[go: up one dir, main page]
More Web Proxy on the site http://driver.im/

CN105549279B - Improve the method for the grey jump of display panel display - Google Patents

Improve the method for the grey jump of display panel display Download PDF

Info

Publication number
CN105549279B
CN105549279B CN201610109506.5A CN201610109506A CN105549279B CN 105549279 B CN105549279 B CN 105549279B CN 201610109506 A CN201610109506 A CN 201610109506A CN 105549279 B CN105549279 B CN 105549279B
Authority
CN
China
Prior art keywords
display
display panel
analog parameter
width
jump
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201610109506.5A
Other languages
Chinese (zh)
Other versions
CN105549279A (en
Inventor
李会
林允植
崔贤植
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BOE Technology Group Co Ltd
Original Assignee
BOE Technology Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BOE Technology Group Co Ltd filed Critical BOE Technology Group Co Ltd
Priority to CN201610109506.5A priority Critical patent/CN105549279B/en
Publication of CN105549279A publication Critical patent/CN105549279A/en
Application granted granted Critical
Publication of CN105549279B publication Critical patent/CN105549279B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of methods for improving the grey jump of display panel display.The display panel includes pixel electrode and public electrode, and both for strip, the method for improving the grey jump of display panel display includes:S1, sets multigroup analog parameter, and the analog parameter includes the width of pixel electrode and the width of public electrode;S2 under the conditions of every group of analog parameter, tests the display ash jump of display panel;S3, under the conditions of determining each group analog parameter, whether the display ash jump of display panel meets the requirements;If definitive result meets the requirements for the display ash jump of display panel in step S3, display panel is prepared according to satisfactory one or more groups of analog parameters;If definitive result is undesirable for the display ash jump of display panel under the conditions of multigroup analog parameter in step S3, analog parameter is reset, repeats step S1~S3.The above method can improve the display ash jump of display panel, improve and show homogeneity.

Description

Improve the method for the grey jump of display panel display
Technical field
The present invention relates to display technology fields, and in particular, to a kind of method for improving the grey jump of display panel display.
Background technology
In display device, for example, TFT-LCD and AMOLED display panels, including multiple electrodes and thin film transistor (TFT) Deng, grid, gate insulator, active layer, source electrode and drain electrode in the electrode and thin film transistor (TFT) etc. respectively be located at difference Layer, so that display device has multilayered structure.When forming every layer structure of display device, generally by depositing, sputtering Method forms a specified material layer, is then exposed, developed using mask plate, and passes through etching to make the specified material layer figure Case, so as to form a layer structure.
In actual fabrication process, due to the size of each layer structure, pattern density difference and other factors, pass through above-mentioned structure Each layer structure that figure technique is formed generally can there are some process deviations.It is strip with pixel electrode and public electrode Exemplified by TFT-LCD, the process deviation of strip pixel electrode and strip public electrode is typically implemented between CD bias and every layer The overlapping surplus (overlay margin) of mask, these process deviations can cause each display area of TFT-LCD, and there are grayscale Difference influences to show homogeneity.
The content of the invention
It is contemplated that at least solving one of technical problem in the prior art, propose that a kind of improvement display panel is shown Show the method for grey jump, the display ash jump of display panel can be improved, improve and show homogeneity.
Purpose to realize the present invention and a kind of method for improving the grey jump of display panel display is provided, the display panel Including pixel electrode and public electrode, and the pixel electrode and public electrode are strip, and the improvement display panel is shown The method of grey jump includes:
S1, sets multigroup analog parameter, and the analog parameter includes the width of pixel electrode and the width of public electrode;
S2 under the conditions of every group of analog parameter, tests the display ash jump of the display panel;
S3, under the conditions of determining each group analog parameter, whether the display ash jump of the display panel meets the requirements;
If definitive result meets the requirements for the display ash jump of display panel in step S3, according to described satisfactory One or more groups of analog parameters prepare display panel;
If definitive result does not meet for the display ash jump of display panel under the conditions of multigroup analog parameter and wants in step S3 It asks, then resets analog parameter, repeat step S1~S3.
Wherein, the difference between the width of pixel electrode in multigroup analog parameter and the width of public electrode is not It is identical.
Wherein, in multigroup analog parameter, the number of the difference between the width of pixel electrode and the width of public electrode Amount is less than the quantity of analog parameter group.
Wherein, multigroup analog parameter is divided into multiple subsets, and each subset includes at least two groups of analog parameters;Per height Difference between the width of pixel electrode of each group analog parameter of concentration and the width of public electrode is identical.
