Kim et al., 2009 - Google Patents
Interfacial reaction and die attach properties of Zn-Sn high-temperature soldersKim et al., 2009
- Document ID
- 854051870501478898
- Author
- Kim S
- Kim K
- Kim S
- Suganuma K
- Publication year
- Publication venue
- Journal of electronic materials
External Links
Snippet
Interfacial reaction and die attach properties of Zn-x Sn (x= 20 wt.%, 30 wt.%, and 40 wt.%) solders on an aluminum nitride–direct bonded copper substrate were investigated. At the interface with Si die coated with Au/TiN thin layers, the TiN layer did not react with the solder …
- 229910000679 solder 0 title abstract description 103
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/26—Selection of soldering or welding materials proper with the principal constituent melting at less than 400 degrees C
- B23K35/262—Sn as the principal constituent
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/30—Selection of soldering or welding materials proper with the principal constituent melting at less than 1550 degrees C
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/02—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by mechanical features, e.g. shape
- B23K35/0222—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by mechanical features, e.g. shape for use in soldering, brazing
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C13/00—Alloys based on tin
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Kim et al. | Interfacial reaction and die attach properties of Zn-Sn high-temperature solders | |
Lee et al. | Interfacial properties of Zn–Sn alloys as high temperature lead-free solder on Cu substrate | |
Zhang et al. | Effect of Sb content on properties of Sn—Bi solders | |
Zhang et al. | Interface reaction between SnAgCu/SnAgCuCe solders and Cu substrate subjected to thermal cycling and isothermal aging | |
Wang et al. | Microstructural evolution and joint strength of Sn-58Bi/Cu joints through minor Zn alloying substrate during isothermal aging | |
Kim et al. | Improving the reliability of Si die attachment with Zn-Sn-based high-temperature Pb-free solder using a TiN diffusion barrier | |
Gao et al. | Effects of trace rare earth Nd addition on microstructure and properties of SnAgCu solder | |
Takahashi et al. | Improvement of high-temperature performance of Zn-Sn solder joint | |
Wei et al. | Torch brazing 3003 aluminum alloy with Zn—Al filler metal | |
Kim et al. | Interfacial reactions of Si die attachment with Zn-Sn and Au-20Sn high temperature lead-free solders on Cu substrates | |
Dai et al. | Microstructure and properties of 6061 aluminum alloy brazing joint with Al–Si–Zn filler metal | |
Garcia et al. | Wetting behavior and mechanical properties of Sn-Zn and Sn-Pb solder alloys | |
Zhao et al. | Effect of immersion Ni plating on interface microstructure and mechanical properties of Al/Cu bimetal | |
Torres et al. | Effect of antimony additions on corrosion and mechanical properties of Sn-Bi eutectic lead-free solder alloy | |
Shen et al. | Effects of Cu, Zn on the wettability and shear mechanical properties of Sn-Bi-based lead-free solders | |
Ma et al. | A study on the physical properties and interfacial reactions with Cu substrate of rapidly solidified Sn-3.5 Ag lead-free solder | |
Ho et al. | TEM investigation of interfacial microstructure and fracture mode of the Sn-Ag-Cu/Ni joint system | |
Yang et al. | Microstructure and Solderability of Zn-6Al-x Sn Solders | |
Yen et al. | Effect of Cu addition on interfacial reaction between Sn–9Zn solder and Ag | |
Laksono et al. | Interfacial reaction between Sn and Cu-Ti alloy (C1990HP) | |
Tsao et al. | Direct active soldering of Al0. 3CrFe1. 5MnNi0. 5 high entropy alloy to 6061-Al using Sn-Ag-Ti active solder | |
Abdullah et al. | Role of Cu percentage in the Sn-x Cu alloy on the mechanical performance at Sn-x Cu/ENIG interface produced by laser soldering | |
Zhang et al. | Wetting behavior of a novel Al-Si-Ti active brazing filler metal foil on aluminum matrix composite | |
Xiaoguo et al. | Microstructure and joining properties of high Nb-containing TiAl alloy brazed joints | |
Wang et al. | Liquid-state interfacial reactions of Sn-Zn/Co couples at 250° C |