in the same period, corresponding draft speed and time are set, the formation problems of fluorine carbon reducing fishing line are solved well, the product quality of reducing fishing line is also improved, high-precision reducing requirement is realized.

Description

A kind of drafting system of fluorine carbon reducing fishing line and preparation method thereof
Technical field
The present invention relates to a kind of fishing line production method, the drafting system of more particularly to a kind of fluorine carbon reducing fishing line and its preparation Method.
Background technology
Reducing fishing line is as one kind of fishing line, and general length has 2.2 meters, 2.7 meters, 3.6 meters, 4.5 meters etc., actual production In, in order to improve production efficiency, the continuously elongated thick section-reducer-thin segment-reducer-thick section that is shaped to of fishing line is connected successively And, the straight line of line footpath not etc., wire drawing cuts off after terminating from midpoint, the midpoint of thin segment of thick section, forms " thick section-reducing The finished product of section-thin segment ".This fine rule system hook for becoming radial line, thick line is buckled on link tool and used.The characteristics of this line is node Pulling force is strong, and wearability is strong, and disguised strong, sensitive performance is good, and centre slightly thick portion point draws drag strong, is difficult broken string and runs fish;Taper end is fine Fine and soft soft, good concealment eats hook rate high.
Existing reducing fishing line is mainly made using nylon wire, and the proportion of nylon wire is 1.16, and it is relatively low to cut water speed, PVDF The proportion of fluorine carbon raw material is 1.76, cuts water fast, it is adaptable to the fly fishing method of reducing fishing line.
PVDF is for PA nylon raw materials, with the features such as hardness is high, toughness is big, heat transfer is fast, contraction distortion is big, If continuing to use nylon reducing fishing line equipment, because both material characters are different, production difficulty is bigger, and Draft Effect is low, and drawing-off effect is poor.
In addition, existing reducing fishing line is the water-bath drawing-off groove and the conventional drawing-off roller group arranged by extruder rear Secondary draw forming, wherein, a drawing-off is that, by controlling the draft speed of water-bath drawing-off groove to realize, and secondary drawing-off is Completed, i.e., adopted in thick section, reducer and the thin segment of fishing line using same draft speed by the drawing-off roller group of conventional arrangement Use same draft speed, this drawing-off mode easily causes thick section and can not draw away or pull open that effect is undesirable, and thin segment can be broken, special The drawing-off of fluorine carbon reducing fishing line is not suitable for, meanwhile, the drawing-off part of existing drafting machine and heating part are provided separately, Drawing-off again is first heated, at low ambient temperatures, serious influence drawing-off effect.
The content of the invention
The technical problems to be solved by the invention are that there is provided a kind of reasonable in design, structure letter in view of the shortcomings of the prior art It is single, the drafting system of the good fluorine carbon reducing fishing line of drawing-off effect.
Another technical problem to be solved by this invention is in view of the shortcomings of the prior art, there is provided one kind is reasonable in design, to lead Stretch that effect is good, the preparation method of fluorine carbon reducing fishing line.
The technical problems to be solved by the invention are realized by following technical scheme, and the present invention is a kind of fluorine carbon The drafting system of reducing fishing line, is characterized in, including frame and the drawing-off roller group being arranged in frame, described drawing-off roller group bag Include the heating roller being arranged side by side along inlet wire direction and draw roll, what heating roller was arranged on draw roll enters line side;The heating roller with Draw forming distance is formed between draw roll, the compression that is used for coordinated with it is equipped with above heating roller and draw roll and is become The pressure regulating mechanism for adjusting platen pressure is additionally provided with the pressure roller of footpath fishing line, frame.
What the technical problems to be solved by the invention can also be realized by following technical scheme, the draw forming The length of distance is 200-240mm, preferably 220 mm.
What the technical problems to be solved by the invention can also be realized by following technical scheme, described pressure is adjusted Section mechanism includes the pressure roller mounting seat being located in frame, and the pressure roller is connected by cursor with pressure roller mounting seat, cursor Rotary shaft is provided with swing arm, and the drive cylinder of swing arm is provided with frame.
What the technical problems to be solved by the invention can also be realized by following technical scheme, the drive cylinder Piston rod outer end be provided with the hinged-support that connects with swing arm.
What the technical problems to be solved by the invention can also be realized by following technical scheme, the heating roller Enter line side at least provided with two pre- hot-rollings, the outgoing line side of draw roll is provided with guide roller, and the heating roller and pre- hot-rolling are heat conduction Oiling roller.