Wherein, in step s3, if identical multigroup of difference between the width of pixel electrode and the width of public electrode The display ash jump of display panel under the conditions of analog parameter meets the requirements, then according to common in multigroup analog parameter condition The width of pixel electrode and the width of public electrode between difference prepare display panel.
Wherein, after step s 3, if in multigroup analog parameter, institute's definitive result is aobvious under the conditions of having n group analog parameters Show that the display ash jump of panel meets the requirements, and the width of pixel electrode and the width of public electrode in the n group analog parameter conditions Difference between degree differs, and n >=1 then carries out following step:
S4 is once again set up multigroup analog parameter, and multigroup analog parameter is divided into n subset, is simulated respectively with above-mentioned n groups Parameter corresponds to;Each subset includes at least one set of analog parameter, and the width of pixel electrode and public affairs wherein in each group analog parameter The width of pixel electrode and public electrode in difference one group of analog parameter corresponding with the subset between the width of common electrode Difference between width is identical;
S5 under the conditions of every group of analog parameter of each subset, tests the display ash jump of display panel;
S6, under the conditions of determining each group analog parameter, whether the display ash jump of the display panel meets the requirements;
If in step S6, at least one subset, it includes each group analog parameter under the conditions of, institute's definitive result be display The display ash jump of panel meets the requirements, then according to the width of pixel electrode under the conditions of each group analog parameter at least one subset Difference between degree and the width of public electrode prepares display panel;
If in step S6, in each subset if there is at least one set of analog parameter under the conditions of, institute's definitive result be display surface The display ash jump of plate is undesirable, then records the satisfactory mould of display ash jump that can make display panel in the subset Intend parameter group and one group of analog parameter corresponding with the subset, and display panel is prepared according to the analog parameter group recorded.
Wherein, in step S4, the quantity of the analog parameter group in each subset is not less than 3.
Wherein, in the pixel of the display panel, each strip public electrode is located between two strip pixel electrodes, and The spacing of two strip pixel electrodes of itself and this in the horizontal direction differs.
Wherein, each pixel of the display panel is double domain structures.
Wherein, in each pixel of the display panel, double domain structures are set gradually along the first direction to second direction;And Strip public electrode in a farmland in a first direction and the strip pixel electrode positioned at the strip public electrode first direction it Between spacing be equal to strip public electrode in another farmland of second direction with positioned at the strip public electrode second direction Spacing between strip pixel electrode and, strip public electrode in a farmland in a first direction with it is public positioned at the strip Spacing between the strip pixel electrode of electrode second direction be equal to strip public electrode in another farmland of second direction with Spacing between the strip pixel electrode of the strip public electrode first direction.
Wherein, the grey jump of satisfactory display is less than or equal to 3.
The invention has the advantages that:
The method provided by the invention for improving the grey jump of display panel display, by setting multigroup analog parameter, is tested The display ash jump of display panel under the conditions of multigroup analog parameter determines if to meet the requirement for showing homogeneity, can be with Obtaining can make the grey jump of display of display panel meet the width of pixel electrode and public electrode when showing uniformity requirements Width or the difference in further preferred scheme between the width of acquisition pixel electrode and the width of public electrode, so as to According between the width of the width or pixel electrode of the width of the pixel electrode and public electrode and the width of public electrode Difference prepares display panel, and the display ash jump that can make prepared display panel is smaller, so as to improve display panel Show homogeneity.
Description of the drawings
Attached drawing is for providing a further understanding of the present invention, and a part for constitution instruction, with following tool Body embodiment is together for explaining the present invention, but be not construed as limiting the invention.In the accompanying drawings:
Fig. 1 is the flow chart for the method for improving the grey jump of display panel display in the embodiment of the present invention 1;
Fig. 2 is the schematic diagram of display panel;
Fig. 3 is the display ash jump of display panel under the conditions of the 1st~3 group of analog parameter;
Fig. 4 is the display ash jump of display panel under the conditions of the 4th~7 group of analog parameter;
Fig. 5 is the display ash jump of display panel under the conditions of the 8th~9 group of analog parameter;
Fig. 6 is the flow chart for the method for improving the grey jump of display panel display in the embodiment of the present invention 4;
Fig. 7 is the schematic diagram of double domain structures of display panel pixel.
Wherein, reference numeral:
10:Pixel electrode;11:Public electrode.
