CN104130541A - 一种超级电容器用防爆橡胶密封胶盖 - Google Patents
一种超级电容器用防爆橡胶密封胶盖 Download PDFInfo
- Publication number
- CN104130541A CN104130541A CN201410374288.9A CN201410374288A CN104130541A CN 104130541 A CN104130541 A CN 104130541A CN 201410374288 A CN201410374288 A CN 201410374288A CN 104130541 A CN104130541 A CN 104130541A
- Authority
- CN
- China
- Prior art keywords
- explosion
- rubber
- proof rubber
- ultracapacitor
- titanium dioxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明涉及电容器技术领域,具体涉及一种超级电容器用防爆橡胶密封胶盖。其特征在于其组成原料的重量份为:高苯橡胶32-38、聚丙烯酸橡胶22-32、二氧化钛6-12、硬脂酸锌3-5、卵磷脂3-5、氧化石墨烯5-10、氧化铝5-10、茶多酚3-5、二甲基二硫代氨基甲酸锌5-10、滑石粉3-5、硫磺2-4和蒙脱土3-5。本发明制备方法简单,与现有技术相比,减少能耗,绿色环保;配方合理,制备的产品具有较好的力学性能、疲劳性能、耐老化、生热低良好综合性能,在超级电容器的外壳上安装可以有效的防止电容器的爆裂。
Description
技术领域
本发明涉及电容器技术领域,具体涉及一种超级电容器用防爆橡胶密封胶盖。
背景技术
作为一种介于传统电容器和锂离子电池之间的新型环境友好型储能体系,超级电容器具有许多其它储能器件无法比拟的优异特性,其容量可达几百甚至上千法拉,为化石能源枯竭和环境恶化等问题提供绿色解决方案。
由于超级电容器一般由电极材料、电解液、集流体和隔膜等组成,如电容器出现故障,将发生爆裂,电解液会外泄污染机器设备,并有起火的危险。寻找一种具有较好的力学性能、疲劳性能、耐老化、生热低良好综合性能防爆橡胶及其制品,一直是科学研究的重要领域。
发明内容
本发明的目的是提供一种超级电容器用防爆橡胶密封胶及其制品,以避免由于电容器出现故障导致发生爆裂,进而引起电解液外泄污染机器设备并起火。
为了解决上述问题,本发明提供的技术方案:
一种超级电容器用防爆橡胶密封胶盖,其特征在于其组成原料的重量份为:高苯橡胶32-38、聚丙烯酸橡胶22-32、二氧化钛6-12、硬脂酸锌3-5、卵磷脂3-5、氧化石墨烯5-10、氧化铝5-10、茶多酚3-5、二甲基二硫代氨基甲酸锌5-10、滑石粉3-5、硫磺2-4和蒙脱土3-5。
所述的超级电容器用防爆橡胶密封胶盖,其组成原料的重量份为:高苯橡胶35、聚丙烯酸橡胶23、二氧化钛8、硬脂酸锌4、卵磷脂4、氧化石墨烯4、氧化铝5、茶多酚3、二甲基二硫代氨基甲酸锌5、滑石粉3、硫磺2.2和蒙脱土3.8。
所述的超级电容器用防爆橡胶密封胶盖的制备方法,包括以下步骤:
(1)混炼:在密炼机中按一定重量份加入高苯橡胶、聚丙烯酸橡胶、二氧化钛、卵磷脂、滑石粉、蒙脱土和氧化石墨烯炼胶10-15分钟,保持密炼温度80-95℃,停放44-48小时;
(2)硫化:再上述混炼胶中加入硫磺、二甲基二硫代氨基甲酸锌、硬脂酸锌、混炼3-4分钟,混炼温度控制:密炼机排料90℃~110℃,密炼出料后在开炼机上返胶混炼3-5分钟,然后在压片机上压成成品。
本发明与现有技术相比,其显著优点是:本发明制备方法简单,与现有技术相比,减少能耗,绿色环保;配方合理,制备的产品具有较好的力学性能、疲劳性能、耐老化性能以及低生热性能,在超级电容器的外壳上安装可以有效的防止电容器的爆裂。