Another technical problem to be solved by this invention is realized by following technical scheme, and the present invention is a kind of The method that fluorine carbon reducing fishing line is prepared using above-mentioned drafting system, it is characterised in that:Its step is as follows,
First fluorine carbon raw material is added in extruder and is heated, plastified, extruded, the drawing-off through water-bath drawing-off groove after extrusion, into Type is the reducing fishing line semi-finished product connected successively by thick section-reducer-thin segment-reducer, and reducing fishing line semi-finished product are through warm After blower fan heating, into the drafting system described in claim any one of 1-5;
When the thick section of reducing fishing line semi-finished product enters the heating roller of drafting system, the lower surging of pressure roller is adjusted so that pressure roller It is pressed on heating roller and draw roll, while normal inlet wire is ensured, realizes reducing fishing line semi-finished product in draw forming distance The independent drawing-off at place, meanwhile, the draw ratio between heating roller and draw roll is adjusted to 5.5-6.0, realized to reducing fishing line half The drawing-off of thick section on finished product, after 4500-5000 milliseconds of drawing-off, draw ratio is adjusted to 4.2-5.0, realize to reducing fishing line half into The drawing-off of reducer on product, after 3600-4200 milliseconds of drawing-off, draw ratio is adjusted to 3.5-3.9, realize to reducing fishing line half into The drawing-off of thin segment on product, after 5000-6000 milliseconds of drawing-off, draw ratio is adjusted to 4.2-5.0, realized to reducing fishing line semi-finished product The drawing-off of upper next reducer, 1500-2400 millisecond of drawing-off so circulates drawing-off, so as to be made by thick section-reducer-carefully The reducing fishing line finished product that section-reducer connects successively.
What the technical problems to be solved by the invention can also be realized by following technical scheme, in drafting system Drafting process, when the thick section of reducing fishing line semi-finished product enters the heating roller of drafting system, by between heating roller and draw roll Draw ratio is adjusted to 5.8, realizes the drawing-off to thick section on reducing fishing line semi-finished product, after 4700 milliseconds of drawing-off, draw ratio is adjusted To 4.6, the drawing-off to reducer on reducing fishing line semi-finished product is realized, after 4000 milliseconds of drawing-off, draw ratio is adjusted to 3.7, it is real Now to the drawing-off of thin segment on reducing fishing line semi-finished product, after 5500 milliseconds of drawing-off, draw ratio is adjusted to 4.6, realized to reducing fishing The drawing-off of next reducer on line semi-finished product, 1700 milliseconds of drawing-off, so circulates drawing-off, thus be made by thick section-reducer- The reducing fishing line finished product that thin segment-reducer connects successively.
What the technical problems to be solved by the invention can also be realized by following technical scheme, in water-bath drawing-off groove In, the draft speed of water-bath drawing-off groove is controlled after 0.70-1.00 ms/min, 800-1200 milliseconds of drawing-off, reducing fishing is made Thick section on line semi-finished product, draft speed is at the uniform velocity adjusted to 2.00-3.00 ms/min, after 600-1000 milliseconds of drawing-off, is made Reducer on reducing fishing line semi-finished product, then, draft speed is at the uniform velocity adjusted to 7.00-8.00 ms/min, drawing-off 600- After 1000 milliseconds, the thin segment on reducing fishing line semi-finished product is made, then draft speed is at the uniform velocity adjusted to 2.00-3.00 ms/min, After 1500-2000 milliseconds of drawing-off, the another reducer on reducing fishing line semi-finished product is made, drawing-off is so circulated, be made by thick section- The reducing fishing line semi-finished product that reducer-thin segment-reducer connects successively.
What the technical problems to be solved by the invention can also be realized by following technical scheme, the heating roller and The heating-up temperature of air-heater is 80-100 DEG C.
What the technical problems to be solved by the invention can also be realized by following technical scheme, the reducing drawing-off Machine is close to set with the outlet of air-heater.
What the technical problems to be solved by the invention can also be realized by following technical scheme, from thin segment and thick section Middle position cut, formed finished product, so as to complete the post processing of fluorine carbon reducing fishing line.