Specific embodiment
The specific embodiment of the present invention is described in detail below in conjunction with attached drawing.It should be appreciated that this place is retouched The specific embodiment stated is merely to illustrate and explain the present invention, and is not intended to limit the invention.
The present invention provides a kind of display panel that improves and shows the method for grey jump, and provides embodiments thereof.Specifically, exist In 1st embodiment (hereinafter referred to as embodiment 1) of the method for improving the grey jump of display panel display, such as Fig. 1 and Fig. 2 institutes Show, the display panel includes pixel electrode 10 and public electrode 11, and the pixel electrode 10 and public electrode 11 are item Shape.And the method for improving the grey jump of display panel display comprises the following steps S1~S3.
Step S1, sets multigroup analog parameter, and the analog parameter includes the width of pixel electrode and the width of public electrode Degree.
Specifically, using the width of public electrode as W1, the width of pixel electrode is W2, in step S1, is set multigroup Analog parameter;For example, 9 groups of analog parameters shown in following form.Below to set 9 groups described in following form in step sl Embodiments of the present invention are described in detail exemplified by analog parameter.
9 groups of analog parameters that table 1 is set
As above described in form, above-mentioned 9 groups of analog parameters are set in the case where craft precision is 8 μm.
S2 under the conditions of every group of analog parameter, tests the display ash jump of the display panel.
Specifically, according to the display ash jump of the 9 groups of analog parameters set in step S1, respectively test display panel, institute State test result as seen in figures 3-5, wherein, the test result of the 1st~3 group of analog parameter is shown in figure 3, the 4th~7 group of mould The test result for intending parameter shows that in Fig. 4 the test result of the 8th~9 group of analog parameter is shown in Figure 5.
S3, under the conditions of determining each group analog parameter, whether the display ash jump of the display panel meets the requirements.
Specifically, the grey jump of display for setting display panel shows the condition of uniformity requirements no more than 3 for satisfaction.Such as figure Shown in 3, in the 1st~3 group of analog parameter, in the range of fabrication error (CD bias) is ± 0.5 μm, only in the 1st group of mould Intend under Parameter Conditions, the display ash jump of display panel meets the requirements no more than 3;And the 2nd group and the 3rd group of analog parameter condition Under, the display ash jump of display panel is all higher than 3, and therefore, 2 groups of analog parameters are undesirable.As shown in figure 4, the 4th~ Under the conditions of 7 groups of analog parameters, in the range of fabrication error is ± 0.5 μm, the display ash jump of display panel is all higher than 3, because This, 4 groups of analog parameters are undesirable.As shown in figure 5, under the conditions of the 8th group of analog parameter, fabrication error for ± In the range of 0.5 μm, the display ash jump of display panel is more than 3, and therefore, the 8th group of analog parameter is undesirable;9th group of mould Intend under Parameter Conditions, in the range of fabrication error is ± 0.5 μm, the display ash jump of display panel is no more than 3, therefore, the 9th Group analog parameter meets the requirements.
According to above-mentioned analysis, when craft precision is 8 μm, in the range of fabrication error is ± 0.5 μm, at the 1st group and the 9th The grey jump of display of display panel under the conditions of group analog parameter meets the requirement of display homogeneity, it is to be understood that herein In the case of, according to the 1st group and the 9th group of analog parameter, display panel is prepared, i.e., is 1.6 μm according to the width W1 of public electrode, as The width of plain electrode W2 is 2.6 μm or is 2.1 μm according to the width of public electrode W1, and the width of pixel electrode W2 is 3.1 μm Display panel is prepared, then the display ash jump for the display panel prepared can be not more than 3, disclosure satisfy that the display homogeneity of setting Condition, so that display panel has good display homogeneity.
, whereas if under the conditions of above-mentioned 9 groups of analog parameters, the display ash jump of display panel is all higher than 3, then namely It says, the display panel that any group of analog parameter in above-mentioned 9 groups is prepared, shows that grey jump can be more than 3, so as to The requirement for meeting display homogeneity is difficult to, at this moment, it is necessary to reset analog parameter, test the analog parameter of the reset Whether meet the requirements.
In short, in step s3, if under the conditions of having at least one set of analog parameter, definitive result is grey for the display of display panel Jump meets display uniformity requirements, then prepares display panel according to satisfactory one or more groups of analog parameters;If Definitive result is undesirable for the display ash jump of display panel under the conditions of multigroup analog parameter, then needs to reset mould Intend parameter, repeat step S1~S3, uniformity requirements are shown until obtaining and can meet the grey jump of display of display panel Analog parameter.
