CN104741506A - 一种铸造用粘结剂促硬剂 - Google Patents
一种铸造用粘结剂促硬剂 Download PDFInfo
- Publication number
- CN104741506A CN104741506A CN201310723223.6A CN201310723223A CN104741506A CN 104741506 A CN104741506 A CN 104741506A CN 201310723223 A CN201310723223 A CN 201310723223A CN 104741506 A CN104741506 A CN 104741506A
- Authority
- CN
- China
- Prior art keywords
- casting
- parts
- binder
- hardening accelerator
- polyvinyl alcohol
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种铸造用粘结剂促硬剂,它包括以下重量份的成分:氢氧化钙25-35份、425#水泥25-40份、水硬性材料1-5份。本发明提供的铸造用粘结剂促硬剂,氢氧化钙对CO2硬化聚乙烯醇粘结剂有着反应发热促进聚乙烯醇脱水硬化、弥散分布提高强度的特点,添加425#硅酸盐水泥对改善吸湿性和提高强度效果明显,添加的水硬性材料也对强度有明显的增强作用。通过几种粉末状促硬物质的复合,很大程度上提高了CO2硬化聚乙烯醇粘结剂的工艺强度。
Description
技术领域
本发明涉及一种促硬剂,具体涉及一种铸造用粘结剂促硬剂。
背景技术
铸造工业是一个能耗高、污染大的行业,在发展铸造业的同时,环境的保护日益重要。铸造生产中,造型材料直接影响铸件的质量,同时也是铸造生产的污染源之一。传统的冷芯盒工艺,如SO2法、三乙胺法等常采用有毒有害的气体作为催化剂或固化剂,不仅危害人体健康,也不利于绿色铸造生产。聚乙烯醇为有机高分子化合物,是一种水溶性树脂,可用做铸造粘结剂。但是,单纯使用聚乙烯醇粘结剂,湿强度低,因此需要与某些促硬剂一同使用。
发明内容
本发明的目的在于,提供一种铸造用粘结剂促硬剂,通过几种粉末状促硬物质的复合,很大程度上提高CO2硬化聚乙烯醇粘结剂的工艺强度。
所述铸造用粘结剂促硬剂,它包括以下重量份的成分:
氢氧化钙25-35份、425#水泥25-40份、水硬性材料1-5份。
本发明提供的铸造用粘结剂促硬剂,其有益效果在于,氢氧化钙对CO2硬化聚乙烯醇粘结剂有着反应发热促进聚乙烯醇脱水硬化、弥散分布提高强度的特点,添加425#硅酸盐水泥对改善吸湿性和提高强度效果明显,添加的水硬性材料也对强度有明显的增强作用。通过几种粉末状促硬物质的复合,很大程度上提高了CO2硬化聚乙烯醇粘结剂的工艺强度。
具体实施方式
下面结合一个实施例,对本发明提供的铸造用粘结剂促硬剂进行详细的说明。
实施例
所述铸造用粘结剂促硬剂,它包括以下重量份的成分:
氢氧化钙30份、425#水泥30份、水硬性材料3份。
上述铸造用粘结剂促硬剂的制备方法如下:按上述配方取氢氧化钙、425#水泥、水硬性材料,混合均匀,即得粉末状促硬剂。
Claims (1)
1.一种铸造用粘结剂促硬剂,其特征在于:它包括以下重量份的成分:
氢氧化钙25-35份、425#水泥25-40份、水硬性材料1-5份。