The present invention by setting heating roller and draw roll, by pressure roller by will the fishing line of reducing be pressed on heating roller and drawing-off On roller, obtain a segment distance as draw forming distance, realize the reducing drawing-off of correspondent section, with ensure reducing fishing line thick section and Thin segment does not obtain drawing-off in the same period, it is to avoid not enough and fine line diameter drawing-off fracture of wire the situation of thick segment drawing-off occur, according to The property of raw material of fluorine carbon and drawing-off position, set corresponding draft speed and time, fluorine carbon reducing fishing line are solved well Formation problems, also improve the product quality of reducing fishing line, and whole process uses Automatic Control, and realizing high-precision reducing will Ask.Compared with prior art, its is reasonable in design, simple in construction, easy to operate, and drawing-off effect is good, and Draft Effect is high, particularly suitable In the drawing-off using fishing line made from fluorocarbon material.
Brief description of the drawings
Fig. 1 is the structural representation of the present invention.
Embodiment
Referring to the drawings, the concrete technical scheme of the present invention is further described, in order to which those skilled in the art enters One step the present invention is understood, without constituting the limitation to its right.
Embodiment 1, reference picture 1, a kind of drafting system of fluorine carbon reducing fishing line, including frame 1 and drawing-off roller group, it is described Drawing-off roller group includes the heating roller 4 that is arranged side by side along inlet wire direction and draw roll 2, and what heating roller 4 was located at draw roll 2 enters line side, Draw forming distance 10 is formed between heating roller 4 and draw roll 2, is equipped with and matches somebody with somebody with it in the top of heating roller 4 and draw roll 2 The pressure roller 3 of the tight reducing fishing line of combined pressure, is provided with the pressure regulating mechanism of pressure roller 3 in frame 1.
Embodiment 2, the drafting system of the fluorine carbon reducing fishing line described in embodiment 1, the length of the draw forming distance 10 For 200-240mm, preferably 220 mm.
Embodiment 3, the drafting system of the fluorine carbon reducing fishing line described in embodiment 1, described pressure regulating mechanism includes setting Pressure roller mounting seat 7 in frame 1, the pressure roller 3 is connected by cursor 5 with pressure roller mounting seat 7, the rotary shaft of cursor 5 Swing arm 6 is provided with, the drive cylinder 8 of swing arm 6 is provided with frame 1.
Embodiment 4, the drafting system of the fluorine carbon reducing fishing line described in embodiment 1, the piston rod outer end of the drive cylinder 8 Provided with the hinged-support connected with swing arm 6, the heating roller 4 enters line side at least provided with two pre- hot-rollings 9, the outlet of draw roll 2 Side is provided with guide roller 11, and the heating roller 4 and pre- hot-rolling 9 are heat conduction oiling roller;
The heating roller 4 and pre- hot-rolling 9 are heat conduction oiling roller, and heating-up temperature is 60 °C -160 °C adjustable, and its function is for monofilament Preheating and insulation;
Each pressure roller 3 is pneumatic pressure roller, be can work independently, pressure adjustable can be according to computer instruction, it is ensured that reducing fishing line is being led Stretch non-slip during stress, obtain good dimensional accuracy;
The fishing line for needing reducing is entered into heating roller 4 at pre- hot-rolling 9, then come out at draw roll 2, is exported through guide roller 11, Draw forming distance 10 is set between heating roller 4 and draw roll 2, the pressure roller 3 of draw roll 2 and the top of heating roller 4 is compressed downwards, Improve the velocity of rotation of draw roll 2 so that the velocity of rotation of draw roll 2 is more than 4 speed of heating roller, by fishing line in draw forming Drawing-off is obtained at distance 10, the change path position of fishing line so can be strictly controlled and become electrical path length, improve the reducing of fluorine carbon fishing line Effect and efficiency, and in the conventional traction of outgoing line side use for entering line side, draw roll 2 of heating roller 4.