Specifically, in embodiment 1, the width W2 of pixel electrode and the width of public electrode in multigroup analog parameter Difference between degree W1 differs.Usually, the difference between W2 and W1 for display panel display ash jump have compared with It is big to influence, that is to say, that as long as W2-W1 is certain numerical value, the numerical value of W2 and W1 can free floating within the specific limits, And some or several special values are not limited to, it can meet the grey jump of display of display panel and show wanting for homogeneity It asks.Therefore, above-mentioned setting can make the quantity of the difference between W2 and W1 in multigroup analog parameter most, for example, 10 groups of simulations In parameter, the difference between W2 and W1 differs, and the quantity for alloing the numerical value of W2-W1 is 10.Such effect is energy It is enough to increase the satisfactory probability of display ash jump for making display panel in multigroup analog parameter, so as to reduce simulation The quantity of parameter group thus reduces and the consumed process time is tested in step S2;It more meets the requirements alternatively, obtaining Analog parameter group, so as to when preparing display panel, can have the process choice scope of bigger;Or repetition can be reduced The probability of step S1~S3, in this embodiment it is not even necessary to repeat step S1~S3.
In another embodiment 2 of present embodiment, above-described embodiment 1 is different from, in multigroup analog parameter, pixel The quantity of difference between the width W2 of electrode 10 and the width W1 of public electrode 11 is less than the quantity of analog parameter group.So set For the purpose put in each group analog parameter is made, there is one or more common differences, so-called common difference in the numerical value of W2-W1 Refer to W2-W1 numerical value be equal to the common difference there are two or more group analog parameter.For example, it is enumerated in embodiment 1 upper State in 9 groups of analog parameters, there are one common differences for the 1st group of analog parameter and the 9th group of analog parameter tool --- 1 μm, and the 2nd group of mould Intend parameter then has another common difference with the 4th group of analog parameter --- and 0.5 μm, the 3rd group of analog parameter and the 5th group of simulation are joined Number has the 3rd common difference --- and 0 μm.
In another embodiment 3 of present embodiment, above-described embodiment 1 and embodiment 2, multigroup simulation ginseng are different from Number is divided into multiple subsets, and each subset includes at least two groups of analog parameters;The pixel electricity of each group analog parameter in each subset Difference between the width W2 of pole 10 and the width W1 of public electrode 11 is identical, that is to say, that each group simulation in each subset Parameter has 1 common difference.For example, in step sl, 12 groups of analog parameters are set, by 12 groups of analog parameters be divided into a, b, Tri- subsets of c, each subset include 4 groups of analog parameters, and shown in the following form of concrete numerical value of 3 groups of analog parameters:
The analog parameter for 4 subsets that table 2 is set
As shown above, 4 groups of analog parameters in a subsets, between pixel electrode width W2 and public electrode width W1 Difference W2-W1 be 0.5 μm;And 4 groups of analog parameters in b subsets, pixel electrode width W2 and public electrode width W1 Between difference W2-W1 be 0.5 μm of ﹣;And 4 groups of analog parameters in c subsets, pixel electrode width W2 and public electrode Difference W2-W1 between width W1 is 0 μm.If it is understood that under the conditions of 4 groups of analog parameters in a subsets, show Show that the grey jump of display of panel meets the requirement of display homogeneity, it, then at least can be by the verification of 4 groups of analog parameters As long as thinking to meet W2-W1=0.5 μm to a certain extent, i.e., the common difference of 4 groups of analog parameters can make display in a subsets The grey jump of display of panel meets the requirement of display homogeneity, and prepares display panel according to the common difference accordingly, makes made The display homogeneity of standby display panel meets the requirements;So can when preparing display panel, be just not limited in a subsets 4 Group technological parameter expands the scope of process choice.On the contrary, and if a are concentrated under the conditions of 1 group or multigroup analog parameter, The grey jump of display of display panel does not meet the requirement of display homogeneity, then it is assumed that the common difference of the subset can not meet display The requirement of homogeneity is, it is necessary to reset other common differences.B subsets and c subsets are similar, just repeat no more again.
In short, in above-described embodiment 2 and embodiment 3, if in step S3 pixel electrode 10 width W2 and common electrical The display ash jump of display panel under the conditions of the identical multigroup analog parameter of difference between the width W1 of pole 11 conforms to It asks, then according to the difference system between the width of pixel electrode and the width of public electrode common in multigroup analog parameter condition Standby display panel;When preparing display panel, to realize the purpose for expanding process choice scope.
