Healing of glass in humid environmentsHolden et al., 1989
- Document ID
- 16594869625191150764
- Author
- Holden M
- Frechette V
- Publication year
- Publication venue
- Journal of the American Ceramic Society
External Links
Snippet
Chill checks of controlled depth were produced in soda‐lime‐silica glass, and an optimum humidity of 30 kPa (300 mbar) water vapor pressure was found to heal these checks in an annealing cycle. Critical factors were found to be a fluxing effect, having a direct …
- 230000035876 healing 0 title abstract description 34
Classifications
-
- C—CHEMISTRY; METALLURGY
- C04—CEMENTS; CONCRETE; ARTIFICIAL STONE; CERAMICS; REFRACTORIES
- C04B—LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE; CERAMICS; REFRACTORIES; TREATMENT OF NATURAL STONE
- C04B41/00—After-treatment of mortars, concrete, artificial stone or ceramics; Treatment of natural stone
- C04B41/009—After-treatment of mortars, concrete, artificial stone or ceramics; Treatment of natural stone characterised by the material treated
-
- C—CHEMISTRY; METALLURGY
- C04—CEMENTS; CONCRETE; ARTIFICIAL STONE; CERAMICS; REFRACTORIES
- C04B—LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE; CERAMICS; REFRACTORIES; TREATMENT OF NATURAL STONE
- C04B41/00—After-treatment of mortars, concrete, artificial stone or ceramics; Treatment of natural stone
- C04B41/45—Coating or impregnating, e.g. injection in masonry, partial coating of green or fired ceramics, organic coating compositions for adhering together two concrete elements
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Ritter Jr et al. | Dynamic and static fatigue of silicate glasses | |
Ito et al. | Crack blunting of high‐silica glass | |
Borom et al. | Strength and microstructure in lithium disilicate glass‐ceramics | |
Parikh | Effect of atmosphere on surface tension of glass | |
Wachtman Jr | Highlights of progress in the science of fracture of ceramics and glass | |
Shelby et al. | Quantitative determination of the hydroxyl content of vitreous silica | |
Korwin-Edson et al. | Strength of high performance glass reinforcement fiber | |
HIRAO et al. | Kinetics of crack tip blunting of glasses | |
Holden et al. | Healing of glass in humid environments | |
Sheth et al. | Effects of tempering and heat strengthening on hardness, indentation fracture resistance, and wear of soda lime float glass | |
RITTER JR et al. | Effect of Test Environment on Stress‐Corrosion Susceptibility of Glass | |
Tandon et al. | Surface stress effects on indentation fracture sequences | |
Wilder et al. | Property Variation in Alkali Alkaline‐Earth Metaphosphate Glasses | |
Gogotsi et al. | Stress‐Enhanced Oxidation of Silicon Nitride Ceramics | |
Taniguchi | Surface tension of melts in the system CaMgSi2O6-CaAl2Si2O8 and its structural significance | |
Shelby et al. | Weathering of glasses for solar applications | |
James et al. | Strengthening of soda-lime-silica glass by sol-gel-and melt-derived coatings | |
Lucchini et al. | Sintering of glass bonded ceramic barium hexaferrite magnetic powders | |
Han et al. | Mechanism of mechanical strength increase of soda–lime glass by aging | |
McMillan et al. | The effect of hydroxyl ion content on the mechanical and other properties of soda-lime-silica glass | |
Michalske et al. | Mechanical properties and adhesion of hydrated glass surface layers | |
Lezzi et al. | Static fatigue and compressive stress generation in an aged crack | |
Benbahouche et al. | Effect of water corrosion on cracks and vickers imprints in glass | |
Koide et al. | Viscosity of fluoride glasses at glass transition temperature | |
Choi et al. | Slow crack growth of indent cracks in glass with and without applied stress |