Mondal et al., 2020 - Google Patents
Effect of ultrasonic shot peening on oxidation behavior of T91 and SS347 steels in air and steam at 650° CMondal et al., 2020
- Document ID
- 10554051530368959605
- Author
- Mondal D
- Chattopadhyay K
- Singh V
- Publication year
- Publication venue
- Journal of Materials Engineering and Performance
External Links
Snippet
Ultrasonic shot peening (USP) is a relatively new process of surface modification to improve mechanical properties as well as corrosion and high-temperature oxidation resistance of metallic materials. The effect of USP on surface properties and the process of high …
- 238000007254 oxidation reaction 0 title abstract description 189
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/18—Ferrous alloys, e.g. steel alloys containing chromium
- C22C38/40—Ferrous alloys, e.g. steel alloys containing chromium with nickel
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C8/00—Solid state diffusion of only non-metal elements into metallic material surfaces; Chemical surface treatment of metallic material by reaction of the surface with a reactive gas, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C8/02—Pre-treatment of the material to be coated
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C8/00—Solid state diffusion of only non-metal elements into metallic material surfaces; Chemical surface treatment of metallic material by reaction of the surface with a reactive gas, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C8/06—Solid state diffusion of only non-metal elements into metallic material surfaces; Chemical surface treatment of metallic material by reaction of the surface with a reactive gas, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using gases
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C30/00—Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Segura et al. | Grain boundary and microstructure engineering of Inconel 690 cladding on stainless-steel 316L using electron-beam powder bed fusion additive manufacturing | |
Mondal et al. | Effect of ultrasonic shot peening on oxidation behavior of T91 and SS347 steels in air and steam at 650° C | |
Romedenne et al. | High temperature air oxidation behavior of Hastelloy X processed by Electron Beam Melting (EBM) and Selective Laser Melting (SLM) | |
Oleksak et al. | Effect of surface finish on high-temperature oxidation of steels in CO2, supercritical CO2, and air | |
Zengwu et al. | Effect of shot peening on the oxidation resistance of TP304H and HR3C steels in water vapor | |
Günen et al. | Properties and corrosion behavior of chromium and vanadium carbide composite coatings produced on ductile cast iron by thermoreactive diffusion technique | |
Guo et al. | Characteristics of the corrosion products on three scratched heat-resisting alloys in closed-loop supercritical and high-temperature CO2 | |
Pour-Ali et al. | High-temperature oxidation behavior of GTD-111 Ni-based superalloy with an ultrafine-grained surface at 900 C | |
Dudziak et al. | Steam oxidation behavior of advanced steels and Ni-based alloys at 800 C | |
Chen et al. | A high-resolution study of the different surface state effects on the corrosion behaviors of a ferritic steel and an austenitic steel in supercritical water | |
Chyrkin et al. | External α-Al2O3 scale on Ni-base alloy 602 CA.–Part I: Formation and long-term stability | |
Guo et al. | Revealing the long-term oxidation and carburization mechanism of 310S SS and Alloy 800H exposed to supercritical carbon dioxide | |
Liu et al. | On the role of mechanical deformation in the environmental degradation of 310S stainless steels in supercritical carbon dioxide | |
Su et al. | Short-term oxidation behavior of 304 stainless steel in N2-21 vol% O2 environment between 900 and 1200° C | |
Dudziak et al. | Steam oxidation resistance of advanced steels and Ni-based alloys at 700° C for 1000 h | |
Archana et al. | High-temperature air and steam oxidation and oxide layer characteristics of alloy 617 | |
Zhao et al. | Oxidation behavior analysis of a ferritic ODS steel in supercritical Water | |
Chen et al. | Effect of surface conditions and alloying elements on the early oxidation behaviour of two austenitic alloys in the pure steam environment | |
Wei et al. | Understanding the high-temperature oxidation resistance of heat-resistant austenitic stainless steel with gradient nanostructure | |
Kong et al. | Microstructure and high temperature oxidation behavior of laser cladding C22 coating | |
Yan et al. | High-temperature oxidation behavior of 9Cr-5Si-3Al ferritic heat-resistant steel | |
Starostin et al. | High-Temperature Corrosion of Stainless Steels and Ni Alloys During Combustion of Urea–Ammonium Nitrate (UAN) Fuel | |
Huang et al. | Preparation and characterization of slurry aluminide coating on TP347H FG stainless steel | |
Bopape et al. | Effect of Co and Fe contents on the microstructure and corrosion behaviour of heat-treated Ni-Fe-Co superalloys in 3.5 wt% NaCl aqueous solution | |
Kikuchi et al. | Dynamic recrystallization of Fe-Cr alloys by atmospheric-controlled induction-heating fine particle peening |