Liu et al., 2016 - Google Patents
Effects of Nd/Gd value on the microstructures and mechanical properties of Mg–Gd–Y–Nd–Zr alloysLiu et al., 2016
View HTML- Document ID
- 6514909978475610375
- Author
- Liu X
- Zhang Z
- Le Q
- Bao L
- Publication year
- Publication venue
- Journal of Magnesium and Alloys
External Links
Snippet
Abstract Four Mg–Gd–Y–Nd–Zr alloys were prepared by mold casting to investigate the effects of Nd/Gd ratios on microstructures and mechanical properties. The as-cast alloys mainly consist of α-Mg and β-Mg 5 (GdYNd). Volume fractions of the second phase increase …
- 230000000694 effects 0 title abstract description 14
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C1/00—Making alloys
- C22C1/02—Making alloys by melting
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C21/00—Alloys based on aluminium
- C22C21/02—Alloys based on aluminium with silicon as the next major constituent
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/04—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of aluminium or alloys based thereon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C23/00—Alloys based on magnesium
- C22C23/02—Alloys based on magnesium with aluminium as the next major constituent
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C14/00—Alloys based on titanium
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C18/00—Alloys based on zinc
- C22C18/04—Alloys based on zinc with aluminium as the next major constituent
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C16/00—Alloys based on zirconium
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Liu et al. | Effects of Nd/Gd value on the microstructures and mechanical properties of Mg–Gd–Y–Nd–Zr alloys | |
Yin et al. | Effects of Zn/Gd ratio on the microstructures and mechanical properties of Mg-Zn-Gd-Zr alloys | |
Elsayed et al. | Effect of extrusion conditions on microstructure and mechanical properties of microalloyed Mg–Sn–Al–Zn alloys | |
Zhao et al. | Influences of Fe, Si and homogenization on electrical conductivity and mechanical properties of dilute Al–Mg–Si alloy | |
Yu et al. | Effects of extrusion speed on the microstructure and mechanical properties of ZK60 alloys with and without 1 wt% cerium addition | |
Liu et al. | Influence of Zn content on the microstructure and mechanical properties of extruded Mg–5Y–4Gd–0.4 Zr alloy | |
Liu et al. | Microstructures and mechanical properties of high performance Mg–6Gd–3Y–2Nd–0.4 Zr alloy by indirect extrusion and aging treatment | |
Guo et al. | Achieving high-strength magnesium matrix nanocomposite through synergistical effect of external hybrid (SiC+ TiC) nanoparticles and dynamic precipitated phase | |
Wang et al. | Grain refinement limit and mechanical properties of 6063 alloy inoculated by Al–Ti–C (B) master alloys | |
Liu et al. | Refinement effect of cerium, calcium and strontium in AZ91 magnesium alloy | |
Meng et al. | Microstructures and properties of superlight Mg–Li–Al–Zn wrought alloys | |
Lv et al. | The effect of addition of Nd and Ce on the microstructure and mechanical properties of ZM21 Mg alloy | |
Wang et al. | Microstructure and properties of Mg–8Li–1Al–1Ce alloy | |
Zhao et al. | Optimizing microstructures of dilute Al–Fe–Si alloys designed with enhanced electrical conductivity and tensile strength | |
Nie et al. | Effect of extrusion temperature on microstructure and mechanical properties of a low-alloying and ultra-high strength Mg–Zn–Ca–Mn matrix composite containing trace TiC nanoparticles | |
Hu et al. | Enhanced mechanical properties of an Al-Mg-Si alloy by repetitive continuous extrusion forming process and subsequent aging treatment | |
Xiang et al. | Influence of Sn on microstructure and mechanical properties of Mg–5Li–3Al–2Zn alloys | |
Wen et al. | Effect of Ca addition on the microstructure and tensile properties of Mg–4.0 Zn–2.0 Gd alloys | |
Ma et al. | Microstructure, texture evolution, and mechanical properties of ECAP-processed ZAT522 magnesium alloy | |
Zhang et al. | Microstructures and mechanical properties of Mg–13Gd–5Er–1Zn–0.3 Zr alloy | |
Chen et al. | Effects of Ti addition on the microstructure and mechanical properties of Mg–Zn–Zr–Ca alloys | |
Chen et al. | Microstructure and high temperature mechanical properties of the Mg-Gd-Y (-Nd)-Zr alloy | |
Wu et al. | Effects of minor scandium addition on the properties of Mg–Li–Al–Zn alloy | |
Liu et al. | Effect of Ce addition on hot tearing behavior of AZ91 alloy | |
Jiang et al. | Effect of Sr on microstructure and aging behavior of Mg–14Li alloys |