Embodiment 5, the method that drafting system described in a kind of use embodiment 1-4 prepares fluorine carbon reducing fishing line, its step is such as Under, its step is as follows, and its step is as follows,
First fluorine carbon raw material is added in extruder and is heated, plastified, extruded, water-bath drawing-off groove is entered after extrusion, by water-bath The draft speed of drawing-off groove is controlled after 0.70 m/min, 800 milliseconds of drawing-off, and the thick section on reducing fishing line semi-finished product is made, will Draft speed is at the uniform velocity adjusted to 2.00 ms/min, after 600 milliseconds of drawing-off, and the reducer on reducing fishing line semi-finished product is made, connects , draft speed at the uniform velocity adjusted to 7.00 ms/min, after 600 milliseconds of drawing-off, the thin segment on reducing fishing line semi-finished product is made, Draft speed is at the uniform velocity adjusted again to 2.00 ms/min, after 1500 milliseconds of drawing-off, the another change on reducing fishing line semi-finished product is made Footpath section, so circulates drawing-off, and the reducing fishing line semi-finished product connected successively by thick section-reducer-thin segment-reducer are made, After reducing fishing line semi-finished product are heated through air-heater, into above-mentioned drafting system;
When the thick section of reducing fishing line semi-finished product enters the heating roller of drafting system, the lower surging of pressure roller is adjusted so that pressure roller It is pressed on heating roller and draw roll, while normal inlet wire is ensured, realizes reducing fishing line semi-finished product in draw forming distance The independent drawing-off at place, meanwhile, the draw ratio between heating roller and draw roll is adjusted to 5.5, realized to reducing fishing line semi-finished product The drawing-off of upper thick section, after 4500 milliseconds of drawing-off, draw ratio is adjusted to 4.2, realized to reducer on reducing fishing line semi-finished product Drawing-off, after 3600 milliseconds of drawing-off, draw ratio is adjusted to 3.5, the drawing-off to thin segment on reducing fishing line semi-finished product, drawing-off is realized After 5000 milliseconds, draw ratio is adjusted to 4.2, the drawing-off to next reducer on reducing fishing line semi-finished product, drawing-off is realized 1500 milliseconds, drawing-off is so circulated, so that the reducing fishing line connected successively by thick section-reducer-thin segment-reducer is made Finished product, then cut from the middle position of thin segment and thick section, so as to complete the post processing of fluorine carbon reducing fishing line.
Embodiment 6, the method that drafting system described in a kind of use embodiment 1-4 prepares fluorine carbon reducing fishing line, its step is such as Under, its step is as follows, and its step is as follows,
First fluorine carbon raw material is added in extruder and is heated, plastified, extruded, water-bath drawing-off groove is entered after extrusion, by water-bath The draft speed of drawing-off groove is controlled after 1.00 ms/min, 1200 milliseconds of drawing-off, and the thick section on reducing fishing line semi-finished product is made, Draft speed is at the uniform velocity adjusted to 3.00 ms/min, after 1000 milliseconds of drawing-off, the reducer on reducing fishing line semi-finished product is made, Then, draft speed is at the uniform velocity adjusted to 8.00 ms/min, after 1000 milliseconds of drawing-off, is made thin on reducing fishing line semi-finished product Section, then draft speed is at the uniform velocity adjusted to 3.00 ms/min, after 2000 milliseconds of drawing-off, it is made on reducing fishing line semi-finished product again One reducer, so circulates drawing-off, be made the reducing fishing line half that is connected successively by thick section-reducer-thin segment-reducer into Product, after reducing fishing line semi-finished product are heated through air-heater, into above-mentioned drafting system;
When the thick section of reducing fishing line semi-finished product enters the heating roller of drafting system, the lower surging of pressure roller is adjusted so that pressure roller It is pressed on heating roller and draw roll, meanwhile, the draw ratio between heating roller and draw roll is adjusted to 6.0, realized to reducing The drawing-off of thick section on fishing line semi-finished product, after 5000 milliseconds of drawing-off, draw ratio is adjusted to 5.0, realized to reducing fishing line semi-finished product The drawing-off of upper reducer, after 4200 milliseconds of drawing-off, draw ratio is adjusted to 3.9, realized to thin segment on reducing fishing line semi-finished product Drawing-off, after 6000 milliseconds of drawing-off, draw ratio is adjusted to 5.0, realization is led to next reducer on reducing fishing line semi-finished product Stretch, 2400 milliseconds of drawing-off so circulates drawing-off, connected successively by thick section-reducer-thin segment-reducer so as to be made Reducing fishing line finished product, then cut from the middle position of thin segment and thick section, so as to complete the post processing of fluorine carbon reducing fishing line.
