CN104829093A - Glass bottle forming mold base having cooling effect - Google Patents
Glass bottle forming mold base having cooling effect Download PDFInfo
- Publication number
- CN104829093A CN104829093A CN201510242740.0A CN201510242740A CN104829093A CN 104829093 A CN104829093 A CN 104829093A CN 201510242740 A CN201510242740 A CN 201510242740A CN 104829093 A CN104829093 A CN 104829093A
- Authority
- CN
- China
- Prior art keywords
- mould
- sides
- cavity
- vial
- glass bottle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a glass bottle forming mold base having a cooling effect. The glass bottle forming mold base having the cooling effect is characterized in that the inside of the mold base is a cavity, air outlets are formed at two sides of the cavity, an air inlet is formed at the bottom of the mold base and used for introduction of a metal hose. The bottom of the glass bottle can be cooled sufficiently, the glass bottle can be cooled uniformly and the molding rate of the product is improved.
Description
Technical field
The present invention relates to technology for making glass mould, specifically a kind of have at the bottom of the vial shaping dies mould of cooling performance.
Background technology
Vial shaping dies is made up of blank mould, mouth mould, Cheng Mo etc., and feed liquid flows in blank mould and forms blank, and then enters in mould and carry out blowing, and shaping mould is formed by becoming (i.e. bottom mould tool) combination at the bottom of mould and mould; As shown in Figure 1, the cold wind becoming mould 3 to be blown out by the cooling tuyere 4 on both sides in the process of blowing cools, and 1 become the middle part of mould 3 in both sides at the bottom of mould, be subject to into mould 3 stop cooling wind less than or seldom can blow to 1 position at the bottom of mould, 1 is so just made at the bottom of mould as shown in Figure 1a to can not get abundant cooling, thus cause at the bottom of mould 3 and mould 1 temperature unbalanced, be easily out of shape at the bottom of bottle, affect quality product and restrict the lifting of machine speed.
Summary of the invention
The present invention solves the weak point that above-mentioned prior art exists, and proposes a kind ofly to have at the bottom of the vial shaping dies mould of cooling performance, to fully at the bottom of cooled glass bottle bottle, ensureing vial cooling evenly, thus improve formed product rate.
The present invention adopts following technical scheme in order to technical solution problem:
The present invention is a kind of to be had at the bottom of the vial shaping dies mould of cooling performance, described vial shaping dies is become at the bottom of the mould of mould middle position to form with in described both sides by the both sides Cheng Mo be articulated on mould rack, and the both sides of described vial shaping dies are provided with cooling die tuyere; Carry out blowing with the one-tenth mold cavity that the both sides that the injection of vial feed liquid is closed become mould to be formed, thus obtain the shaped bottle be at the bottom of described mould; Its constructional feature is:
The inside arranged at the bottom of described mould is cavity, and the both sides of described cavity are provided with production well; Bottom at the bottom of described mould is provided with air inlet port for accessing metallic hose;
The compressed gas accessed with described metallic hose is entered in described cavity by described air inlet port, and discharges from described production well, thus forms the circulation cooling mechanism at the bottom of described shaped bottle bottle.
Compared with the prior art, beneficial effect of the present invention is embodied in:
The present invention is cavity by the inside arranged at the bottom of mould, and both sides at the bottom of mould and bottom arrange four production wells and an air inlet port respectively, compressed gas can be entered at the bottom of mould and constantly carry out circulating cooling, thus to reach at the bottom of cooling frame, solve distortion at the bottom of bottle and promote the effect of bottle speed processed.
Accompanying drawing explanation
Fig. 1 is vial shaping dies schematic diagram in prior art;
Fig. 1 a is schematic diagram at the bottom of mould in prior art;
Fig. 2 is vial shaping dies schematic diagram of the present invention;
Fig. 2 a is schematic diagram at the bottom of mould of the present invention;
Number in the figure: at the bottom of 1 mould; 1a air inlet port; 1b venting hole; 1c cavity; 2 mould bases; 3 one-tenth moulds; 3a becomes mold cavity; 3b embraces pincers; 4 cooling die tuyeres; 5 mould racks; 6 shaped bottles; 7 metallic hoses.
Embodiment
As shown in Figure 2, vial shaping dies becomes mould 3 to become at the bottom of the mould of mould 3 middle position 1 to form with in both sides by the both sides that are articulated on mould rack 5, and the both sides of vial shaping dies are provided with cooling die tuyere 4; In bottle process processed, ceaselessly blow cooling air, vial feed liquid is injected the one-tenth mold cavity 3a that closed both sides become mould 3 to be formed simultaneously and carry out blowing, thus obtain the shaped bottle 6 be at the bottom of mould on 1;
As shown in Figure 2 a, a kind of have at the bottom of the vial shaping dies mould of cooling performance, be the inside hollow out arranging at the bottom of mould 1 is cavity 1c, and retain the thickness of at the bottom of mould 1 three millimeters; At the bottom of mould, the cavity 1c arranged outside of 1 has four production well 1b; At the bottom of mould, the bottom of 1 arranges air inlet port 1a for accessing metallic hose 7, and metallic hose 7 is through to compressed gas;
Entered in cavity 1c by air inlet port 1a with the compressed gas that metallic hose 7 accesses, and discharge from production well 1b, thus form the circulation cooling mechanism at the bottom of shaped bottle 6 bottles.
Claims (1)
1. one kind has at the bottom of the vial shaping dies mould of cooling performance, described vial shaping dies by the both sides Cheng Mo (3) be articulated on mould rack (5) and at the bottom of the mould of described both sides Cheng Mo (3) middle position (1) form, the both sides of described vial shaping dies are provided with cooling die tuyere (4); Carry out blowing with the one-tenth mold cavity (3a) that the both sides Cheng Mo (3) that the injection of vial feed liquid is closed is formed, thus obtain the shaped bottle (6) be on (1) at the bottom of described mould; It is characterized in that:
The inside arranging (1) at the bottom of described mould is cavity (1c), and the both sides of described cavity (1c) are provided with production well (1b); At the bottom of described mould, the bottom of (1) is provided with air inlet port (1a) for accessing metallic hose (7);
The compressed gas accessed with described metallic hose (7) enters in described cavity (1c) by described air inlet port (1a), and discharge from described production well (1b), thus form the circulation cooling mechanism at the bottom of described shaped bottle (6) bottle.