In another embodiment 4 of present embodiment, above-described embodiment 1~3 is different from, it can also be real by other means Now expand the purpose of process choice scope.Specifically, as shown in fig. 6, after step s 3, in multigroup analog parameter, if its In there is institute's definitive result under the conditions of n group analog parameters to meet the requirements for the display ash jump of display panel, and the n group analog parameters Difference in condition between 11 width W1 of 10 width W2 of pixel electrode and public electrode differs, n >=1;For example, embodiment The 9 groups of analog parameters included in 1, wherein under the conditions of having 2 groups of analog parameters, the display ash jump of display panel meets display The requirement of one property, but under the conditions of 2 groups of analog parameters, the numerical value of W2-W1 is identical, it is determined that and the value of n is 1;, whereas if this 2 Under the conditions of group analog parameter, the numerical value of W2-W1 is different, that is, the value for determining n is 2;In these cases, following step S4 is carried out ~S6.
S4 is once again set up multigroup analog parameter, and multigroup analog parameter is divided into n subset, is simulated respectively with above-mentioned n groups Parameter corresponds to;Each subset includes at least one set of analog parameter, and wherein in each group analog parameter pixel electrode 10 width W2 The width W2 of pixel electrode 10 in difference one group of analog parameter corresponding with the subset between the width W1 of public electrode 11 Difference between the width W1 of public electrode 11 is identical.
S5 under the conditions of every group of analog parameter of each subset, tests the display ash jump of display panel.
S6, under the conditions of determining each group analog parameter, whether the display ash jump of the display panel meets the requirements.
If in step S6, at least one subset, it includes each group analog parameter under the conditions of, institute's definitive result be display surface The display ash jump of plate meets the requirements, as long as then can at least think that the common difference in the subset can make to a certain extent The grey jump of display of display panel meets the requirement of display homogeneity, so as to according to each group analog parameter at least one subset Under the conditions of difference between the width of pixel electrode and the width of public electrode prepare display panel.If conversely, in step S6, often Height is concentrated, and under the conditions of at least one set of analog parameter, institute's definitive result does not meet for the display ash jump of display panel It is required that then record the satisfactory analog parameter group of display ash jump that can make display panel in the subset and with the subset Corresponding one group of analog parameter, and display panel is prepared according to the analog parameter group recorded.
Preferably, each subset in step S4 includes 3 groups or more analog parameters, that is to say, that just each common poor Value, at least 4 groups of analog parameters come under the simplation verification common difference, and it is aobvious whether the display ash jump of display panel can meet Show the requirement of homogeneity, so as to improve the accuracy rate of simplation verification.
Specifically, in the pixel of the display panel, each strip public electrode 11 is located at two strip pixel electrodes 10 Between, and the spacing of two strip pixel electrodes 10 of itself and this in the horizontal direction differs, so setting preferably to avoid The influence of process deviation helps to further improve display homogeneity.In addition, each pixel of the display panel can be double farmlands Structure, as shown in fig. 7, each pixel includes two farmlands of A, B, double domain structures can improve the colour cast of pixel, improve the standard of display True property.Specifically, in each pixel of the display panel, double domain structures are set gradually along the first direction to second direction;And The strip public electrode 11 in a farmland A and the strip pixel electricity positioned at 11 first direction of strip public electrode in a first direction Spacing between pole 10 is equal to the strip public electrode 11 in another farmland B of second direction and is located at the strip public electrode 11 Spacing between the strip pixel electrode 10 of second direction and, strip public electrode 11 in a farmland A in a first direction with Spacing between the strip pixel electrode 10 of 11 second direction of strip public electrode is equal to another farmland B in second direction In strip public electrode 11 and the spacing between the strip pixel electrode 10 of 11 first direction of strip public electrode.
It is understood that the principle that embodiment of above is intended to be merely illustrative of the present and the exemplary implementation that uses Mode, however the present invention is not limited thereto.For those skilled in the art, the essence of the present invention is not being departed from In the case of refreshing and essence, various changes and modifications can be made therein, these variations and modifications are also considered as protection scope of the present invention.