Embodiment 7, the method that drafting system described in a kind of use embodiment 1-4 prepares fluorine carbon reducing fishing line, its step is such as Under, its step is as follows, and its step is as follows,
First fluorine carbon raw material is added in extruder and is heated, plastified, extruded, water-bath drawing-off groove is entered after extrusion, by water-bath The draft speed of drawing-off groove is controlled after 0.90 m/min, 1000 milliseconds of drawing-off, and the thick section on reducing fishing line semi-finished product is made, Draft speed is at the uniform velocity adjusted to 2.66 ms/min, after 990 milliseconds of drawing-off, the reducer on reducing fishing line semi-finished product is made, connects , draft speed at the uniform velocity adjusted to 7.50 ms/min, after 990 milliseconds of drawing-off, the thin segment on reducing fishing line semi-finished product is made, Draft speed is at the uniform velocity adjusted again to 2.50 ms/min, after 1700 milliseconds of drawing-off, the another change on reducing fishing line semi-finished product is made Footpath section, so circulates drawing-off, and the reducing fishing line semi-finished product connected successively by thick section-reducer-thin segment-reducer are made, After reducing fishing line semi-finished product are heated through air-heater, into above-mentioned drafting system;
When the thick section of reducing fishing line semi-finished product enters the heating roller of drafting system, the lower surging of pressure roller is adjusted so that pressure roller It is pressed on heating roller and draw roll, meanwhile, the draw ratio between heating roller and draw roll is adjusted to 5.8, realized to reducing The drawing-off of thick section on fishing line semi-finished product, after 4700 milliseconds of drawing-off, draw ratio is adjusted to 4.6, realized to reducing fishing line semi-finished product The drawing-off of upper reducer, after 4000 milliseconds of drawing-off, draw ratio is adjusted to 3.7, realized to thin segment on reducing fishing line semi-finished product Drawing-off, after 5500 milliseconds of drawing-off, draw ratio is adjusted to 4.6, realization is led to next reducer on reducing fishing line semi-finished product Stretch, 1700 milliseconds of drawing-off so circulates drawing-off, connected successively by thick section-reducer-thin segment-reducer so as to be made Reducing fishing line finished product, then cut from the middle position of thin segment and thick section, so as to complete the post processing of fluorine carbon reducing fishing line.
Embodiment 8, the method described in embodiment 5-7, the heating-up temperature of the heating roller and air-heater is 80 DEG C.
Embodiment 9, the method described in embodiment 5-7, the heating-up temperature of the heating roller and air-heater is 150 DEG C.
Embodiment 10, the method described in embodiment 5-7, the heating-up temperature of the heating roller and air-heater is 120 DEG C.
Embodiment 11, the method described in embodiment 5-7, the reducing drafting machine is close to set with the outlet of air-heater.
Whole reducing fishing line is cut into some by embodiment 12, the method described in embodiment 5-7 from the middle position of thin segment Root line segment, so as to complete the post processing of fluorine carbon reducing fishing line.
Through testing, reducing fishing line is prepared using the method described in embodiment 5-7 respectively, under relatively, described in embodiment 7 The drawing-off reducing effect of fluorine carbon line produced of method and reducing uniformity it is good, production efficiency, speed is fast.
The present invention is by after first time is shaped to reducing fishing line, then selects at draw forming distance different drawing-offs Than realizing second of drawing-off of reducing fishing line product, shaping efficiency is high, good forming effect;The present invention is using Automatic Control system System operation, by on-line dynamic measurement line footpath, computer system automatically controls and adjusted drawing-off according to that can compile input data, correspondence Speed, realizes high-precision reducing requirement;The draw forming distance of drafting machine of the present invention(I.e. in heating roller and draw roll The heart away from)Control is within 0.5 meter, preferably 0.2-0.24 meters, more preferably 0.22 meter, to ensure the thick section and thin segment of reducing fishing line not Drawing-off is obtained in the same period, it is to avoid not enough and fine line diameter drawing-off fracture of wire the situation of thick segment drawing-off occur, the present invention is very well Ground solves the formation problems of PVDF reducing fishing lines, can be used for the drawing-off of PA reducing fishing lines.

Claims (10)

1. a kind of drafting system of fluorine carbon reducing fishing line, it is characterised in that:Including frame and the drawing-off roller group being arranged in frame, Described drawing-off roller group includes heating roller and the draw roll being arranged side by side along inlet wire direction, and heating roller is arranged on the inlet wire of draw roll Side;Draw forming distance is formed between the heating roller and draw roll, is equipped with and it above heating roller and draw roll The pressure regulating mechanism for adjusting platen pressure is additionally provided with the pressure roller for being used to compress reducing fishing line coordinated, frame.
2. the drafting system of fluorine carbon reducing fishing line according to claim 1, it is characterised in that:The draw forming distance Length is 200-240mm.
3. the drafting system of fluorine carbon reducing fishing line according to claim 1, it is characterised in that:Described pressure regulating mechanism Including the pressure roller mounting seat being located in frame, the pressure roller is connected by cursor with pressure roller mounting seat, the rotary shaft of cursor Swing arm is provided with, the drive cylinder of swing arm is provided with frame.