具体实施方式
下面结合附图和具体实施方式对本发明的技术方案作进一步具体说明。
实施例1
一种超级电容器用防爆橡胶密封胶盖,其组成原料的重量份为:高苯橡胶32、聚丙烯酸橡胶27、二氧化钛6、硬脂酸锌3、卵磷脂3、氧化石墨烯5、氧化铝5、茶多酚3、二甲基二硫代氨基甲酸锌5、滑石粉3、硫磺2和蒙脱土3。
所述的超级电容器用防爆橡胶密封胶盖的制备方法,包括以下步骤:
(1)混炼:在密炼机中按一定重量份加入高苯橡胶、聚丙烯酸橡胶、二氧化钛、卵磷脂、滑石粉、蒙脱土和氧化石墨烯炼胶10分钟,保持密炼温度80℃,停放44小时;
(2)硫化:再上述混炼胶中加入硫磺、二甲基二硫代氨基甲酸锌、硬脂酸锌、混炼3分钟,混炼温度控制:密炼机排料90℃,密炼出料后在开炼机上返胶混炼3分钟,然后在压片机上压成成品。
实施例2
一种超级电容器用防爆橡胶密封胶盖,其特征在于其组成原料的重量份为:高苯橡胶35、聚丙烯酸橡胶23、二氧化钛8、硬脂酸锌4、卵磷脂4、氧化石墨烯4、氧化铝5、茶多酚3、二甲基二硫代氨基甲酸锌5、滑石粉3、硫磺2.2和蒙脱土3.8。
所述的超级电容器用防爆橡胶密封胶盖的制备方法,包括以下步骤:
(1)混炼:在密炼机中按一定重量份加入高苯橡胶、聚丙烯酸橡胶、二氧化钛、卵磷脂、滑石粉、蒙脱土和氧化石墨烯炼胶15分钟,保持密炼温度95℃,停放48小时;
(2)硫化:再上述混炼胶中加入硫磺、二甲基二硫代氨基甲酸锌、硬脂酸锌、混炼4分钟,混炼温度控制:密炼机排料110℃,密炼出料后在开炼机上返胶混炼5分钟,然后在压片机上压成成品。
实施例3
一种超级电容器用防爆橡胶密封胶盖,其特征在于其组成原料的重量份为:高苯橡胶38、聚丙烯酸橡胶22、二氧化钛6.5、硬脂酸锌3.5、卵磷脂3.1、氧化石墨烯5.2、氧化铝5.1、茶多酚3.4、二甲基二硫代氨基甲酸锌5.2、滑石粉3、硫磺2和蒙脱土3。
所述的超级电容器用防爆橡胶密封胶盖的制备方法,包括以下步骤:
(1)混炼:在密炼机中按一定重量份加入高苯橡胶、聚丙烯酸橡胶、二氧化钛、卵磷脂、滑石粉、蒙脱土和氧化石墨烯炼胶12分钟,保持密炼温度805℃,停放46小时;
(2)硫化:再上述混炼胶中加入硫磺、二甲基二硫代氨基甲酸锌、硬脂酸锌、混炼3.5分钟,混炼温度控制:密炼机排料100℃,密炼出料后在开炼机上返胶混炼4分钟,然后在压片机上压成成品。
以上显示和描述了本发明的基本原理、主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。
Claims (3)
1.一种超级电容器用防爆橡胶密封胶盖,其特征在于其组成原料的重量份为:高苯橡胶32-38、聚丙烯酸橡胶22-32、二氧化钛6-12、硬脂酸锌3-5、卵磷脂3-5、氧化石墨烯5-10、氧化铝5-10、茶多酚3-5、二甲基二硫代氨基甲酸锌5-10、滑石粉3-5、硫磺2-4和蒙脱土3-5。
2.一种超级电容器用防爆橡胶密封胶盖,其特征在于其组成原料的重量份为:高苯橡胶35、聚丙烯酸橡胶23、二氧化钛8、硬脂酸锌4、卵磷脂4、氧化石墨烯4、氧化铝5、茶多酚3、二甲基二硫代氨基甲酸锌5、滑石粉3、硫磺2.2和蒙脱土3.8。
3.一种如权利要求1或2所述的超级电容器用防爆橡胶密封胶盖的制备方法,其特征在于包括以下步骤:
(1)混炼:在密炼机中按一定重量份加入高苯橡胶、聚丙烯酸橡胶、二氧化钛、卵磷脂、滑石粉、蒙脱土和氧化石墨烯炼胶10-15分钟,保持密炼温度80-95℃,停放44-48小时;
(2)硫化:再上述混炼胶中加入硫磺、二甲基二硫代氨基甲酸锌、硬脂酸锌、混炼3-4分钟,混炼温度控制:密炼机排料90℃~110℃,密炼出料后在开炼机上返胶混炼3-5分钟,然后在压片机上压成成品。