Lee et al., 2008 - Google Patents
Femtosecond laser micromilling of Si wafersLee et al., 2008
View PDF- Document ID
- 16190896440228475929
- Author
- Lee S
- Yang D
- Nikumb S
- Publication year
- Publication venue
- Applied Surface Science
External Links
Snippet
Femtosecond laser micromilling of silicon is investigated using a regeneratively amplified 775nm Ti: Sapphire laser with a pulse duration of 150fs operating at 1kHz repetition rate. The morphological observation and topological analysis of craters fabricated by single-shot …
- 235000012431 wafers 0 title description 4
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/02—Positioning or observing the workpiece, e.g. with respect to the point of impact; Aligning, aiming or focusing the laser beam
- B23K26/06—Shaping the laser beam, e.g. by masks or multi-focusing
- B23K26/062—Shaping the laser beam, e.g. by masks or multi-focusing by direct control of the laser beam
- B23K26/0626—Energy control of the laser beam
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/36—Removing material
- B23K26/40—Removing material taking account of the properties of the material involved
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/02—Positioning or observing the workpiece, e.g. with respect to the point of impact; Aligning, aiming or focusing the laser beam
- B23K26/06—Shaping the laser beam, e.g. by masks or multi-focusing
- B23K26/073—Shaping the laser spot
- B23K26/0736—Shaping the laser spot into an oval shape, e.g. elliptic shape
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/36—Removing material
- B23K26/38—Removing material by boring or cutting
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/08—Devices involving relative movement between laser beam and workpiece
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Lee et al. | Femtosecond laser micromilling of Si wafers | |
Lei et al. | Ultrafast laser applications in manufacturing processes: A state-of-the-art review | |
Liu et al. | Hybrid laser precision engineering of transparent hard materials: challenges, solutions and applications | |
Nikumb et al. | Precision glass machining, drilling and profile cutting by short pulse lasers | |
Raciukaitis et al. | Accumulation effects in laser ablation of metals with high-repetition-rate lasers | |
Mishra et al. | Laser beam micromachining (LBMM)–a review | |
Knowles et al. | Micro-machining of metals, ceramics and polymers using nanosecond lasers | |
US6995336B2 (en) | Method for forming nanoscale features | |
Rihakova et al. | Laser micromachining of glass, silicon, and ceramics | |
Qi et al. | Femtosecond laser ablation of sapphire on different crystallographic facet planes by single and multiple laser pulses irradiation | |
Cheng et al. | Effects of laser operating parameters on metals micromachining with ultrafast lasers | |
Samad et al. | Ultrashort laser pulses machining | |
Liao et al. | High quality full ablation cutting and stealth dicing of silica glass using picosecond laser Bessel beam with burst mode | |
Ngoi et al. | Effect of energy above laser-induced damage thresholds in the micromachining of silicon by femtosecond pulse laser | |
Chen et al. | Anisotropy of material removal during laser-induced plasma assisted ablation of sapphire | |
Wang et al. | Improving the quality of femtosecond laser processing micro-hole array by coated with aluminum film on fused silica sheet | |
Zhu et al. | Fabrication of oxide-free dimple structure on germanium via electrochemical jet machining enhanced by opposing laser irradiation | |
Shalini et al. | Ultrafast pulse laser inscription and surface quality characterization of micro-structured silicon wafer | |
Jiao et al. | Picosecond laser drilling of silicon with applied voltage | |
Raciukaitis et al. | Efficiency aspects in processing of metals with high-repetition-rate ultra-short-pulse lasers | |
Kononenko et al. | Optimization strategy for high-quality laser milling of silicon | |
Chen et al. | Fabrication of microstructures on glass by imprinting in conventional furnace for lab-on-chip application | |
Karnakis et al. | Comparison of glass processing using high-repetition femtosecond (800 nm) and UV (255 nm) nanosecond pulsed lasers | |
Hu et al. | Femtosecond laser modification combined with chemical etching to achieve high-quality cutting of millimeter-thick fused silica | |
Qin et al. | Process characterization of fabricating 3D micro channel systems by laser-micromachining |