4. the drafting system of fluorine carbon reducing fishing line according to claim 3, it is characterised in that:The piston of the drive cylinder Bar outer end is provided with the hinged-support connected with swing arm.
5. the drafting system of fluorine carbon reducing fishing line according to claim 1, it is characterised in that:The heating roller enters line side At least provided with two pre- hot-rollings, the outgoing line side of draw roll is provided with guide roller, and the heating roller and pre- hot-rolling are heat conduction oiling roller.
6. the method that the drafting system described in a kind of use claim any one of 1-5 prepares fluorine carbon reducing fishing line, its feature exists In:Its step is as follows,
First fluorine carbon raw material is added in extruder and is heated, plastified, extruded, the drawing-off through water-bath drawing-off groove after extrusion, into Type is the reducing fishing line semi-finished product connected successively by thick section-reducer-thin segment-reducer, and reducing fishing line semi-finished product are through warm After blower fan heating, into the drafting system described in claim any one of 1-5;
When the thick section of reducing fishing line semi-finished product enters the heating roller of drafting system, the lower surging of pressure roller is adjusted so that pressure roller It is pressed on heating roller and draw roll, meanwhile, the draw ratio between heating roller and draw roll is adjusted to 5.5-6.0, realization pair The drawing-off of thick section on reducing fishing line semi-finished product, after 4500-5000 milliseconds of drawing-off, draw ratio is adjusted to 4.2-5.0, realized to becoming The drawing-off of reducer on the fishing line semi-finished product of footpath, after 3600-4200 milliseconds of drawing-off, draw ratio is adjusted to 3.5-3.9, realized to becoming The drawing-off of thin segment on the fishing line semi-finished product of footpath, after 5000-6000 milliseconds of drawing-off, draw ratio is adjusted to 4.2-5.0, realized to reducing The drawing-off of next reducer on fishing line semi-finished product, 1500-2400 milliseconds of drawing-off, so circulates drawing-off, thus be made by thick section- The reducing fishing line finished product that reducer-thin segment-reducer connects successively.
7. method according to claim 6, it is characterised in that:In the drafting process of drafting system, when reducing fishing line half into When the thick section of product enters the heating roller of drafting system, the draw ratio between heating roller and draw roll is adjusted to 5.8, realized to becoming The drawing-off of thick section on the fishing line semi-finished product of footpath, after 4700 milliseconds of drawing-off, draw ratio is adjusted to 4.6, realize to reducing fishing line half into The drawing-off of reducer on product, after 4000 milliseconds of drawing-off, draw ratio is adjusted to 3.7, realized to thin segment on reducing fishing line semi-finished product Drawing-off, after 5500 milliseconds of drawing-off, draw ratio is adjusted to 4.6, realized to next reducer on reducing fishing line semi-finished product Drawing-off, 1700 milliseconds of drawing-off, so circulates drawing-off, is connected formed successively by thick section-reducer-thin segment-reducer so as to be made Reducing fishing line finished product.
8. method according to claim 6, it is characterised in that:In water-bath drawing-off groove, by the drawing-off speed of water-bath drawing-off groove After 0.70-1.00 ms/min, 800-1200 milliseconds of drawing-off the thick section on reducing fishing line semi-finished product is made, by drawing-off in degree control Speed is at the uniform velocity adjusted to 2.00-3.00 ms/min, after 600-1000 milliseconds of drawing-off, and the reducing on reducing fishing line semi-finished product is made Section, then, draft speed is at the uniform velocity adjusted to 7.00-8.00 ms/min, after 600-1000 milliseconds of drawing-off, and reducing fishing line is made Thin segment on semi-finished product, then draft speed is at the uniform velocity adjusted to 2.00-3.00 ms/min, after 1500-2000 milliseconds of drawing-off, system The another reducer on reducing fishing line semi-finished product is obtained, drawing-off is so circulated, is made by thick section-reducer-thin segment-reducer successively The reducing fishing line semi-finished product connected.
9. method according to claim 6, it is characterised in that:The heating-up temperature of the heating roller and air-heater is 80-100 DEG C, the heating roller of the drafting system is close to set with the outlet of air-heater.
10. method according to claim 6, it is characterised in that:Cut, formed into from the middle position of thin segment and thick section Product, so as to complete the post processing of fluorine carbon reducing fishing line.
CN201710653141.7A 2017-08-02 2017-08-02 A kind of preparation method of fluorine carbon variable diameter fishing line Active CN107310139B (en)