Claims (11)

1. a kind of method for improving the grey jump of display panel display, the display panel include pixel electrode and public electrode, and The pixel electrode and public electrode are strip, which is characterized in that the method bag for improving the grey jump of display panel display It includes:
S1, sets multigroup analog parameter, and the analog parameter includes the width of pixel electrode and the width of public electrode;
S2 under the conditions of every group of analog parameter, tests the display ash jump of the display panel;
S3, under the conditions of determining each group analog parameter, whether the display ash jump of the display panel meets the requirements;
If definitive result meets the requirements for the display ash jump of display panel in step S3, according to described satisfactory one group Or multigroup analog parameter prepares display panel;
If definitive result is undesirable for the display ash jump of display panel under the conditions of multigroup analog parameter in step S3, Analog parameter is reset, repeats step S1~S3.
2. the method according to claim 1 for improving the grey jump of display panel display, which is characterized in that multigroup simulation Difference between the width of pixel electrode in parameter and the width of public electrode differs.
3. the method according to claim 1 for improving the grey jump of display panel display, which is characterized in that multigroup simulation In parameter, the quantity of the difference between the width of pixel electrode and the width of public electrode is less than the quantity of analog parameter group.
4. the method according to claim 1 for improving the grey jump of display panel display, which is characterized in that multigroup simulation Parameter is divided into multiple subsets, and each subset includes at least two groups of analog parameters;
The difference between the width of pixel electrode of each group analog parameter and the width of public electrode in each subset is identical.
5. the method for improving the grey jump of display panel display according to claim 3 or 4, which is characterized in that in step S3 In, if the display surface under the conditions of the identical multigroup analog parameter of difference between the width of pixel electrode and the width of public electrode The display ash jump of plate meets the requirements, then according to the width of pixel electrode common in multigroup analog parameter condition and public Difference between the width of electrode prepares display panel.
6. the method according to claim 1 for improving the grey jump of display panel display, which is characterized in that step S3 it Afterwards, if in multigroup analog parameter, institute's definitive result conforms to for the display ash jump of display panel under the conditions of having n group analog parameters It asks, and the difference in the n group analog parameter conditions between the width of pixel electrode and the width of public electrode differs, the n >=1, then carry out following step:
S4 is once again set up multigroup analog parameter, and multigroup analog parameter is divided into n subset, respectively with above-mentioned n groups analog parameter It is corresponding;Each subset includes at least one set of analog parameter, and wherein in each group analog parameter pixel electrode width and common electrical The width of pixel electrode and the width of public electrode in difference one group of analog parameter corresponding with the subset between the width of pole Between difference it is identical;
S5 under the conditions of every group of analog parameter of each subset, tests the display ash jump of display panel;
S6, under the conditions of determining each group analog parameter, whether the display ash jump of the display panel meets the requirements;
If in step S6, at least one subset, it includes each group analog parameter under the conditions of, institute's definitive result is display panel Display ash jump meet the requirements, then according to the width of pixel electrode under the conditions of each group analog parameter at least one subset with Difference between the width of public electrode prepares display panel;
If in step S6, in each subset if there is at least one set of analog parameter under the conditions of, institute's definitive result is display panel The grey jump of display is undesirable, then records the satisfactory simulation ginseng of display ash jump that can make display panel in the subset Array and one group of analog parameter corresponding with the subset, and display panel is prepared according to the analog parameter group recorded.
7. the method according to claim 6 for improving the grey jump of display panel display, which is characterized in that in step S4, often The quantity for the analog parameter group that height is concentrated is not less than 3.
8. the method according to claim 1 for improving the grey jump of display panel display, which is characterized in that the display panel Pixel in, each strip public electrode is located between two strip pixel electrodes, and two strip pixel electrodes of itself and this exist Spacing in horizontal direction differs.
9. the method for improving the grey jump of display panel display according to claim 1 or 8, which is characterized in that the display Each pixel of panel is double domain structures.
10. the method according to claim 9 for improving the grey jump of display panel display, which is characterized in that the display surface In each pixel of plate, double domain structures are set gradually along the first direction to second direction;
And strip pixel of the strip public electrode in a farmland in a first direction with being located at the strip public electrode first direction Spacing between electrode is equal to the strip public electrode in another farmland of second direction and is located at the strip public electrode second Spacing between the strip pixel electrode in direction and, strip public electrode in a farmland in a first direction with positioned at this The strip that spacing between the strip pixel electrode of shape public electrode second direction is equal in another farmland of second direction is public Electrode and the spacing between the strip pixel electrode of the strip public electrode first direction.
11. the method according to claim 1 for improving the grey jump of display panel display, which is characterized in that satisfactory The grey jump of display is less than or equal to 3.
CN201610109506.5A 2016-02-26 2016-02-26 Improve the method for the grey jump of display panel display Expired - Fee Related CN105549279B (en)