Attarzadeh et al., 2017 - Google Patents
Comparison of the electrochemical behavior of Ti and nanostructured Ti-coated AISI 304 stainless steel in strongly acidic solutionsAttarzadeh et al., 2017
- Document ID
- 9568497030765321695
- Author
- Attarzadeh F
- Elmkhah H
- Fattah-Alhosseini A
- Publication year
- Publication venue
- Metallurgical and Materials Transactions B
External Links
Snippet
In this study, the electrochemical behaviors of pure titanium (Ti) and nanostructured (NS) Ti- coated AISI 304 stainless steel (SS) in strongly acidic solutions of H 2 SO 4 were investigated and compared. A type of physical vapor deposition method, cathodic arc …
- 239000003929 acidic solution 0 title abstract description 6
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C14/00—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C14/06—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material characterised by the coating material
- C23C14/14—Metallic material, boron or silicon
- C23C14/16—Metallic material, boron or silicon on metallic substrates or on substrates of boron or silicon
- C23C14/165—Metallic material, boron or silicon on metallic substrates or on substrates of boron or silicon by cathodic sputtering
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C14/00—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C14/22—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material characterised by the process of coating
- C23C14/34—Sputtering
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C14/00—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C14/06—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material characterised by the coating material
- C23C14/08—Oxides
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C14/00—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C14/0005—Separation of the coating from the substrate
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C28/00—Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Ruden et al. | Corrosion resistance of CrN thin films produced by dc magnetron sputtering | |
Liu et al. | EIS comparison on corrosion performance of PVD TiN and CrN coated mild steel in 0.5 N NaCl aqueous solution | |
Attarzadeh et al. | Comparison of the electrochemical behavior of Ti and nanostructured Ti-coated AISI 304 stainless steel in strongly acidic solutions | |
Wang et al. | Microstructure, spallation and corrosion of plasma sprayed Al2O3–13% TiO2 coatings | |
Sharifirad et al. | Electrodeposition and characterization of polypyrrole films on copper | |
Kang et al. | Effects of structural relaxation and crystallization on the corrosion resistance of an Fe-based amorphous coating | |
Fattah-alhosseini et al. | On the electrochemical behavior of PVD Ti-coated AISI 304 stainless steel in borate buffer solution | |
Kumar et al. | Effect of heat treatment on mechanical properties and corrosion performance of cold-sprayed tantalum coatings | |
Ramadan et al. | Calotropis Procera plant extract as green corrosion inhibitor for 304 stainless steel in hydrochloric acid solution | |
Schäfer et al. | Improving the corrosion protection of aluminium alloys using reactive magnetron sputtering | |
Maeng et al. | Corrosion behaviour of magnetron sputtered α-and β-Ta coatings on AISI 4340 steel as a function of coating thickness | |
Mendizabal et al. | Effect of N2 flow rate on the microstructure and electrochemical behavior of TaNx films deposited by modulated pulsed power magnetron sputtering | |
Bahari et al. | Surface analysis of Cu coated with ALD Al2O3 and its corrosion protection enhancement in NaCl solution: EIS and polarization | |
Fan et al. | Microstructure and corrosion resistance of the AlTiN coating deposited by arc ion plating | |
Jiang et al. | Effect of heat treatment on erosion-corrosion behavior of electroless Ni-P coatings in saline water | |
Zhou et al. | Preparation of Cu–Ni–Fe alloy coating and its evaluation on corrosion behavior in 3.5% NaCl solution | |
Kayali et al. | Investigation of wear and corrosion behaviour of AISI 316 L stainless steel coated by ESD surface modification | |
Heller et al. | Effect of phosphate source on post-treatment of cerium-based conversion coatings on Al 2024-T3 | |
Xing et al. | Corrosion resistance and passivation behavior of CoCrFeNi-TiAl high-entropy alloy coatings in acidic solutions | |
Velasco et al. | Effect of Si addition on the structure and corrosion behavior of NbN thin films deposited by unbalanced magnetron sputtering | |
Bahari et al. | Corrosion inhibition of Cu coated with Ni and annealed with flow of oxygen in NaCl solution as a function of annealing temperature | |
An et al. | Self‐regulated super‐hydrophobic Cu/CuO electrode film deposited by one‐step high‐power sputtering | |
Kameneva et al. | Effect of structure, phase, and elemental composition of AlN, CrAlN, and ZrAlN coatings on their electrochemical behavior in 3% NaCl solution | |
Deepa et al. | Tuning of electrochemical and topographical characteristics for enhancement of anti-corrosion performance of hot-dip TiO2–Zn–(1%) Al composite coatings | |
Asl et al. | The effects of heat treatment on the corrosion behavior of HVOF-sprayed WC-17 wt% Co coatings |